Combinatorial Effects of the Recipes of the Initial Gas-atomized Powder Sizes on Microstructure and Passivation Characteristics of the SLM-ed Ti-6Al-4V Bulk Alloys

被引:1
|
作者
Zhang, Yu [1 ]
Lei, Jiazhuo [1 ]
Dan, Zhenhua [1 ]
Chang, Hui [1 ]
Zhou, Lian [1 ]
机构
[1] Nanjing Tech Univ, Tech Inst Adv Mat, Coll Mat Sci & Engn, 5 Xinmofan Rd, Nanjing 211816, Peoples R China
来源
MATERIALS SCIENCE-MEDZIAGOTYRA | 2023年 / 29卷 / 02期
基金
中国国家自然科学基金;
关键词
gas-atomized Ti-6Al-4V powders; combinatorial recipe of powders; selective laser melting; electrochemical properties; passive films; CORROSION BEHAVIOR; HEAT-TREATMENT; ELECTROCHEMICAL-BEHAVIOR; MECHANICAL-PROPERTIES; TI6AL4V; TITANIUM; EVOLUTION; RESISTANCE; FATIGUE;
D O I
10.5755/j02.ms.31220
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Bulk Ti-6Al-4V alloys have been fabricated by selective laser melting (SLM) in three recipes with different combinations of powder sizes. Combinatorial effects of initial gas-atomized powder sizes on microstructure and corrosion properties of SLM-ed Ti-6Al-4V alloys have been investigated by optical microscopy, X-ray diffraction, electrochemical measurements and surface free energy. The SLM-ed Ti-6Al-4V alloys are composed of acicular & alpha;' martensite and & alpha; phases. Many pinhole defects and twin boundaries exist in the SLM-ed Ti-6Al-4V alloys. According to electrochemical tests and surface free energy calculation, the SLM-ed Ti-6Al-4V alloys with 0 - 53 & mu;m powders have the most positive corrosion potential, the lowest current density and the smallest surface free energy of 20.89 mJ m2. The passive film of SLM-ed Ti-6Al-4V alloys with 0 - 53 & mu;m powders has superior protection ability due to their large thickness. The carrier concentration of SLM-ed Ti-6Al-4V alloys with 0 - 53 & mu;m powders is the lowest by the Mott-Schottky curves. The SLM-ed samples with contact angles higher than 90o are hydrophobic, but the small contact angle of 46.98o reflects the hydrophilic features of as-rolled Ti-6Al-4V alloys. The combinatorial recipe of SLM-ed Ti-6Al-4V alloys with 0 - 53 & mu;m powders is optimal for improvements on the passivation and corrosion resistance.
引用
收藏
页码:176 / 185
页数:10
相关论文
共 45 条
  • [31] Spall Microstructure Characteristics and Fracture Mechanism of Ti-6Al-4V and Ti-47Nb Alloys under Dynamic High-pressure Loading
    动高压加载条件下Ti-6Al-4V和Ti-47Nb合金 层裂微结构特征与断裂机理
    Yu, Xiaodong (yuxiaodong.bit@163.com), 2018, Science Press (47):
  • [32] Increasing the productivity of laser powder bed fusion: Influence of the hull-bulk strategy on part quality, microstructure and mechanical performance of Ti-6Al-4V
    de Formanoir, Charlotte
    Paggi, Umberto
    Colebrants, Thomas
    Thijs, Lore
    Li, Guichuan
    Vanmeensel, Kim
    Van Hooreweder, Brecht
    ADDITIVE MANUFACTURING, 2020, 33 (33)
  • [33] Effects of local processing parameters on microstructure, texture, and mechanical properties of electron beam powder bed fusion manufactured Ti-6Al-4V
    Schwalbach, Edwin J.
    Benzing, Jake T.
    Sinha, Vikas
    Butler, Todd M.
    Pilchak, Adam L.
    Chaput, Kevin J.
    Schehl, Norman D.
    John, Reji
    Hrabe, Nikolas
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 855
  • [34] Heat-treatment effects on mechanical properties and microstructure evolution of Ti-6Al-4V alloy fabricated by laser powder bed fusion
    Tsai, Min-Tsang
    Chen, Yi-Wen
    Chao, Chih-Yeh
    Jang, Jason S. C.
    Tsai, Chih-Ching
    Su, Yu-Lun
    Kuo, Che-Nan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 816
  • [35] The Effects of Geometry Size and Initial Microstructure on Deformation Behavior of Electrically-Assisted Micro-Compression in Ti-6Al-4V Alloy
    Bao, Jianxing
    Lv, Shoudan
    Wang, Bo
    Shan, Debin
    Guo, Bin
    Xu, Jie
    MATERIALS, 2022, 15 (05)
  • [36] Comparison study on microstructure and mechanical properties of Ti-6Al-4V alloys fabricated by powder-based selective-laser-melting and sintering methods
    Yan, Q.
    Chen, B.
    Kang, N.
    Lin, X.
    Lv, S.
    Kondoh, K.
    Li, S.
    Li, J. S.
    MATERIALS CHARACTERIZATION, 2020, 164
  • [37] The effects of heat treatment and carbon content on the microstructure and mechanical properties of laser powder bed fusion Ti-6Al-4V with dissolved TiC particles
    Peterson, Jack
    Issariyapat, Ammarueda
    Umeda, Junko
    Kondoh, Katsuyoshi
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 920
  • [38] Bonding pressure effects on characteristics of microstructure, mechanical properties, and mass diffusivity of Ti-6Al-4V and TiAlNb diffusion-bonded joints
    Kundu, J.
    Chakraborty, A.
    Kundu, S.
    WELDING IN THE WORLD, 2020, 64 (12) : 2129 - 2143
  • [39] Bonding pressure effects on characteristics of microstructure, mechanical properties, and mass diffusivity of Ti-6Al-4V and TiAlNb diffusion-bonded joints
    J. Kundu
    A. Chakraborty
    S. Kundu
    Welding in the World, 2020, 64 : 2129 - 2143
  • [40] Effects of Lamellar Microstructure Characteristics on Quasi-static and Dynamic Deformation Behavior of Ti-6Al-4V-4Zr-Mo Alloys
    Huo Dongmei
    Li Shukui
    Fan Qunbo
    RARE METAL MATERIALS AND ENGINEERING, 2013, 42 (03) : 457 - 461