Mechanism of primary Si and Fe-segregation for a hypereutectic 90 wt.% Si-Ti alloy melt in directional solidification via electromagnetism

被引:3
|
作者
Zhu, Kui-song [1 ]
Cao, Li [1 ]
Zhao, Ying-tao [1 ]
Wang, Jun [1 ]
Cheng, Xiang-kui [1 ]
机构
[1] Panzhihua Univ, Coll Vanadium & Titanium, Panzhihua 617000, Sichuan, Peoples R China
关键词
High silicon Si-Ti alloy; Primary Si; Electromagnetic directional solidification; Si enriched layer; Impurity segregation; BEARING; SEPARATION; KINETICS; SLAG;
D O I
10.1007/s42243-023-00925-5
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The electromagnetic directional solidification (DS) phase separation experiments of high silicon 90 wt.% Si-Ti alloy were performed under various pulling-down speeds. The results showed that Si enriched layer, Si + TiSi2-rich layer and Si-Ti-Fe alloy layer appeared successively in axial direction of ingot after electromagnetic DS of 90 wt.% Si-Ti alloy melt at different pulling-down speeds. Separation of primary Si and segregation mechanism of metal impurities (Fe) during the electromagnetic DS process were controlled by pulling-down speed of ingot and electromagnetic stirring. When pulling-down speed was 5 mu m/s, minimum thickness of the Si enriched layer was 29.4 mm, and the highest content of primary Si in this layer was 92.46 wt.%; meanwhile, the highest removal rate of Fe as metal impurity was 92.90%. The type of inclusions in the Si enriched layer is determined by Fe content of segregated Si enriched layer. When the pulling-down speed was 5 mu m/s, the inclusions in the Si enriched layer were TiSi2. Finally, when the pulling-down speed reached greater than 5 mu m/s, the inclusions in the Si enriched layer evolved into TiSi2 + tau(5).
引用
收藏
页码:726 / 735
页数:10
相关论文
共 44 条
  • [41] Modification of Hypereutectic Al-20wt%Si Alloy Based on the Addition of Yttrium and Al-5Ti-1B Modifiers Mixing Melt
    Li, Qinglin
    Li, Binqiang
    Liu, Jianjun
    Li, Jinbao
    Liu, Dexue
    Lan, Yefeng
    Xia, Tiandong
    INTERNATIONAL JOURNAL OF METALCASTING, 2019, 13 (02) : 367 - 383
  • [42] Effect of Al-P-Ti-TiC-Nd2O3 modifier on the microstructure and mechanical properties of hypereutectic Al-20 wt. %Si alloy
    Xu, C. L.
    Wang, H. Y.
    Yang, Y. F.
    Jiang, Q. C.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 452 : 341 - 346
  • [43] On the growth mechanism of the primary silicon particle in a hypereutectic Al-20 wt% Si alloy using synchrotron X-ray tomography
    Wang, J.
    Guo, Z.
    Song, J. L.
    Hu, W. X.
    Li, J. C.
    Xiong, S. M.
    MATERIALS & DESIGN, 2018, 137 : 176 - 183
  • [44] Mechanism of boron removal of primary Si phases and morphology evolution of impurity phases during slow cooling solidification refining of Al-30wt.%Si alloy with Zr additions
    Chen, Chen
    Ban, Boyuan
    Sun, Jifei
    Li, Jingwei
    Jiang, Xuesong
    Shi, Jian
    Chen, Jian
    Jia, Jianbo
    Sakiani, Hassan
    Tabaian, Seyed Hadi
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 860 (860)