The Effect of Cold Rolling on the Corrosion Behaviour of 5083 Aluminium Alloys

被引:3
|
作者
Panagopoulos, C. N. [1 ]
Georgiou, E. P. [2 ]
机构
[1] Natl Tech Univ Athens, Lab Phys Met, Athens 15780, Greece
[2] Hellenic Air Force Acad, Fac Aerosp Studies, Athens 19005, Greece
关键词
aluminium alloys; cold rolling; corrosion; FILIFORM CORROSION; PITTING CORROSION; RESISTANCE; KINETICS;
D O I
10.3390/met14020159
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Aluminium-magnesium alloys find widespread application in diverse industrial and technological fields owing to their unique characteristics such as lightweight nature, favourable physical and mechanical properties, corrosion resistance and cost-effectiveness. During production, these alloys often undergo various forming processes that significantly affect the morphology and microstructure of their surface layers. Consequently, the surface properties, including corrosion resistance, are notably influenced by these treatments. In this study, the impact of cold rolling on the corrosion behaviour of the 5083 aluminium alloy, which is considered as an important alloy for the aerospace and naval industry, was investigated. The 5083 Al alloy underwent a cold-rolling process, resulting in specimens with reduced average thicknesses of 7% and 15%, respectively. The microstructure of the alloy was examined by using X-ray diffraction, optical and scanning electron microscopy techniques. Furthermore, the corrosion behaviour of both the as-received and cold-rolled aluminium alloy specimens was evaluated through potentiostatic and potentiodynamic corrosion measurements. The experimental results demonstrated that higher cold deformation percentages, within the specified experimental parameters, led to an enhanced corrosion resistance for the alloy. This improvement was primarily attributed to the reduction in grain size induced by recrystallization and to the formation of a passivating aluminium oxide film.
引用
收藏
页数:13
相关论文
共 50 条
  • [1] Cold rolling and lubricated wear of 5083 aluminium alloy
    Panagopoulos, C. N.
    Georgiou, E. P.
    MATERIALS & DESIGN, 2010, 31 (03): : 1050 - 1055
  • [2] Corrosion behaviour of the microbially modified surface of 5083 aluminium alloy
    Nkoua, C.
    Josse, C.
    Proietti, A.
    Basseguy, R.
    Blanc, C.
    CORROSION SCIENCE, 2023, 210
  • [3] Hot and Cold Rolling Behavior of AA5083 Aluminium Alloy
    Das, S.
    Meena, Shiwani
    Sarvesha, R.
    LIGHT METALS 2019, 2019, : 217 - 224
  • [4] Effect of chemical cleaning on the corrosion behaviour of painted aluminium alloys
    Fedrizzi, L
    Bianchi, A
    Deflorian, F
    Rossi, S
    Bonora, PL
    ELECTROCHIMICA ACTA, 2002, 47 (13-14) : 2159 - 2168
  • [5] LUBRICANTS FOR COLD ROLLING ALUMINIUM AND ITS ALLOYS
    SIMS, RO
    BUTLER, LH
    ALGER, JL
    STEET, WR
    WILCOX, RJ
    SINGER, ARE
    LUNN, B
    HERENGUEL, J
    HOURQUIN, MR
    KING, F
    GUMINSKI
    WILLIS
    SCHEY
    JOURNAL OF THE INSTITUTE OF METALS, 1961, 89 (09): : 297 - 303
  • [6] THE CONTROL OF QUALITY IN THE HOT AND COLD ROLLING OF ALUMINIUM AND ALUMINIUM ALLOYS
    KING, F
    TURNER, AN
    JOURNAL OF THE INSTITUTE OF METALS, 1954, 82 (07): : 291 - 306
  • [7] Effect of microstructure on the corrosion behaviour of extruded heat exchanger aluminium alloys
    Laferrere, A.
    Parson, N.
    Zhou, X.
    Thompson, G.
    SURFACE AND INTERFACE ANALYSIS, 2013, 45 (10) : 1597 - 1603
  • [8] Mechanical Properties and Corrosion Behaviour of MIG Welded 5083 Aluminium Alloy
    Durmus, Hulya
    MATERIALS TESTING, 2011, 53 (06) : 356 - 363
  • [9] DEVELOPMENT OF COLD-ROLLING LUBRICANTS FOR ALUMINIUM ALLOYS
    GUMINSKI, RD
    WILLIS, J
    JOURNAL OF THE INSTITUTE OF METALS, 1960, 88 (12): : 481 - 492
  • [10] DEFORMATIONS AND VELOCITIES DURING THE COLD ROLLING OF ALUMINIUM ALLOYS
    Misovic, Mitar
    Tadic, Nebojsa
    Jacimovic, Milojica
    Janjic, Mileta
    MATERIALI IN TEHNOLOGIJE, 2016, 50 (01): : 59 - 67