Combinatorial Effects of the Recipes of the Initial Gas-atomized Powder Sizes on Microstructure and Passivation Characteristics of the SLM-ed Ti-6Al-4V Bulk Alloys

被引:1
|
作者
Zhang, Yu [1 ]
Lei, Jiazhuo [1 ]
Dan, Zhenhua [1 ]
Chang, Hui [1 ]
Zhou, Lian [1 ]
机构
[1] Nanjing Tech Univ, Tech Inst Adv Mat, Coll Mat Sci & Engn, 5 Xinmofan Rd, Nanjing 211816, Peoples R China
来源
MATERIALS SCIENCE-MEDZIAGOTYRA | 2023年 / 29卷 / 02期
基金
中国国家自然科学基金;
关键词
gas-atomized Ti-6Al-4V powders; combinatorial recipe of powders; selective laser melting; electrochemical properties; passive films; CORROSION BEHAVIOR; HEAT-TREATMENT; ELECTROCHEMICAL-BEHAVIOR; MECHANICAL-PROPERTIES; TI6AL4V; TITANIUM; EVOLUTION; RESISTANCE; FATIGUE;
D O I
10.5755/j02.ms.31220
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Bulk Ti-6Al-4V alloys have been fabricated by selective laser melting (SLM) in three recipes with different combinations of powder sizes. Combinatorial effects of initial gas-atomized powder sizes on microstructure and corrosion properties of SLM-ed Ti-6Al-4V alloys have been investigated by optical microscopy, X-ray diffraction, electrochemical measurements and surface free energy. The SLM-ed Ti-6Al-4V alloys are composed of acicular & alpha;' martensite and & alpha; phases. Many pinhole defects and twin boundaries exist in the SLM-ed Ti-6Al-4V alloys. According to electrochemical tests and surface free energy calculation, the SLM-ed Ti-6Al-4V alloys with 0 - 53 & mu;m powders have the most positive corrosion potential, the lowest current density and the smallest surface free energy of 20.89 mJ m2. The passive film of SLM-ed Ti-6Al-4V alloys with 0 - 53 & mu;m powders has superior protection ability due to their large thickness. The carrier concentration of SLM-ed Ti-6Al-4V alloys with 0 - 53 & mu;m powders is the lowest by the Mott-Schottky curves. The SLM-ed samples with contact angles higher than 90o are hydrophobic, but the small contact angle of 46.98o reflects the hydrophilic features of as-rolled Ti-6Al-4V alloys. The combinatorial recipe of SLM-ed Ti-6Al-4V alloys with 0 - 53 & mu;m powders is optimal for improvements on the passivation and corrosion resistance.
引用
收藏
页码:176 / 185
页数:10
相关论文
共 45 条
  • [41] The effects of specimens geometry on solidification conditions and microstructure formation in laser powder bed fusion fabricated Ti–6Al–4V alloys
    Zhao, Rijie
    Kou, Ronghui
    Wang, Haoliang
    Song, Chenghao
    Li, Chuan
    Sun, Zhenzhong
    Journal of Materials Research and Technology, 2024, 33 : 5030 - 5039
  • [42] Fatigue of additive manufactured Ti-6Al-4V, Part I: The effects of powder feedstock, manufacturing, and post-process conditions on the resulting microstructure and defects
    Pegues, J. W.
    Shao, S.
    Shamsaei, N.
    Sanaei, N.
    Fatemi, A.
    Warner, D. H.
    Li, P.
    Phan, N.
    INTERNATIONAL JOURNAL OF FATIGUE, 2020, 132
  • [43] Influence of non-equilibrium solidification of melt pools and annealing on microstructure formation and mechanical properties of laser powder bed fusion-built Ti-6Al-4V alloys
    Zhao, Rijie
    Yan, Xingchen
    Wang, Haoliang
    Song, Chenghao
    Li, Chuan
    Mao, Lei
    Liu, Min
    Gao, Jianrong
    Sun, Zhenzhong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 873
  • [44] Arc Characteristics and Weld Bead Microstructure of Ti-6Al-4V Titanium Alloy in Ultra-high Frequency Pulse Gas Tungsten Arc Welding (UHFP-GTAW) Process
    Li, Wei
    Lv, Gaochong
    Wang, Qiang
    Huang, Songtao
    MATERIALS SCIENCE-MEDZIAGOTYRA, 2020, 26 (04): : 426 - 431
  • [45] Effects of Y2O3 addition on the microstructure and wear-resistant performance of TiN/TiB-reinforced Ti-based laser-clad coatings on Ti-6Al-4V alloys
    Wang, Lixin
    Yang, Lijun
    Huang, Yiming
    Yuan, Yuxue
    Jia, Chenpeng
    MATERIALS TODAY COMMUNICATIONS, 2021, 29