Study on Carbon Deposition and Coil Breakdown Mechanism of Medium Frequency Coreless Induction Furnace

被引:1
|
作者
Cong, Jianchen [1 ,2 ]
Wang, Haixiao [1 ]
Wang, Darui [2 ]
Jiang, Tao [2 ]
Feng, Meizhen [3 ]
Ni, Peixiang [2 ]
Wang, Jinling [4 ]
机构
[1] Shandong Univ Technol, Sch Mech Engn, Zibo 255049, Peoples R China
[2] Tianrun Ind Technol Co Ltd, Weihai 264200, Peoples R China
[3] Caterpillar Res & Dev Ctr China Co Ltd, Wuxi 214028, Peoples R China
[4] Zibo Vocat Inst, Sch Intelligent Mfg, Zibo 255314, Peoples R China
关键词
coil breakdown; carbon attaching mechanism; cast iron melting; medium frequency coreless induction furnace; HIGH-TEMPERATURE ELECTROLYSIS; HYDROGEN-PRODUCTION; STEAM ELECTROLYSIS; MIXTURE;
D O I
10.1007/s40962-023-01122-6
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The medium frequency coreless induction furnace has gradually replaced the cupola in cast iron melting. However, induction coils at the bottom 1-6 turns can experience issues posing production and resulting safety risks. A kind of coil interturn breakdown failure caused by black attachment has occurred in our engineering practices. To explain the attaching and breakdown mechanism, an experimental investigation and detailed analysis of physical and chemical processes are performed. SEM, EDS and Fourier transform infrared spectrum results show that the attachment is primarily composed of free carbon, with a mass and atomic fraction of 62 and 71%, respectively. There were no C-H bonds in the powdered black attachment. The redox reactions of SiO2 and C, hydrogen and disproportionation reactions of CO and the ionization reactions of H2O contribute to the C transfers. The physical isolation of the Isoplan board, which prevents the mixture of CO, CO2, H-2, H2O, and O-2 from diffusing, causes C deposited only on the coil surface. The conductive carbon deposition in a moisture environment reduces the insulation degree of interturns and generates high-voltage discharge between adjacent coils. According to the findings, three improvement strategies are proposed and validated: (1) drilling holes in the Isoplan board; (2) unplugging the silicate insulating cloth in the lining sintering; and (3) as new lining is put into service, silicon steel sheets are prioritized for use as furnace charge.
引用
收藏
页码:1236 / 1246
页数:11
相关论文
共 50 条
  • [31] DETERMINATION OF TRACE AMOUNT OF CARBON IN IRON AND STEEL BY TUBE FURNACE COMBUSTION CONDUCTOMETRIC METHOD AND HIGH-FREQUENCY INDUCTION FURNACE-INFRARED ABSORPTIOMETRIC METHOD
    INOKUMA, Y
    ENDO, J
    OKA, Y
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1987, 27 (02) : B34 - B34
  • [32] Austenite grain coarsening of V-microalloyed medium carbon steel during high frequency induction heating: Monte Carlo simulation study
    Kim, T. H.
    Park, J. K.
    MATERIALS SCIENCE AND TECHNOLOGY, 2013, 29 (12) : 1414 - 1422
  • [33] Electrochemical Deposition of Silicon-Carbon Films: A Study on the Nucleation and Growth Mechanism
    Plugotarenko, Nina K.
    Myasoedova, Tatiana N.
    Grigoryev, Mikhail N.
    Mikhailova, Tatiana S.
    NANOMATERIALS, 2019, 9 (12)
  • [34] Study of carbonation mechanism of blast-furnace slag cement with different carbon dioxide concentrations
    Iyoda, T.
    Toyomura, E.
    Goto, S.
    Asaga, K.
    LIFE-CYCLE OF STRUCTURAL SYSTEMS: DESIGN, ASSESSMENT, MAINTENANCE AND MANAGEMENT, 2015, : 1686 - 1693
  • [35] STUDY ON OXIDATION MECHANISM OF CARBON-BLACKS BY OZONE IN AQUEOUS-MEDIUM
    DONNET, JB
    EHRBURGE.P
    VOET, A
    CARBON, 1972, 10 (06) : 737 - &
  • [36] NON-AQUEOUS TITRIMETRIC METHOD FOR CARBON DETERMINATION IN IRON AND STEEL MODIFIED FOR USE WITH A HIGH-FREQUENCY INDUCTION FURNACE
    WILKINSON, T
    FOSTER, WW
    HARRISON, TS
    METALLURGIA AND METAL FORMING, 1973, 40 (02): : 61 - 62
  • [37] I. The efficiency of generation of high-frequency oscillations by means of an induction coil and ordinary spark-gap. II. An oscillographic study of some induction coil phenomena.
    Howe, GWO
    Peattie, JD
    PROCEEDINGS OF THE PHYSICAL SOCIETY OF LONDON, 1912, 24 : 317 - 341
  • [38] Investigation on Energy-Effectiveness Enhancement of Medium-Frequency Induction Furnace Based on an Adaptive Chaos Immune Optimization Algorithm with Mutative Scale
    Zuo, Hongyan
    Zhu, Yun
    Tan, Dongli
    Cui, Shuwan
    Tan, Jiqiu
    Zhong, Dingqing
    PROCESSES, 2022, 10 (03)
  • [39] Calibration method for the determination of trace amounts of carbon in steel by an infrared absorption method after combustion in a high-frequency induction furnace
    Koga, H
    Ogata, M
    BUNSEKI KAGAKU, 2002, 51 (09) : 825 - 830
  • [40] Synthesis and growth mechanism of carbon-supported nanoparticle catalysts by physical vapor deposition onto a liquid medium substrate
    Cha, In Young
    Kim, Hyung Tae
    Ahn, Minjeh
    Jang, Jong Hyun
    Kim, Young Gyu
    Sung, Yung-Eun
    Yoo, Sung Jong
    APPLIED SURFACE SCIENCE, 2019, 471 : 1083 - 1087