Corrosion behaviour of the microbially modified surface of 5083 aluminium alloy

被引:6
|
作者
Nkoua, C. [1 ]
Josse, C. [2 ]
Proietti, A. [2 ]
Basseguy, R. [3 ]
Blanc, C. [1 ]
机构
[1] Univ Toulouse, CNRS, INP, ENSIACET,CIRIMAT, 4 Allee Emile Monso,CS 44362, F-31030 Toulouse 4, France
[2] Univ Toulouse, CNRS, INP, UPS,INSA,UAR Raimond Castaing, 3 Rue Caroline Aigle, F-31400 Toulouse, France
[3] Univ Toulouse, CNRS, INP, LGC,UPS, 4 Allee Emile Monso,CS 44362, F-31030 Toulouse 4, France
关键词
A; aluminium; intermetallics; B; polarization; C; pitting corrosion; microbiological corrosion; AL-MG ALLOYS; INTERMETALLIC PHASES; PERFORMANCE; AA5083;
D O I
10.1016/j.corsci.2022.110812
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The influence of microorganism-induced surface modifications on the corrosion behaviour of 5083 H11 aluminium alloy was studied. Pre-immersion in natural seawater (between 15 days and 2 months) led to the growth of a dense oxy-hydroxyde layer on the AA5083 surface. This layer led to a decrease in the cathodic and corrosion current densities, and an increase in the passivity domain on the polarisation curves plotted in chloride-containing sulphate solution for pre-immersed samples compared to bare samples. This improvement in the corrosion behaviour of AA5083 depended on the alloy microstructure, and the sunlight exposure during the pre-immersion in natural seawater.
引用
收藏
页数:16
相关论文
共 50 条
  • [1] Mechanical Properties and Corrosion Behaviour of MIG Welded 5083 Aluminium Alloy
    Durmus, Hulya
    MATERIALS TESTING, 2011, 53 (06) : 356 - 363
  • [2] Wear behaviour of 5083 wrought aluminium alloy under free corrosion conditions
    Panagopoulos, C. N.
    Georgiou, E. P.
    TRIBOLOGY-MATERIALS SURFACES & INTERFACES, 2007, 1 (03) : 161 - 164
  • [3] Pretreatment effects on the electrochemical responses for aluminium–magnesium alloy AA5083 corrosion behaviour
    Nacer Zazi
    Ahcène Bouabdallah
    Omar Aaboubi
    J.-P. Chopart
    Journal of Solid State Electrochemistry, 2010, 14 : 1705 - 1711
  • [4] Microstructure and corrosion behaviour of A356 aluminium alloy modified with Nd
    Arrabal, R.
    Mingo, B.
    Pardo, A.
    Mohedano, M.
    Matykina, E.
    Merino, M. C.
    Rivas, A.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2015, 66 (06): : 535 - 541
  • [5] The Effect of Cold Rolling on the Corrosion Behaviour of 5083 Aluminium Alloys
    Panagopoulos, C. N.
    Georgiou, E. P.
    METALS, 2024, 14 (02)
  • [6] Pretreatment effects on the electrochemical responses for aluminium-magnesium alloy AA5083 corrosion behaviour
    Zazi, Nacer
    Bouabdallah, Ahcene
    Aaboubi, Omar
    Chopart, J. -P.
    JOURNAL OF SOLID STATE ELECTROCHEMISTRY, 2010, 14 (09) : 1705 - 1711
  • [7] Thermomechanical treatments effect on corrosion behaviour of aluminium-magnesium alloy AA5083-H321
    Nacer Zazi
    Jean-Paul Chopart
    Ahcène Bouabdallah
    Protection of Metals and Physical Chemistry of Surfaces, 2015, 51 : 267 - 274
  • [8] Thermomechanical treatments effect on corrosion behaviour of aluminium-magnesium alloy AA5083-H321
    Zazi, Nacer
    Chopart, Jean-Paul
    Bouabdallah, Ahcene
    PROTECTION OF METALS AND PHYSICAL CHEMISTRY OF SURFACES, 2015, 51 (02) : 267 - 274
  • [9] Intergranular corrosion susceptibility of friction stir processed aluminium alloy 5083
    Vignesh, R. Vaira
    Padmanaban, R.
    MATERIALS TODAY-PROCEEDINGS, 2018, 5 (08) : 16443 - 16452
  • [10] ENHANCEMENT OF EXFOLIATION CORROSION RESISTANCE OF ALUMINIUM ALLOY 5083 BY SHOT PEENING
    Jebaraj, A. Vinoth
    Ajaykumar, L.
    Deepak, C. R.
    Aditya, K. V. V.
    SURFACE REVIEW AND LETTERS, 2018, 25 (07)