摘要
For magnesium, nickel, and stainless steel, solidification cracking is a critical failure mode that has been extensively studied for decades. The nature of solidification cracking can be investigated through experiments or theoretical calculations. Different models have been proposed for these calculations, including the cracking susceptibility index (CSI), which was developed in the last decade. Building a CSI map for a group of metals facilitates referencing or comparison when the metal is applied in casting, welding, or developing new alloys. In this study, the CSI of various types of stainless steel was examined, and CSI maps were constructed. For each type of alloy, the calculations include more than ten experimentally determined compositions from commercial alloys. The CSI maps of stainless steel were constructed and compared with those of the Cr and Ni equivalents, as well as their respective phase diagrams. The CSI sequence matched the cracking results of previous studies on austenitic steels. The ferritic type had a lower CSI but a higher cracking rate, which could be attributed to the ductility gap during the austenite-ferrite transformation, as reported in previous studies. (c) 2023 The Authors. Published by Elsevier B.V. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).
引用
收藏
页码:1030 / 1040
页数:11
相关论文
共 50 条
  • [21] Solidification cracking susceptibility of ferritic stainless steels using Modified Varestraint Transvarestraint (MVT) method
    Konadu, D. S.
    Pistorius, P. G. H.
    Du Toit, M.
    Griesche, Axel
    SADHANA-ACADEMY PROCEEDINGS IN ENGINEERING SCIENCES, 2019, 44 (09):
  • [22] Prediction of solidification mode and hot cracking susceptibility in laser welds of high nitrogen stainless steels
    Nishimoto, K
    Mori, H
    TRENDS IN WELDING RESEARCH, PROCEEDINGS, 2003, : 53 - 58
  • [23] EFFECT OF ELECTRODE GEOMETRY ON THE WELD SOLIDIFICATION CRACKING OF 2 STAINLESS-STEELS IN GTA WELDING
    HABCHI, G
    MARYA, SK
    SCRIPTA METALLURGICA, 1986, 20 (02): : 207 - 212
  • [24] Effects of ferrite content and concentrations of carbon and silicon on weld solidification cracking susceptibility of stainless steels
    Kadoi, Kota
    Ueno, Seiya
    Inoue, Hiroshige
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 25 : 1314 - 1321
  • [25] Solidification cracking susceptibility of ferritic stainless steels using Modified Varestraint Transvarestraint (MVT) method
    D S Konadu
    P G H Pistorius
    M Du Toit
    Axel Griesche
    Sādhanā, 2019, 44
  • [26] Effect of nitrogen and solidification mode on hot cracking susceptibility in laser welds of austenitic stainless steels
    Nishimoto, K
    Mori, H
    FIRST INTERNATIONAL SYMPOSIUM ON HIGH-POWER LASER MACROPROCESSING, 2003, 4831 : 214 - 223
  • [27] CASTING AND SOLIDIFICATION OF STAINLESS-STEELS
    THIELMANN, R
    BIESTERFELD, W
    SCHMITTHENNER, HE
    UNGER, KD
    STAHL UND EISEN, 1987, 107 (25-26): : 1205 - 1213
  • [28] DELAYED CRACKING OF STAINLESS-STEELS
    BERDING, JT
    JAYARAMAN, N
    STEELE, JH
    JASPER, JC
    JOURNAL OF METALS, 1983, 35 (08): : A39 - A39
  • [29] Stress corrosion cracking of stainless steels
    Steel Products Lab., Nippon Steel Corp., Japan
    Yosetsu Gakkai Shi, 2006, 3 (27-30):
  • [30] Stress corrosion cracking of stainless steels
    Steel Products Lab., Nippon Steel Corp., Japan
    Weld. Int., 2007, 2 (95-99): : 95 - 99