Mechanism of primary Si and Fe-segregation for a hypereutectic 90 wt.% Si-Ti alloy melt in directional solidification via electromagnetism

被引:3
|
作者
Zhu, Kui-song [1 ]
Cao, Li [1 ]
Zhao, Ying-tao [1 ]
Wang, Jun [1 ]
Cheng, Xiang-kui [1 ]
机构
[1] Panzhihua Univ, Coll Vanadium & Titanium, Panzhihua 617000, Sichuan, Peoples R China
关键词
High silicon Si-Ti alloy; Primary Si; Electromagnetic directional solidification; Si enriched layer; Impurity segregation; BEARING; SEPARATION; KINETICS; SLAG;
D O I
10.1007/s42243-023-00925-5
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The electromagnetic directional solidification (DS) phase separation experiments of high silicon 90 wt.% Si-Ti alloy were performed under various pulling-down speeds. The results showed that Si enriched layer, Si + TiSi2-rich layer and Si-Ti-Fe alloy layer appeared successively in axial direction of ingot after electromagnetic DS of 90 wt.% Si-Ti alloy melt at different pulling-down speeds. Separation of primary Si and segregation mechanism of metal impurities (Fe) during the electromagnetic DS process were controlled by pulling-down speed of ingot and electromagnetic stirring. When pulling-down speed was 5 mu m/s, minimum thickness of the Si enriched layer was 29.4 mm, and the highest content of primary Si in this layer was 92.46 wt.%; meanwhile, the highest removal rate of Fe as metal impurity was 92.90%. The type of inclusions in the Si enriched layer is determined by Fe content of segregated Si enriched layer. When the pulling-down speed was 5 mu m/s, the inclusions in the Si enriched layer were TiSi2. Finally, when the pulling-down speed reached greater than 5 mu m/s, the inclusions in the Si enriched layer evolved into TiSi2 + tau(5).
引用
收藏
页码:726 / 735
页数:10
相关论文
共 44 条
  • [31] Effect of Ce on solute redistribution in liquid ahead of solid–liquid interface during solidification of Fe–4 wt.%Si alloy
    Yun-ping Ji
    Ming-xing Zhang
    Yuan Hou
    Tong-xin Zhao
    Yi-ming Li
    Hui-ping Ren
    Journal of Iron and Steel Research International, 2021, 28 : 1251 - 1258
  • [32] PRIMARY SILICON SEGREGATION DURING ISOTHERMAL HOLDING OF HYPEREUTECTIC AL-18.3 WT-PERCENT-SI ALLOY IN THE FREEZING RANGE
    LIANG, D
    BAYRAKTAR, Y
    MOIR, SA
    BARKHUDAROV, M
    JONES, H
    SCRIPTA METALLURGICA ET MATERIALIA, 1994, 31 (04): : 363 - 367
  • [33] Effect of Fe and Si on the Phase Composition and Microstructure Evolution in Al-2 wt.% Cu-2 wt.% Mn Alloy During Solidification, Cold Rolling and Annealing
    Belov, N. A.
    Akopyan, T. K.
    Korotkova, N. O.
    Cherkasov, S. O.
    Yakovleva, A. O.
    JOM, 2021, 73 (12) : 3827 - 3837
  • [34] Simulation of a directional solidification of a binary Al-7wt%Si and a ternary alloy Al-7wt%Si-1wt%Fe under the action of a rotating magnetic field
    Budenkova, O.
    Baltaretu, F.
    Kovacs, J.
    Roosz, A.
    Ronafoeldi, A.
    Bianchi, A-M
    Fautrelle, Y.
    MCWASP XIII: INTERNATIONAL CONFERENCE ON MODELING OF CASTING, WELDING AND ADVANCED SOLIDIFICATION PROCESSES, 2012, 33
  • [35] Effect of Fe and Si on the Phase Composition and Microstructure Evolution in Al-2 wt.% Cu-2 wt.% Mn Alloy During Solidification, Cold Rolling and Annealing
    N. A. Belov
    T. K. Akopyan
    N. O. Korotkova
    S. O. Cherkasov
    A. O. Yakovleva
    JOM, 2021, 73 : 3827 - 3837
  • [36] Primary silicon formation in hypereutectic alloy Al-16.5% wt. Si treated in the liquid state by a changing unipolar pulsed electric current
    Prigunova, A. G.
    Koshelev, M. V.
    Borisov, A. G.
    MATERIALS SCIENCE AND TECHNOLOGY, 2024,
  • [37] Microstructural evolution during annealing of the melt-spun ternary hypoeutectic Al-7.6Si-3.3Fe (in wt.%) alloy
    Ünlü, N
    Genç, A
    Öveçoglu, ML
    Lavernia, EJ
    Froes, FH
    JOURNAL OF ALLOYS AND COMPOUNDS, 2002, 343 (1-2) : 223 - 233
  • [38] Effect of a transverse weak magnetic field on the texture evolution and magnetic property of Fe-1.0 wt.% Si alloy during bulk solidification
    Liu, Chummei
    Zhong, Yunbo
    Shen, Zhe
    Dong, Licheng
    Zheng, Tianxiang
    Ren, Weili
    Lei, Zuosheng
    Ren, Zhongming
    MATERIALS RESEARCH EXPRESS, 2019, 6 (06)
  • [39] Effect of Ce on solute redistribution in liquid ahead of solid-liquid interface during solidification of Fe-4 wt.%Si alloy
    Ji, Yun-ping
    Zhang, Ming-xing
    Hou, Yuan
    Zhao, Tong-xin
    Li, Yi-ming
    Ren, Hui-ping
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2021, 28 (10) : 1251 - 1258
  • [40] Modification of Hypereutectic Al–20 wt%Si Alloy Based on the Addition of Yttrium and Al–5Ti–1B Modifiers Mixing Melt
    Qinglin Li
    Binqiang Li
    Jianjun Liu
    Jinbao Li
    Dexue Liu
    Yefeng Lan
    Tiandong Xia
    International Journal of Metalcasting, 2019, 13 : 367 - 383