The Effect of a Deproteinizing Pretreatment on the Bonding Performance and Acid Resistance of a Two-step Self-etch Adhesive on Eroded Dentin

被引:2
|
作者
Yang, Y. [1 ]
Inoue, G. [1 ,7 ]
Hosaka, K. [2 ]
Tichy, A. [1 ,3 ,4 ]
Ikeda, M. [5 ]
Tagami, J. [6 ]
Shimada, Y. [1 ,3 ]
机构
[1] Tokyo Med & Dent Univ, Grad Sch Med & Dent Sci, Dept Cariol & Operat Dent, Tokyo, Japan
[2] Tokushima Univ, Grad Sch Biomed Sci, Dept Regenerat Dent Med, Tokushima, Japan
[3] Charles Univ Prague, Fac Med 1, Inst Dent Med, Prague, Czech Republic
[4] Gen Univ Hosp Prague, Prague, Czech Republic
[5] Tokyo Med & Dent Univ, Grad Sch Med & Dent Sci, Dept Oral Prosthet Engn, Tokyo, Japan
[6] Chulalongkorn Univ, Fac Dent, Dept Operat Dent, Bangkok, Thailand
[7] 1-5-45 Yushima,Bunkyo Ku, Tokyo 1138549, Japan
关键词
HYPOCHLOROUS ACID; INTERFACE; STRENGTH; EROSION; LAYER; ZONE; ULTRASTRUCTURE; POLYMERIZATION; DURABILITY; STABILITY;
D O I
10.2341/23-005-L
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives: This study evaluated how deproteinization using sodium hypochlorite (6% NaOCl) or hypochlorous acid (50 ppm HOCl) with or without the subsequent use of an arylsulfinate salt -containing agent (Clearfil DC Activator; DCA; Kuraray Noritake Dental) affects the micro -tensile bond strength (mu TBS) and formation of an acidbase resistant zone (ABRZ) of a two-step self -etch adhesive on eroded dentin. Methods: Coronal dentin surfaces of sound human molars were exposed to 48 cycles of demineralization (1% citric acid; 5 minutes) and remineralization (buffer solution with pH=6.4; 3.5 hours). They were then assigned to experimental groups according to the pretreatment used: none (negative control), NaOCl, NaOCl+DCA, HOCl, and HOCl+DCA. Sound dentin surfaces with no pretreatment were used as a positive control. The dentin surfaces were bonded with Clearfil SE Bond 2 (Kuraray Noritake Dental), and mu TBS was measured either after 24 hours or 20,000 thermal cycles (TC). The mu TBS data were statistically analyzed using a mixed -model analysis of variance (ANOVA) and t -tests with Bonferroni correction. Failure mode was determined with scanning electron microscopy (SEM), which was also used for the observation of ABRZ. Results: Among experimental groups, there was no significant difference between the negative control, HOCl, and HOCl+DCA after 24 hours, but the HOCl-pretreated groups exhibited significantly higher mu TBS than the negative control after TC (p<0.01). Pretreatment with NaOCl and NaOCl+DCA resulted in significantly higher mu TBS (p<0.001), but the highest mu TBS was measured on sound dentin (p<0.001). TC decreased mu TBS significantly in all groups (p<0.001) except for sound dentin and NaOCl+DCA (p>0.05). Adhesive failures prevailed in eroded groups, whereas cohesive failures were predominant on sound dentin. ABRZ was recognized in all groups but marked morphological differences were observed. Conclusions: The combined use of 6% NaOCl and the arylsulfinate salt -containing agent partially reversed the compromised bonding performance on eroded dentin, while the effect of 50 ppm HOCl was negligible.
引用
收藏
页码:65 / 75
页数:11
相关论文
共 50 条
  • [41] A Randomized Clinical Evaluation of a One- and Two-step Self-etch Adhesive Over 24 Months
    Loguercio, A. D.
    Manica, D.
    Ferneda, F.
    Zander-Grande, C.
    Amaral, R.
    Stanislawczuk, R.
    Carvalho, R. M.
    Manso, A.
    Reis, A.
    OPERATIVE DENTISTRY, 2010, 35 (03) : 265 - 272
  • [42] Microleakage assessment of one- and two-step self-etch adhesive systems with the low shrinkage composites
    Hoseinifar, Razieh
    Kermanshah, Hamid
    JOURNAL OF ORAL HEALTH AND ORAL EPIDEMIOLOGY, 2015, 4 (02): : 71 - 79
  • [43] SHORT-AND LONG-TERM BOND STRENGTHS OF A GOLD STANDARD TWO-STEP SELF-ETCH ADHESIVE SYSTEM TO DENTIN: A PRELIMINARY STUDY
    Tuncer, Safa
    Tekce, Neslihan
    Pashaev, Dial
    Demirci, Mustafa
    Baydemir, Canan
    JOURNAL OF ISTANBUL UNIVERSITY FACULTY OF DENTISTRY, 2015, 49 (02) : 1 - 7
  • [44] Effect of Bur Roughness on Bond to Sclerotic Dentin With Self-etch Adhesive Systems
    Luque-Martinez, I. V.
    Mena-Serrano, A.
    Munoz, M. A.
    Hass, V.
    Reis, A.
    Loguercio, A. D.
    OPERATIVE DENTISTRY, 2013, 38 (01) : 39 - 47
  • [45] Antibacterial effect of a brominated self-etch adhesive on carious dentin - An in vivo study
    Schmidt, Jana
    Krohn, Sandra
    Kallies, Rene
    Schneider, Hartmut
    Zeller, Katharina
    Ziebolz, Dirk
    Berg, Thomas
    Haak, Rainer
    JOURNAL OF DENTISTRY, 2021, 105
  • [46] High intensity focused ultrasound enhances bonding of universal adhesive to dentin in self-etch mode
    Fu, Cheryl
    Awad, Mohamed M.
    Bridgwood, Jackie
    Boon, Sarah
    Hashimi, Masooma
    Clode, Peta L.
    Fawzy, Amr S.
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2025, 138
  • [47] Effects of photocuring strategy on bonding of dual-cure one-step self-etch adhesive to root canal dentin
    Aksornmuang, Juthatip
    Nakajima, Masatoshi
    Panyayong, Woraphong
    Tagami, Junji
    DENTAL MATERIALS JOURNAL, 2009, 28 (02) : 133 - 141
  • [48] Comparison of enamel bond fatigue durability of universal adhesives and two-step self-etch adhesives in self-etch mode
    Tsujimoto, Akimasa
    Barkmeier, Wayne W.
    Hosoya, Yumiko
    Nojiri, Kie
    Nagura, Yuko
    Takamizawa, Toshiki
    Latta, Mark A.
    Miyazaki, Masashi
    AMERICAN JOURNAL OF DENTISTRY, 2017, 30 (05): : 279 - 284
  • [49] Dimethyl Sulfoxide Dentin Pretreatments Do Not Improve Bonding of a Universal Adhesive in Etch-and-Rinse or Self-etch Modes
    Magalhaes de Mello, Rodrigo Mafra
    Roquim Alcantara, Barbara Albertini
    Gomes Franca, Fabiana Mantovani
    Botelho do Amaral, Flavia Lucisano
    Basting, Roberta Tarkany
    JOURNAL OF ADHESIVE DENTISTRY, 2022, 24 (01): : 49 - 56
  • [50] Influence of orthodontic self-etch adhesive on acid resistance of surface enamel
    Nakazawa, Yuki
    Suzuki, Shoichi
    Inoue, Go
    Nikaido, Toru
    Tagami, Junji
    Moriyama, Keiji
    DENTAL MATERIALS JOURNAL, 2018, 37 (04) : 568 - 574