Influence of two-step austempering at different temperatures on mechanical and microstructural properties of AISI 9254 high silicon steel

被引:2
|
作者
Nalcaci, Burak [1 ,2 ,7 ,8 ]
Baysun, Meltem [3 ]
Bahador, Abdollah [4 ,5 ]
Umeda, Junko [4 ]
Muenstermann, Sebastian [2 ]
Kaya, Ali Arslan [6 ]
Erdogan, Mehmet [1 ]
机构
[1] Gazi Univ, Dept Met & Mat Engn, Ankara, Turkiye
[2] RWTH Aachen Univ Aachen, Steel Inst, Integr Mat & Struct, Aachen, Germany
[3] Gazi Univ, Inst Sci, Dept Met & Mat Engn, Ankara, Turkiye
[4] Osaka Univ, Joining & Welding Res Inst, Osaka, Japan
[5] Univ Teknol Malaysia, Razak Fac Technol & Informat, Kuala Lumpur, Malaysia
[6] Mugla Sitki Kocman Univ, Dept Met & Mat Engn, Mugla, Turkiye
[7] Gazi Univ, Dept Met & Mat Engn, TR-06560 Yenimahalle, Ankara, Turkiye
[8] Rhein Westfal TH Aachen, Steel Inst, Integr Mat & Struct, D-52072 Aachen, Germany
关键词
AISI 9254 high silicon steel; two-step austempering; mechanical properties; carbide-free bainite; martensite; strain hardening; phase transformation; EBSD analysis; ISOTHERMAL TRANSFORMATION KINETICS; BAINITIC STEEL; DUCTILE IRON; M-S; STRENGTH; BEHAVIOR; PRECIPITATION; IMPROVEMENT; MARTENSITE; EVOLUTION;
D O I
10.1080/03019233.2023.2204268
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
This study was undertaken to understand the effects of two-step austempering treatment on an AISI 9254 high silicon steel towards tailoring the properties as desired while simultaneously employing the benefits of high and low austempering temperatures. The samples were initially austenitized at 850 degrees C for 20 min, followed by austempering in a salt bath at the temperatures of 250-270-290 degrees C for 20 min during the first stage. Subsequently, a second stage austempering was carried out by raising the temperature of the salt bath to 300 degrees C at an average heating rate of 0.5 degrees C/min, and the samples were kept in the salt bath for achieving a total austempering time of 120 min including the heating time. A conventional single-stage austempering was also conducted for comparison purposes, in which the austenitization temperature, the austempering temperatures and total time (stage I and stage II, i.e. 120 min) were kept the same for the benchmark samples. In the characterization studies, tensile test, hardness test, XRD analysis, optical microscope and field emission-scanning electron microscope (FE-SEM) equipped with EBSD detector were utilized. The findings of this study indicated that lowering the austempering temperature resulted in refining the structure with a decrease in the amount of austenite. According to the carbon content analysis through XRD patterns, the two-step austempering processes appeared to have considerably increased the carbon content of the austenite irrespective of austempering temperature. The best ultimate tensile strength (U.T.S) of 2194 MPa was achieved in the conventionally austempered sample at the lowest temperature of 250 degrees C, while the best yield strength (Y.S.) of 1753 MPa was reached in the stepped austempered sample initially at 250 degrees C followed by 300 degrees C. In general, two-step austempering process led to a higher yield strength while affecting the ultimate tensile strength and total elongation depending on the austempering temperature.
引用
收藏
页码:1331 / 1339
页数:9
相关论文
共 50 条
  • [21] Microstructure and Properties of a Low Carbon Bainitic Steel Produced by Conventional and Inverted Two-Step Austempering Processes
    Tian, Junyu
    Wang, Wei
    Xu, Guang
    Wang, Xiang
    Zhou, Mingxing
    Zurob, Hatem
    METALS AND MATERIALS INTERNATIONAL, 2023, 29 (05) : 1298 - 1310
  • [22] Effects of hot deformation and subsequent austempering on mechanical properties of high silicon and low silicon TRIP steel
    Li, Z.
    Wu, D.
    MATERIALS SCIENCE AND TECHNOLOGY, 2008, 24 (02) : 168 - 176
  • [23] MECHANICAL PROPERTIES OF A HIGH Si AND Mn STEEL HEAT TREATED BY TWO-STEP QUENCHING AND PARTITIONING
    Ghazvinloo, H. R.
    Honarbakhsh-Raouf, A.
    Kiani-Rashid, A. R.
    MATERIALS SCIENCE, 2018, 53 (04) : 481 - 487
  • [24] Mechanical Properties of a High Si and Mn Steel Heat Treated by Two-Step Quenching and Partitioning
    H. R. Ghazvinloo
    A. Honarbakhsh-Raouf
    A. R. Kiani-Rashid
    Materials Science, 2018, 53 : 481 - 487
  • [25] Microstructure and mechanical properties of austempered AISI 9255 high-silicon steel
    Acharya, Palaksha Pilar
    Udupa, Rajendra
    Bhat, Ravishankar
    MATERIALS SCIENCE AND TECHNOLOGY, 2018, 34 (03) : 355 - 365
  • [26] Effects of two-step austempering processes on the wear resistance and fatigue lifetime of high-carbon nanostructured bainitic steel
    Sun, Dongyun
    Feng, Xiaoyong
    Zhang, Peng
    Sun, Xiaowen
    Yang, Zhinan
    Long, Xiaoyan
    Zhang, Fucheng
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 30 : 4739 - 4749
  • [27] Effect of Two-Step Austempering Process on the Microstructure and Mechanical Properties of Low-Carbon Equivalent Austempered Ductile Iron
    Maddi, Lakshmiprasad
    Dakre, Vinayak
    Likhite, Ajay
    Pathak, Shailkumar
    SAE INTERNATIONAL JOURNAL OF MATERIALS AND MANUFACTURING, 2024, 17 (01) : 51 - 58
  • [28] Microstructure and mechanical properties of twostep Cu-alloyed ADI treated by different second step austempering temperatures and times
    Peng-yue Yi
    Er-jun Guo
    Li-ping Wang
    Yi-cheng Feng
    Chang-liang Wang
    ChinaFoundry, 2019, 16 (05) : 342 - 351
  • [29] Influence of PC-GTAW Parameters on the Microstructural and Mechanical Properties of Thin AISI 1008 Steel Joints
    Kumar, Ravindra
    Anant, Ramkishor
    Ghosh, P. K.
    Kumar, Ankit
    Agrawal, B. P.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2016, 25 (09) : 3756 - 3765
  • [30] Influence of PC-GTAW Parameters on the Microstructural and Mechanical Properties of Thin AISI 1008 Steel Joints
    Ravindra Kumar
    Ramkishor Anant
    P. K. Ghosh
    Ankit Kumar
    B. P. Agrawal
    Journal of Materials Engineering and Performance, 2016, 25 : 3756 - 3765