Microstructural and Mechanical Behavior of Friction-Stir-Welded AA6061-T6 and AZ31 Alloys with Improved Electrochemical Corrosion

被引:9
|
作者
Singh, Virendra Pratap [1 ]
Kumar, Deepak [2 ,3 ]
Mahto, Raju Prasad [4 ]
Kuriachen, Basil [1 ,5 ]
机构
[1] Natl Inst Technol Mizoram, Dept Mech Engn, Aizawl 796012, India
[2] Indian Inst Technol Delhi, Dept Mat Sci & Engn, New Delhi 110016, India
[3] Carnegie Mellon Univ, Dept Mech Engn, Pittsburgh, PA 15213 USA
[4] Sardar Vallabhbhai Natl Inst Technol, Dept Mech Engn, Surat 395007, Gujrat, India
[5] Natl Inst Technol Calicut, Dept Mech Engn, Kozhikode 673601, Kerala, India
关键词
AA6061-T6; AZ31; cryo-Charpy impact test; EBSD; electrochemical corrosion friction stir welding; intermetallic compounds; mechanical properties; MAGNESIUM ALLOY; CONSTITUTIONAL LIQUATION; FRACTURE-BEHAVIOR; AQUEOUS-SOLUTIONS; ALUMINUM-ALLOY; MG ALLOYS; AL; JOINTS; PARAMETERS; EVOLUTION;
D O I
10.1007/s11665-022-07380-5
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effect of tool travel speed on the mechanical, microstructure and corrosion behavior of friction-stir-welded dissimilar AA6061-T6/AZ31 alloys has been characterized. Two different electrochemical techniques were studied in detail, i.e., potentiodynamic polarization test and electrochemical impedance spectroscopy at various pH values (i.e., pH = 2, pH = 7 and pH = 12) for all set of welded samples. Microstructural investigations were performed with the help of optical, SEM and EBSD microscopy techniques. The maximum corrosion rate (C-r) (29 mm/yr) at pH = 2 was obtained for sample A1 and minimum C-r (26 mm/yr) corresponding to sample A3, whereas, at pH = 12, maximum Cr (21 mm/yr) was obtained for sample A2 and minimum (19 mm/yr) was corresponding to sample A3. The cryo-Charpy impact test demonstrates the drop in values in all the cases with respect to room temperatures (25 degrees C), i.e., 16, 24 and 47% for sample A1, 19, 24 and 57% for sample A2, and 12, 33 and 36% for sample A3 at 0, - 20 and - 40 degrees C, respectively. The intermetallic compounds (IMCs) like Al12Mg17 and Al3Mg2 (before corrosion) and Mg(OH)(2) and Al(OH)(3) (after corrosion) were formed in the stir zone (SZ). The joint efficiency was 65, 84 and 91%, at different levels of welding speed, i.e., 16, 20 and 25 mm/min, respectively. The fracture analysis of tensile and cryo-Charpy impact toughness test was shown in both ductile and brittle fracture behavior.
引用
收藏
页码:4185 / 4204
页数:20
相关论文
共 50 条
  • [31] Influence of Interlayer Material on Softening and Wear Behavior of Friction Stir Welded AA6061-T6 alloy
    Nagu, Korra
    Satyanarayana, M. V. N. V.
    Harikrishna, K.
    Kumar, Adepu
    [J]. TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2023, 76 (12) : 3347 - 3355
  • [32] Mechanical Behavior and Microstructure of AA6061-T6 Joints Made by Friction Stir Vibration Welding
    Bagheri, Behrouz
    Abbasi, Mahmoud
    Dadaei, Mostafa
    [J]. JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (02) : 1165 - 1175
  • [33] Influence of Interlayer Material on Softening and Wear Behavior of Friction Stir Welded AA6061-T6 alloy
    Korra Nagu
    MVNV Satyanarayana
    K. Harikrishna
    Adepu Kumar
    [J]. Transactions of the Indian Institute of Metals, 2023, 76 : 3347 - 3355
  • [34] Material flow and mechanical properties of friction stir welded AA 5052-H32 and AA6061-T6 alloys with Sc interlayer
    Senthamaraikannan, Balamurugan
    Krishnamoorthy, Jayakumar
    [J]. MATERIALS TESTING, 2023, 65 (07) : 1127 - 1142
  • [35] Microstructure and Corrosion Behavior of Friction Stir-Welded 6061 Al/AZ31 Mg Joints with a Zr Interlayer
    Zheng, Yang
    Pan, Xiaomeng
    Ma, Yinglei
    Liu, Shuming
    Zang, Libin
    Chen, Yong
    [J]. MATERIALS, 2019, 12 (07):
  • [37] Microstructural analysis of friction stir welded Mg AZ31 alloy
    Gulati, Piyush
    Shukla, Dinesh Kumar
    Gupta, Akash
    Singh, Manpreet
    Kumar, Rajeev
    Singh, Jaiinder Preet
    [J]. MATERIALS TODAY-PROCEEDINGS, 2020, 26 : 1145 - 1150
  • [38] Mechanical Behavior and Microstructure of AA6061-T6 Joints Made by Friction Stir Vibration Welding
    Behrouz Bagheri
    Mahmoud Abbasi
    Mostafa Dadaei
    [J]. Journal of Materials Engineering and Performance, 2020, 29 : 1165 - 1175
  • [39] Influence of tool pin profile on mechanical and metallurgical behavior of friction stir welded AA6061-T6 and AA2017-T6 tailored blanks
    Battina, N. Malleswararao
    Vanthala, Varaha Siva Prasad
    Chirala, Hari Krishna
    [J]. ENGINEERING RESEARCH EXPRESS, 2021, 3 (03):
  • [40] The microstructures and mechanical properties of friction stir welded AZ31 with CaO Mg alloys
    Choi, Don-Hyun
    Kim, Shae-Kwang
    Jung, Seung-Boo
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2013, 554 : 162 - 168