Microstructural evolution and mechanical properties of Ti-6Al-4V in situ alloyed with 3.5 wt.% Cu by laser powder bed fusion

被引:9
|
作者
Goettgens, Valerie Sue [1 ]
Kaserer, Lukas [1 ]
Braun, Jakob [1 ]
Busch, Richard [2 ]
Berthold, Lutz [2 ]
Patzig, Christian [2 ]
Leichtfried, Gerhard [1 ]
机构
[1] Univ Innsbruck, Fac Engn Sci, Dept Struct Engn & Mat Sci, Mat Technol, Tech Str 13, A-6020 Innsbruck, Austria
[2] Fraunhofer Inst Microstruct Mat & Syst IMWS, Walter Hulse Str 1, D-06120 Halle, Saale, Germany
关键词
Laser powder bed fusion; Additive manufacturing; Titanium alloy; Alloy design; TENSILE PROPERTIES; TITANIUM-ALLOY; FATIGUE RESISTANCE; HEAT-TREATMENT; MARTENSITE; DUCTILITY; ALPHA; DECOMPOSITION; IMPROVEMENT; BEHAVIOR;
D O I
10.1016/j.mtla.2023.101928
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The present work deals with the fabrication of Ti-6Al-4V in situ alloyed with 3.5 wt.% Cu (Ti-6Al-4V-3.5Cu), its microstructural evolution, and its related tensile properties. Specimens with a relative density of 99 +/- 0.1% presented a microstructure that differed from that of pure Ti-6Al-4V in LPBF, which usually exhibits a fully martensitic structure (alpha '). In Ti-6Al-4V-3.5Cu, apart from alpha-Ti, beta-Ti, and intermetallic Ti2Cu were also observed, generated by in situ martensite decomposition. Initially solidified large columnar beta-Ti grains underwent a martensitic transformation to alpha '. Cyclic reheating caused by layer-wise deposition during LPBF enabled the diffusion of Cu and V, allowing the transformation of alpha ' to stable alpha-Ti and the precipitation of beta-Ti and Ti2Cu. The alpha ' decomposition and formation of beta-Ti and Ti2Cu contributed to an UTS of 1362 +/- 14 MPa and an Rp0.2 of 1313 +/- 14 MPa in the horizontal specimen orientation in the as-built state. The elongation at fracture was 3.9 +/- 0.6%. In the vertical orientation, the specimens exhibited an UTS of 1305 +/- 19 MPa, an Rp0.2 of 1215 +/- 23 MPa, and an elongation at fracture of 5.4 +/- 1.5%. Stress-relief annealing reduced the UTS and Rp0.2 to 1099 +/- 6 MPa and 1014 +/- 5 MPa, respectively, with an increase in elongation at fracture to 6.7 +/- 0.4% in the horizontal specimen orientation. In the vertical specimen orientation, stress relief annealing resulted in an UTS of 1051 +/- 13 MPa and an Rp0.2 of 926 +/- 18 MPa. The elongation at fracture was increased to 11.3 +/- 1.3%.
引用
收藏
页数:11
相关论文
共 50 条
  • [31] The Influence of Iron in Minimizing the Microstructural Anisotropy of Ti-6Al-4V Produced by Laser Powder-Bed Fusion
    Simonelli, Marco
    McCartney, David Graham
    Barriobero-Vila, Pere
    Aboulkhair, Nesma T.
    Tse, Yau Yau
    Clare, Adam
    Hague, Richard
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2020, 51 (05): : 2444 - 2459
  • [32] Thermophysical properties of Ti-6Al-4V fabricated by powder bed fusion methods
    Hayun, Shmuel
    Strumza, Einat
    Landau, Peri
    Kimmel, Giora
    Ganor, Yaron, I
    Yeheskel, Ori
    ADDITIVE MANUFACTURING, 2022, 58
  • [33] Effect of powder recycling in laser-based powder bed fusion of Ti-6Al-4V
    Denti L.
    Sola A.
    Defanti S.
    Sciancalepore C.
    Bondioli F.
    Manufacturing Technology, 2019, 19 (02): : 190 - 196
  • [34] Microstructural evolution and mechanical properties of powder metallurgy Ti-6Al-4V alloy based on heat response
    Guo, Ruipeng
    Xu, Lei
    Wu, Jie
    Yang, Rui
    Zong, Bernie Y.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 639 : 327 - 334
  • [35] Laser surface polishing of Ti-6Al-4V parts manufactured by laser powder bed fusion
    Obeidi, Muhannad Ahmed
    Mussatto, Andre
    Dogu, Merve Nur
    Sreenilayam, Sithara P.
    McCarthy, Eanna
    Ul Ahad, Inam
    Keaveney, Shane
    Brabazon, Dermot
    SURFACE & COATINGS TECHNOLOGY, 2022, 434
  • [36] Coupling effects of microstructure and defects on the fatigue properties of laser powder bed fusion Ti-6Al-4V
    Qua, Z.
    Zhang, Z. J.
    Zhua, Y. K.
    Liu, R.
    Lu, S. L.
    Li, S. J.
    Duan, Q. Q.
    Zhang, B. N.
    Zhao, M. X.
    Eckert, J.
    Zhang, Z. F.
    ADDITIVE MANUFACTURING, 2023, 61
  • [37] Effect of layer thickness on spatter properties during laser powder bed fusion of Ti-6Al-4V
    Pauzon, Camille
    Raza, Ahmad
    Hanif, Imran
    Dubiez-Le Goff, Sophie
    Moverare, Johan
    Hryha, Eduard
    POWDER METALLURGY, 2023, 66 (04) : 333 - 342
  • [38] Fatigue properties of Ti-6Al-4V TPMS scaffolds fabricated via laser powder bed fusion
    Tilton, Maryam
    Borjali, Alireza
    Griffis, Jacklyn C.
    Varadarajan, Kartik Mangudi
    Manogharan, Guha P.
    MANUFACTURING LETTERS, 2023, 37 : 32 - 38
  • [39] Microstructural evolution and mechanical behaviour of laser welding Ti6Al4V fabricated by laser powder bed fusion and direct energy deposition
    Wu, Linkuo
    Liu, Ruizu
    Wang, Leilei
    Zhan, Xiaohong
    Wang, Zhimin
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2025, 30 (01) : 3 - 13
  • [40] Dynamic a globularization in laser powder bed fusion additively manufactured Ti-6Al-4V
    Chen, J.
    Fabijanic, D.
    Brandt, M.
    Zhao, Y.
    Ren, S. B.
    Xu, W.
    ACTA MATERIALIA, 2023, 255