Study on Carbon Deposition and Coil Breakdown Mechanism of Medium Frequency Coreless Induction Furnace

被引:1
|
作者
Cong, Jianchen [1 ,2 ]
Wang, Haixiao [1 ]
Wang, Darui [2 ]
Jiang, Tao [2 ]
Feng, Meizhen [3 ]
Ni, Peixiang [2 ]
Wang, Jinling [4 ]
机构
[1] Shandong Univ Technol, Sch Mech Engn, Zibo 255049, Peoples R China
[2] Tianrun Ind Technol Co Ltd, Weihai 264200, Peoples R China
[3] Caterpillar Res & Dev Ctr China Co Ltd, Wuxi 214028, Peoples R China
[4] Zibo Vocat Inst, Sch Intelligent Mfg, Zibo 255314, Peoples R China
关键词
coil breakdown; carbon attaching mechanism; cast iron melting; medium frequency coreless induction furnace; HIGH-TEMPERATURE ELECTROLYSIS; HYDROGEN-PRODUCTION; STEAM ELECTROLYSIS; MIXTURE;
D O I
10.1007/s40962-023-01122-6
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The medium frequency coreless induction furnace has gradually replaced the cupola in cast iron melting. However, induction coils at the bottom 1-6 turns can experience issues posing production and resulting safety risks. A kind of coil interturn breakdown failure caused by black attachment has occurred in our engineering practices. To explain the attaching and breakdown mechanism, an experimental investigation and detailed analysis of physical and chemical processes are performed. SEM, EDS and Fourier transform infrared spectrum results show that the attachment is primarily composed of free carbon, with a mass and atomic fraction of 62 and 71%, respectively. There were no C-H bonds in the powdered black attachment. The redox reactions of SiO2 and C, hydrogen and disproportionation reactions of CO and the ionization reactions of H2O contribute to the C transfers. The physical isolation of the Isoplan board, which prevents the mixture of CO, CO2, H-2, H2O, and O-2 from diffusing, causes C deposited only on the coil surface. The conductive carbon deposition in a moisture environment reduces the insulation degree of interturns and generates high-voltage discharge between adjacent coils. According to the findings, three improvement strategies are proposed and validated: (1) drilling holes in the Isoplan board; (2) unplugging the silicate insulating cloth in the lining sintering; and (3) as new lining is put into service, silicon steel sheets are prioritized for use as furnace charge.
引用
收藏
页码:1236 / 1246
页数:11
相关论文
共 50 条
  • [21] Experience with a Medium Frequency Crucible Induction Melting Furnace for Copper-Base Alloys.
    Pitch, Richard
    Giesserei, 1981, 68 (23): : 683 - 687
  • [22] Researches of characteristics and problems of liquid iron during melting process with medium frequency induction furnace
    Foundry Research Institute, Shandong Shifeng Group Co., Ltd., Liaocheng 252800, China
    Zhuzao, 2006, 12 (1305-1307):
  • [23] CAST STEEL PRODUCTION IN INDUCTION FURNACE - METALLURGICAL ASPECTS OF CHOICE BETWEEN MEDIUM OR LOW-FREQUENCY
    DETREZ, P
    FONDERIE, 1972, (318): : 441 - 445
  • [24] Study on deposition mechanism of Pt nanoparticles on carbon nanotube
    Yao, YL
    Zhang, D
    Xia, XH
    CHINESE JOURNAL OF INORGANIC CHEMISTRY, 2004, 20 (05) : 531 - 535
  • [25] Determination of carbon in high-melting alloys using the high-frequency induction furnace
    Smith, GF
    Hockenyos, GL
    INDUSTRIAL AND ENGINEERING CHEMISTRY-ANALYTICAL EDITION, 1930, 2 : 0036 - 0038
  • [26] Study on application and realization of integrated control to medium-frequency induction heating
    Wang, Yiwang
    MECHATRONICS AND INTELLIGENT MATERIALS III, PTS 1-3, 2013, 706-708 : 1167 - 1170
  • [27] DEPOSITION OF DIAMOND-LIKE CARBON USING A PLANAR RADIO-FREQUENCY INDUCTION PLASMA
    PAPPAS, DL
    HOPWOOD, J
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A-VACUUM SURFACES AND FILMS, 1994, 12 (04): : 1576 - 1582
  • [28] Silver deposition on silicon and glassy carbon.: A comparative study in cyanide medium
    Márquez, K
    Staikov, G
    Schultze, JW
    ELECTROCHIMICA ACTA, 2003, 48 (07) : 875 - 882
  • [29] Experimental study of a radio-frequency Ionized Physical Vapour Deposition process:: Contamination by the internal coil
    Imbert, J. -C.
    de Poucques, L.
    Boisse-Laporte, C.
    Bretagne, J.
    Hugon, M. C.
    Pagnon, D.
    Pitach, P.
    Teule-Gay, L.
    Touzeau, M.
    THIN SOLID FILMS, 2008, 516 (15) : 4700 - 4708
  • [30] Study of forming mechanism of abnormal erosion line of carbon brick for blast furnace hearth
    You, Jinzhou
    Liu, Zijiu
    Wuhan Gangtie Xueyuan Xuebao/Journal of Wuhan Iron and Steel University, 1998, 21 (02): : 144 - 148