High intensity focused ultrasound enhances bonding of universal adhesive to dentin in self-etch mode

被引:0
|
作者
机构
[1] Fu, Cheryl
[2] Awad, Mohamed M.
[3] Bridgwood, Jackie
[4] Boon, Sarah
[5] Hashimi, Masooma
[6] Clode, Peta L.
[7] Fawzy, Amr S.
基金
澳大利亚国家健康与医学研究理事会;
关键词
Atomic emission spectroscopy - Bond strength (chemical) - Bond strength (materials) - Etching - Fracture energy - High resolution transmission electron microscopy - Hydroelasticity - Laser power transmission - Strain rate - Ultrasonic applications;
D O I
10.1016/j.ijadhadh.2024.103901
中图分类号
学科分类号
摘要
Objective: To investigate the effect of high intensity focused ultrasound (HIFU) exposure on enhancing the bonding of universal adhesives, in self-etch mode, to dentin. To achieve this aim, the effects of HIFU exposure on dentin micro-topography, structure, and nanoscale mechanical and chemical properties were investigated. In addition, resin-dentin interfacial morphology and micro-tensile bond strength (μTBS) were evaluated. Methods: The effect of HIFU exposure at 5, 15, or 30W at varying time intervals (30–120 s) on the dentin surface properties were characterised by scanning electron microscopy (SEM), atomic force microscopy (AFM), Raman spectroscopy, and nano-indentation testing. The interfacial junctions between Scotchbond universal adhesive, in self-etch mode, and HIFU-treated dentin were characterised using confocal laser scanning microscopy (CLSM) and transmission electron microscopy (TEM). Furthermore, μTBS tests were conducted before and after thermocycling. Results: HIFU exposure at 30W for 120 s resulted in almost complete removal of the smear layer. HIFU treatment at 15W for 60 and 90 s, and at 30W for 60 s significantly increased dentin surface roughness. Raman analysis indicated progressive mineral removal at higher HIFU power levels. HIFU treatment at 5, 15, and 30W did not significantly affect dentin reduced elastic-modulus and nano-hardness. Following HIFU application at 30W for 120 s, CLSM examination indicated marked increase in adhesive penetration. HIFU exposure for 120 s at 30 W was effective in removing the overlying smear layer facilitating partial demineralisation of the underlying superficial dentin substrate. Whilst HIFU treatment did not improve the immediate μTBS of Scotchbond universal adhesive in self-etch mode, 120 s HIFU treatment at 30W significantly improved the aged μTBS values compared to the control. Significance: HIFU treatment of dentin surface at 30W for 120 s enhanced the structural integrity of resin-dentin interfacial junctions and the μTBS, after thermocycling, of a mild universal adhesive applied in self-etch mode. © 2024 The Authors
引用
收藏
相关论文
共 50 条
  • [1] Etch-and-rinse vs self-etch mode for dentin bonding effectiveness of universal adhesives
    Yamauchi, Kabun
    Tsujimoto, Akimasa
    Jurado, Carlos A.
    Shimatani, Yusuke
    Nagura, Yuko
    Takamizawa, Toshiki
    Barkmeier, Wayne W.
    Latta, Mark A.
    Miyazaki, Masashi
    JOURNAL OF ORAL SCIENCE, 2019, 61 (04) : 549 - 553
  • [2] Dimethyl Sulfoxide Dentin Pretreatments Do Not Improve Bonding of a Universal Adhesive in Etch-and-Rinse or Self-etch Modes
    Magalhaes de Mello, Rodrigo Mafra
    Roquim Alcantara, Barbara Albertini
    Gomes Franca, Fabiana Mantovani
    Botelho do Amaral, Flavia Lucisano
    Basting, Roberta Tarkany
    JOURNAL OF ADHESIVE DENTISTRY, 2022, 24 (01): : 49 - 56
  • [3] Bonding Performance of Universal Adhesive Systems Applied in Etch-and-Rinse and Self-Etch Strategies on Natural Dentin Caries
    Hass, V
    Cardenas, A. F. M.
    Siqueira, F. S. F.
    Pacheco, R. R.
    Zago, P. M. W.
    Silva, D. O.
    Bandeca, M. C.
    Loguercio, A. D.
    OPERATIVE DENTISTRY, 2019, 44 (05) : 510 - 520
  • [4] Self-etch or etch-and-rinse mode did not affect the microshear bond strength of a universal adhesive to primary dentin
    Thanaratikul, Benjaporn
    Santiwong, Busayarat
    Harnirattisai, Choltacha
    DENTAL MATERIALS JOURNAL, 2016, 35 (02) : 174 - 179
  • [5] Influence of pretreatments on microtensile bond strength to eroded dentin using a universal adhesive in self-etch mode
    Hartz, Julia J.
    Keller, Sarina P.
    Taubock, Tobias T.
    Attin, Thomas
    Wegehaupt, Florian J.
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2022, 114
  • [6] Bond durability of universal adhesive to bovine enamel using self-etch mode
    Suzuki, Soshi
    Takamizawa, Toshiki
    Imai, Arisa
    Tsujimoto, Akimasa
    Sai, Keiichi
    Takimoto, Masayuki
    Barkmeier, Wayne W.
    Latta, Mark A.
    Miyazaki, Masashi
    CLINICAL ORAL INVESTIGATIONS, 2018, 22 (03) : 1113 - 1122
  • [7] Bond durability of universal adhesive to bovine enamel using self-etch mode
    Soshi Suzuki
    Toshiki Takamizawa
    Arisa Imai
    Akimasa Tsujimoto
    Keiichi Sai
    Masayuki Takimoto
    Wayne W. Barkmeier
    Mark A. Latta
    Masashi Miyazaki
    Clinical Oral Investigations, 2018, 22 : 1113 - 1122
  • [8] Bonding Performance of Universal Adhesives Applied to Nano-Hydroxyapatite Desensitized Dentin Using Etch-and-Rinse or Self-Etch Mode
    Meng, Yuchen
    Huang, Fan
    Wang, Silin
    Li, Meiwen
    Lu, Yi
    Pei, Dandan
    Li, Ang
    MATERIALS, 2021, 14 (16)
  • [9] Effects of adhesive application time and air blowing pressure on dentin bond strength of self-etch mode universal adhesives
    Karalar, Buket
    Bayindir, Yusuf Ziya
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2022, 36 (03) : 287 - 301
  • [10] Bonding effectiveness of a total-etch and self-etch adhesive to Er:YAG lased enamel and dentin.
    De Munck, J
    Van Meerbeck, B
    Yudhira, RT
    Lambrechts, P
    Vanherle, G
    JOURNAL OF DENTAL RESEARCH, 2002, 81 : B280 - B280