Influence of two-step austempering at different temperatures on mechanical and microstructural properties of AISI 9254 high silicon steel

被引:2
|
作者
Nalcaci, Burak [1 ,2 ,7 ,8 ]
Baysun, Meltem [3 ]
Bahador, Abdollah [4 ,5 ]
Umeda, Junko [4 ]
Muenstermann, Sebastian [2 ]
Kaya, Ali Arslan [6 ]
Erdogan, Mehmet [1 ]
机构
[1] Gazi Univ, Dept Met & Mat Engn, Ankara, Turkiye
[2] RWTH Aachen Univ Aachen, Steel Inst, Integr Mat & Struct, Aachen, Germany
[3] Gazi Univ, Inst Sci, Dept Met & Mat Engn, Ankara, Turkiye
[4] Osaka Univ, Joining & Welding Res Inst, Osaka, Japan
[5] Univ Teknol Malaysia, Razak Fac Technol & Informat, Kuala Lumpur, Malaysia
[6] Mugla Sitki Kocman Univ, Dept Met & Mat Engn, Mugla, Turkiye
[7] Gazi Univ, Dept Met & Mat Engn, TR-06560 Yenimahalle, Ankara, Turkiye
[8] Rhein Westfal TH Aachen, Steel Inst, Integr Mat & Struct, D-52072 Aachen, Germany
关键词
AISI 9254 high silicon steel; two-step austempering; mechanical properties; carbide-free bainite; martensite; strain hardening; phase transformation; EBSD analysis; ISOTHERMAL TRANSFORMATION KINETICS; BAINITIC STEEL; DUCTILE IRON; M-S; STRENGTH; BEHAVIOR; PRECIPITATION; IMPROVEMENT; MARTENSITE; EVOLUTION;
D O I
10.1080/03019233.2023.2204268
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
This study was undertaken to understand the effects of two-step austempering treatment on an AISI 9254 high silicon steel towards tailoring the properties as desired while simultaneously employing the benefits of high and low austempering temperatures. The samples were initially austenitized at 850 degrees C for 20 min, followed by austempering in a salt bath at the temperatures of 250-270-290 degrees C for 20 min during the first stage. Subsequently, a second stage austempering was carried out by raising the temperature of the salt bath to 300 degrees C at an average heating rate of 0.5 degrees C/min, and the samples were kept in the salt bath for achieving a total austempering time of 120 min including the heating time. A conventional single-stage austempering was also conducted for comparison purposes, in which the austenitization temperature, the austempering temperatures and total time (stage I and stage II, i.e. 120 min) were kept the same for the benchmark samples. In the characterization studies, tensile test, hardness test, XRD analysis, optical microscope and field emission-scanning electron microscope (FE-SEM) equipped with EBSD detector were utilized. The findings of this study indicated that lowering the austempering temperature resulted in refining the structure with a decrease in the amount of austenite. According to the carbon content analysis through XRD patterns, the two-step austempering processes appeared to have considerably increased the carbon content of the austenite irrespective of austempering temperature. The best ultimate tensile strength (U.T.S) of 2194 MPa was achieved in the conventionally austempered sample at the lowest temperature of 250 degrees C, while the best yield strength (Y.S.) of 1753 MPa was reached in the stepped austempered sample initially at 250 degrees C followed by 300 degrees C. In general, two-step austempering process led to a higher yield strength while affecting the ultimate tensile strength and total elongation depending on the austempering temperature.
引用
收藏
页码:1331 / 1339
页数:9
相关论文
共 50 条
  • [41] Mechanical Properties of Steel Bolts with Different Diameters after Exposure to High Temperatures
    Daryan, Amir Saedi
    Ketabdari, Hesam
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2019, 31 (10)
  • [42] On a New Two-Step Air Cooling Method Following Thermomechanically Controlled Rolling: Microstructural Evolution and Mechanical Properties of a High-Strength Multiphase Medium Carbon Microalloyed Steel
    Magham, Hari Srinivasa Rao
    Maheswari, Nandakumar
    Dinesh, Kumar
    Vijayaraghavan, Lakshmanan
    Sankaran, Shanmugam
    Padmanabhan, Kuppuswamy Anantha
    STEEL RESEARCH INTERNATIONAL, 2021, 92 (05)
  • [43] Influence of high temperatures on the mechanical and microstructural properties of hybrid steel-basalt fibers based ultra-high-performance concrete (UHPC)
    Khan, Mehran
    Lao, Jiancong
    Ahmad, Muhammad Riaz
    Dai, Jian-Guo
    CONSTRUCTION AND BUILDING MATERIALS, 2024, 411
  • [44] Effects of two-step annealing on texture and magnetic properties by addition of Co, Mo, or Ni in silicon steel
    Cai, Yan Bo
    Chang, Sam Kyu
    ISIJ INTERNATIONAL, 2007, 47 (11) : 1680 - 1686
  • [45] Influence of Sensitization on Mechanical Properties of AISI 304 Stainless Steel under High-Temperature
    Jung, Kwang-Hu
    Kim, Seong-Jong
    JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2019, 19 (07) : 4265 - 4269
  • [46] INFLUENCE OF TWO-STEP SINTERING ON MICROSTRUCTURE EVOLUTION AND MECHANICAL PROPERTIES OF ALUMINA-NANOZIRCONIA COMPOSITES
    Wojtowicz, Bartosz
    Pyda, Waldemar
    COMPOSITES THEORY AND PRACTICE, 2012, 12 (02): : 132 - 137
  • [47] The Effect of Two-Step Heat Treatment Parameters on Microstructure and Mechanical Properties of 42SiMn Steel
    Kucerova, Ludmila
    METALS, 2017, 7 (12):
  • [48] Microstructure and mechanical properties of TiC steel-bonded carbides prepared by two-step sintering technique
    Guo, Xiaoge
    Zheng, Yong
    Zhang, Guotao
    Wu, Hao
    Yang, Zhengkai
    Gong, Ao
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2020, 93
  • [49] Microstructure and mechanical properties of 18Mn3Si2CrMo steel subjected to austempering at different temperatures below Ms
    Xia, Shule
    Zhang, Fucheng
    Yang, Zhinan
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 724 : 103 - 111
  • [50] Mechanical properties and microstructural features of AISI 4340 high-strength alloy steel under quenched and tempered conditions
    Lee, WS
    Su, TT
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 1999, 87 (1-3) : 198 - 206