Microstructure and enhanced strength-ductility of TiNbCu alloys produced by laser powder bed fusion

被引:7
|
作者
Jin, Jianbo [1 ]
Yang, Huan [2 ]
Liu, Yujing [3 ]
Yang, Junjie [1 ]
Li, Kunmao [1 ]
Yi, Yanliang [1 ]
Chen, Dongchu [4 ]
Zhang, Wencai [5 ]
Zhou, Shengfeng [1 ,6 ]
机构
[1] Jinan Univ, Inst Adv Wear & Corros Resistance & Funct Mat, Guangzhou 510632, Peoples R China
[2] Shenzhen Technol Univ, Sino German Coll Intelligent Mfg, Shenzhen 518118, Peoples R China
[3] Changsha Univ Sci & Technol, Inst Met, Coll Mat Sci & Engn, 960,2 Sect,Wanjiali RD, Changsha 410004, Hunan, Peoples R China
[4] Foshan Univ, Sch Mat Sci & Energy Engn, Foshan 52800, Guangdong, Peoples R China
[5] Jinan Univ, Affiliated Hosp 1, Dept Orthoped, Guangzhou 510632, Peoples R China
[6] Chongqing Univ, State Key Lab Mech Transmiss, Chongqing 400044, Peoples R China
基金
中国国家自然科学基金;
关键词
Laser powder bed fusion (L-PBF); Mechanical properties; Ti2Cu; Tensile strength; Grain boundaries; TI-NB ALLOYS; ANTIBACTERIAL PROPERTIES; MECHANICAL-BEHAVIOR; IN-VITRO; TITANIUM-ALLOY; CORROSION; PRECIPITATION; CYTOTOXICITY; PERFORMANCE; DEPOSITION;
D O I
10.1016/j.msea.2023.145889
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The beta-type Ti35NbxCu alloys (x = 0, 1, 3, 5, and 7 wt%) were produced by laser powder bed fusion (LPBF) and the influence of Cu content on the microstructure and mechanical properties was studied. The results indicate that when the content of Cu is less than 3 wt%, Cu can diffuse completely into the Ti matrix to form solid solution without element segregation. Moreover, the elastic modulus of Ti35Nb1Cu alloy (49.1 +/- 1.6 GPa) is reduced by 33 % compared to that of Ti35Nb alloy (73.2 +/- 1.4 GPa). When the content of Cu exceeds 3 wt%, the eutectoid reaction is activated during the cyclic heating and rapid cooling of LPBF, and the partially supersaturated beta phase is transformed into nano-scale alpha and Ti2Cu phases (beta ->alpha+Ti2Cu). Nano-scale Ti2Cu particles precipitated along beta grain boundary results in a pinning effect, which inhibits the growth of beta grain, hinders dislocation movement, and improves the strength of the alloy. However, when the content of Cu is 7 wt%, the dislocation density (4.179 x 1015 m  2) and the ratio of brittle phase Ti2Cu (8.5 %) are too high, and the stress concentration caused by the initiation of inherent micro-cracks are the main reason for the tensile brittle fracture of Ti35Nb7Cu alloy. As such, the Ti35Nb5Cu alloy has the highest tensile strength of 867.3 +/- 24 MPa and the elongation reaches 11.7 +/- 0.5 %. Therefore, solution strengthening of Cu, fine grain strengthening of beta, dislocation strengthening, and precipitation strengthening of Ti2Cu are the main reasons for the excellent comprehensive mechanical properties of Ti35Nb5Cu alloy.
引用
收藏
页数:19
相关论文
共 50 条
  • [31] Graphene/ZrO2/aluminum alloy composite with enhanced strength and ductility fabricated by laser powder bed fusion
    Zhang, Shuzhe
    Wei, Pei
    Chen, Zhen
    Li, Bobo
    Huang, Ke
    Zou, Yatong
    Lu, Bingheng
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 910
  • [32] Graphene/ZrO2/aluminum alloy composite with enhanced strength and ductility fabricated by laser powder bed fusion
    Zhang, Shuzhe
    Wei, Pei
    Chen, Zhen
    Li, Bobo
    Huang, Ke
    Zou, Yatong
    Lu, Bingheng
    Journal of Alloys and Compounds, 2022, 910
  • [33] Heat treatment of aluminium alloys produced by laser powder bed fusion: A review
    Fiocchi, J.
    Tuissi, A.
    Biffi, C. A.
    MATERIALS & DESIGN, 2021, 204
  • [34] Laser powder bed fusion of an age-hardenable Mg-10Gd-0.2Zr alloy with excellent strength-ductility synergy
    Deng, Qingchen
    Zhang, Yu
    Liu, Ziyi
    Chang, Zhiyu
    Su, Ning
    Wu, Yujuan
    Hao, Longlong
    Peng, Liming
    Ding, Wenjiang
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 910
  • [35] Towards strength-ductility synergy in nanosheets strengthened titanium matrix composites through laser power bed fusion of MXene/Ti composite powder
    Wang, L.
    Li, J.
    Liu, Z. Q.
    Li, S. F.
    Yang, Y. F.
    Misra, R. D. K.
    Tian, Z. J.
    MATERIALS TECHNOLOGY, 2023, 38 (01)
  • [36] Laser powder bed fusion of biodegradable magnesium alloys: process, microstructure and properties
    Wu, Xuehua
    Liu, Junying
    Yang, Youwen
    Bai, Jing
    Shuai, Cijun
    Buhagiar, Joseph
    Ning, Xinghai
    INTERNATIONAL JOURNAL OF EXTREME MANUFACTURING, 2025, 7 (02)
  • [37] Solidification microstructure selection maps for laser powder bed fusion of multicomponent alloys
    Mohammadpour, P.
    Phillion, A. B.
    INTERNATIONAL CONFERENCE ON MODELLING OF CASTING, WELDING AND ADVANCED SOLIDIFICATION PROCESSES (MCWASP XV), 2020, 861
  • [38] Microstructure of aluminum alloys manufactured via laser powder bed fusion: A review
    Yu, Wenhui
    Zheng, Hongyu
    Xiao, Zhen
    Materials Today: Proceedings, 2022, 70 : 382 - 387
  • [39] Achieving strength-ductility balance in a laser powder bed fusion fabricated TiB2/Al-Cu-Mg-Ag alloy
    Jiang, Fuqing
    Tang, Lei
    Li, Sheng
    Ye, Hengqiang
    Attallah, Moataz M.
    Yang, Zhiqing
    JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 945
  • [40] Laser powder bed fusion of Al-Doped CoCrNi Medium Entropy Alloy: Microstructural mechanisms imparting high strength-ductility synergy
    Zhang, Zhengtong
    Tu, Jian
    Zhang, Xingqun
    Qiu, Yingkun
    Du, Yanbin
    Liang, Yanxiang
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2025, 927