Fracture resistance of CAD/CAM blocks cemented on dentin using different cementation strategies

被引:7
|
作者
Anuntasainont, Munlika [1 ]
Po-ngam, Nanthiphorn [1 ]
Luhrs, Anne-Katrin [2 ]
Neoh, Siew Peng [3 ]
Pongprueksa, Pong [1 ]
机构
[1] Mahidol Univ, Fac Dent, Dept Operat Dent & Endodont, Nakhon Pathom, Thailand
[2] Hannover Med Sch, Dept Conservat Dent, Periodontol & Prevent Dent, Hannover, Germany
[3] Mahidol Univ, Fac Dent, Dept Orthodont, Nakhon Pathom, Thailand
关键词
Cemented composite; Light-curing adhesive; Fracture resistance; Curing mode; Cement type; BOND STRENGTH; RESIN CEMENTS; COMPOSITE CEMENTS; PART; ADHESIVE; CONVERSION; RELIABILITY; CROWNS;
D O I
10.2186/jpr.JPR_D_22_00196
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose: To determine whether the fracture resistance of computer-aided design/computer-aided manufacturing (CAD/ CAM) resin-based composites and polymer-infiltrated ceramic network materials cemented on dentin is influenced by the restoration thickness and composite cement application strategy.Methods: Disc-shaped specimens (O = 7 mm) of 0.8 mm and 1.5 mm thicknesses were milled from two CAD/CAM materials: resin-based composite (RBC, Cerasmart 270) and polymer-infiltrated ceramic network (PICN, Vita Enamic). The discs (n = 8 per group) were cemented on flattened dentin using three different cementation strategies: 1) self-adhesive composite cement (RelyX U200) in light-curing mode (LC-SAC), 2) universal adhesive (Single Bond Universal) with composite cement (RelyX Ultimate) in auto-curing mode (AC cement), and 3) adhesive and composite cement as in 2) but in light-curing mode (LC cement). The restorative surface was indented perpendicularly with a compressive load using a universal testing machine until fracture. The fracture resistance (N) of RBC and PICN was separately analyzed using two-way ANOVA andResults: The fracture resistance of each material was significantly influenced by the material thickness and cementation strategy (P < 0.05). Irrespective of the material type and cementation strategy, thicker materials exhibit higher fracture resistance. For RBC, the fracture resistance of the LC cement group was significantly higher than that of AC cement only at 0.8 mm thickness. For PICN, the LC-cement cementation strategy produced superior fracture resistance, regardless of the restoration thickness.Conclusions: The fracture resistance of Cerasmart 270 was higher for the thicker material; the fracture resistance of LC cement was higher than that of AC cement at 0.8 mm thickness cemented to dentin. In comparison, LC cement showed the highest fracture resistance for Vita Enamic for both material thicknesses.
引用
收藏
页码:603 / 609
页数:7
相关论文
共 50 条
  • [31] Fracture resistance of CAD/CAM endocrowns made from different materials in maxillary premolar interproximal defects
    Fuqian Jin
    Xiaoyan Yu
    Haolin Zhou
    Jin Zhou
    Jing Yang
    Yi Luo
    Zhu Chen
    Clinical Oral Investigations, 28
  • [32] Long-term tensile bond strength of differently cemented nanocomposite CAD/CAM crowns on dentin abutment
    Stawarczyk, Bogna
    Stich, Nicola
    Eichberger, Marlis
    Edelhoff, Daniel
    Roos, Malgorzata
    Gernet, Wolfgang
    Keul, Christine
    DENTAL MATERIALS, 2014, 30 (03) : 334 - 342
  • [33] Gloss and Stain Resistance of Ceramic-Polymer CAD/CAM Restorative Blocks
    Lawson, Nathaniel C.
    Burgess, John O.
    JOURNAL OF ESTHETIC AND RESTORATIVE DENTISTRY, 2016, 28 : S40 - S45
  • [34] Shear bond strength vs interfacial fracture toughness - Adherence to CAD/CAM blocks
    Ilie, Nicoleta
    Ruse, N. Dorin
    DENTAL MATERIALS, 2019, 35 (12) : 1769 - 1775
  • [35] Fracture Resistance of Molar Crowns Fabricated with Monolithic All-Ceramic CAD/CAM Materials Cemented on Titanium Abutments: An In Vitro Study
    Dogan, Derya Ozdemir
    Gorler, Oguzhan
    Mutaf, Burcu
    Ozcan, Mutlu
    Eyuboglu, Gunes Bulut
    Ulgey, Melih
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2017, 26 (04): : 309 - 314
  • [36] In Vitro Analysis of the Fracture Resistance of CAD/CAM Denture Base Resins
    Steinmassl, Otto
    Offermanns, Vincent
    Stoeckl, Wolfgang
    Dumfahrt, Herbert
    Grunert, Ingrid
    Steinmassl, Patricia-Anca
    MATERIALS, 2018, 11 (03):
  • [37] Bonding ability of resin cements to different types of CAD/CAM composite blocks
    Takahashi, Nao
    Kurokawa, Hiroyasu
    Wakamatsu, Kengo
    Hirokane, Eizo
    Takamizawa, Toshiki
    Miyazaki, Masashi
    Kitahara, Nobuya
    DENTAL MATERIALS JOURNAL, 2022, 41 (01) : 134 - 141
  • [38] Comparative Study of the Influence of Heat Treatment on Fracture Resistance of Different Ceramic Materials Used for CAD/CAM Systems
    Balladares, Andrea Ordonez
    Abad-Coronel, Cristian
    Ramos, Joao Carlos
    Fajardo, Jorge I.
    Paltan, Cesar A.
    Biedma, Benjamin Jose Martin
    MATERIALS, 2024, 17 (06)
  • [39] Fracture resistance and failure modes of endocrowns manufactured with different CAD/CAM materials under axial and lateral loading
    El Ghoul, Wiam
    Ozcan, Mutlu
    Silwadi, Munir
    Salameh, Ziad
    JOURNAL OF ESTHETIC AND RESTORATIVE DENTISTRY, 2019, 31 (04) : 378 - 387
  • [40] In vitro analysis of the fracture resistance of CAD-CAM monolithic zirconia molar crowns with different occlusal thickness
    Sorrentino, Roberto
    Triulzio, Clementina
    Tricarico, Maria Gabriella
    Bonadeo, Giovanni
    Gherlone, Enrico Felice
    Ferrari, Marco
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2016, 61 : 328 - 333