Using neutron diffraction to explore lithium displacement within cubic phase stabilised Ga-doped Li6.75La3Zr1.75Ta0.25O12 lithium garnet oxides

被引:1
|
作者
Christopher, Timothy Daniel [1 ,2 ]
Zhang, Tianhang [3 ,4 ]
Huang, Saifang [3 ,5 ]
Zujovic, Zoran [1 ,6 ]
Avdeev, Maxim [7 ,8 ]
Cao, Peng [2 ,3 ]
Sohnel, Tilo [1 ,2 ,3 ]
机构
[1] Univ Auckland, Ctr Green Chem Sci, Sch Chem Sci, Private Bag 92019, Auckland 1142, New Zealand
[2] Victoria Univ Wellington, MacDiarmid Inst Adv Mat & Nanotechnol, POB 600, Wellington 6140, New Zealand
[3] Univ Auckland, Dept Chem & Mat Engn, Private Bag 92019, Auckland 1142, New Zealand
[4] China Univ Geosci Beijing, Sch Mat Sci & Technol, Beijing Key Lab Mat Utilisat Nonmet Minerals & Sol, Natl Lab Mineral Mat, Beijing 100083, Peoples R China
[5] Jiangsu Univ Sci & Technol, Sch Mat Sci & Engn, Zhenjiang 212003, Peoples R China
[6] Univ Auckland, Fac Sci, NMR Ctr, Private Bag 92019, Auckland 1010, New Zealand
[7] Univ Sydney, Sch Chem, Sydney, NSW 2006, Australia
[8] Australian Nucl Sci & Technol Org, Lucas Heights, NSW 2234, Australia
关键词
Ceramics; Ionic conduction; Neutron diffraction; X-ray diffraction; LI-ION CONDUCTIVITY; LI7LA3ZR2O12; SOLID-ELECTROLYTE; AL; TA; DENSIFICATION; SUBSTITUTION; LI-7-XLA3ZR2-XTAXO12; ADDITIVES; BATTERY;
D O I
10.1016/j.jallcom.2023.172078
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Typical Li6.75La3Zr1.75Ta0.25O12 exists as a mixture of tetragonal and cubic arrangements, but adding small amounts of Ga3+ (Li6.75-3xGaxLa3Zr1.75Ta0.25O12 x >= 0.1) resulted in a single cubic (I a-3d) phase lithium garnet oxide. Following the stabilisation of the cubic phase, the effects on lithium distributions were explored with neutron powder diffraction concerning Ga3+ content and temperature. Increasing the amount of Ga3+ reduced the amount of lithium within the structure, directly decreasing the Li 96h site occupancy and showing a minimal effect on the Li 24d site occupancy. High-temperature neutron diffraction studies revealed the migration of lithium from the Li 24d site to the Li 96h with increasing temperature. The inclusion of Ga3+ improved the total ionic conductivity over the gallium-free system. However, with increasing gallium content (x > 0.1), a negative correlation between the garnet's gallium content and total lithium ionic conductivity is observed, showing how the total amount of free lithium ions impact the system's total ionic conductivity. Though the electrolytes explored here show some limitations, the lithium-ion displacement trends with doping and temperature give us further insight into how these lithium garnet systems respond to chemical and physical change.
引用
收藏
页数:11
相关论文
共 50 条
  • [21] Excellent Lithium Metal Anode Performance via In Situ Interfacial Layer Induced by Li6.75La3Zr1.75Ta0.25O12@Amorphous Li3OCl Composite Solid Electrolyte
    Tian, Yijun
    Ding, Fei
    Sang, Lin
    He, Yan-Bing
    Liu, Xingjiang
    Xu, Qiang
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2019, 14 (05): : 4781 - 4798
  • [22] Wide range lattice parameter control by aliovalent substitution to the rare-earth site in cubic garnet Li6.75(La1-xSmx)3Zr1.75Ta0.25O12
    Kawaguchi, Takahiko
    Sugihara, Ken
    Sakamoto, Naonori
    Suzuki, Hisao
    Wakiya, Naoki
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2020, 128 (10) : 700 - 705
  • [23] Synergistic Coupling between Li6.75La3Zr1.75Ta0.25O12 and Poly(vinylidene fluoride) Induces High Ionic Conductivity, Mechanical Strength, and Thermal Stability of Solid Composite Electrolytes
    Zhang, Xue
    Liu, Ting
    Zhang, Shuofeng
    Huang, Xin
    Xu, Bingqing
    Lin, Yuanhua
    Xu, Ben
    Li, Liangliang
    Nan, Ce-Wen
    Shen, Yang
    JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 2017, 139 (39) : 13779 - 13785
  • [24] Interface engineering of Li6.75La3Zr1.75Ta0.25O12via in situ built LiI/ZnLix mixed buffer layer for solid-state lithium metal batteries
    Zhai, Lei
    Wang, Jinhuan
    Zhang, Xiaoyu
    Zhou, Xunzhu
    Jiang, Fuyi
    Li, Lin
    Sun, Jianchao
    CHEMICAL SCIENCE, 2024, 15 (19) : 7144 - 7149
  • [25] 石榴石型立方相Li6.75La3Zr1.75Ta0.25O12复合固体电解质的锂电池性能研究
    刘亭
    佛山陶瓷, 2024, 34 (12) : 27 - 31
  • [26] Effect of Simultaneous Substitution of Y and Ta on the Stabilization of Cubic Phase, Microstructure, and Li+ Conductivity of Li7La3Zr2O12 Lithium Garnet
    Dhivya, L.
    Murugan, Ramaswamy
    ACS APPLIED MATERIALS & INTERFACES, 2014, 6 (20) : 17606 - 17615
  • [27] A highly ionic conductive poly(methyl methacrylate) composite electrolyte with garnet-typed Li6.75La3Zr1.75Nb0.25O12 nanowires
    Sun, Jianqi
    Li, Yaogang
    Zhang, Qinghong
    Hou, Chengyi
    Shi, Qiuwei
    Wang, Hongzhi
    CHEMICAL ENGINEERING JOURNAL, 2019, 375
  • [28] Versatile Strategy for Realizing Flexible Room-Temperature All-Solid-State Battery through a Synergistic Combination of Salt Affluent PEO and Li6.75La3Zr1.75Ta0.25O12 Nanofibers
    Fan, Rong
    Liu, Chen
    He, Kangqiang
    Cheng, Samson Ho-Sum
    Chen, Dazhu
    Liao, Chengzhu
    Li, Robert K. Y.
    Tang, Jiaoning
    Lu, Zhouguang
    ACS APPLIED MATERIALS & INTERFACES, 2020, 12 (06) : 7222 - 7231
  • [29] Two-step strategy to optimize interfacial compatibility of polyether sulfone-Li6.75La3Zr1.75Ta0.25O12 composite polymer electrolytes with Li anode for solid lithium battery with a wide working temperature range
    Lu, Zhengyi
    Liu, Changfei
    Wang, Enli
    Yang, Ruizhi
    Yang, Hongxun
    Jin, Chao
    JOURNAL OF POWER SOURCES, 2024, 596
  • [30] Stability of Nb-Doped Cubic Li7La3Zr2O12 with Lithium Metal
    Ishiguro, K.
    Nakata, Y.
    Matsui, M.
    Uechi, I.
    Takeda, Y.
    Yamamoto, O.
    Imanishi, N.
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2013, 160 (10) : A1690 - A1693