Fracture resistance and failure modes of endocrowns manufactured with different CAD/CAM materials under axial and lateral loading

被引:49
|
作者
El Ghoul, Wiam [1 ]
Ozcan, Mutlu [2 ]
Silwadi, Munir [1 ]
Salameh, Ziad [1 ]
机构
[1] Lebanese Univ, Fac Med Dent, Dept Prosthodont, Beirut, Lebanon
[2] Univ Zurich, Ctr Dent & Oral Med, Div Dent Biomat, Zurich, Switzerland
关键词
axial loading; CAD; CAM; Endocrown; fracture resistance; glass-ceramic; lateral loading; resin nano-ceramic; ENDODONTICALLY-TREATED TEETH; LITHIUM DISILICATE; RESTORATIONS; STRENGTH; SURVIVAL; RESIN; BEHAVIOR; CROWNS; POSTS; TOOTH;
D O I
10.1111/jerd.12486
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives The purpose of this in vitro study was to evaluate the fracture resistance and failure modes of endocrowns made of three computer-aided design/computer-aided manufacturing (CAD/CAM) materials subjected to thermo-mechanical cycling loading. Materials and Methods Eighty mandibular molars were divided into four groups (n = 20): one (C E) was restored with lithium disilicate glass-ceramic conventional crowns, three were restored with endocrowns made of three different CAD/CAM materials; (E E) lithium disilicate glass-ceramic, (E V) zirconia-reinforced lithium silicate glass-ceramic, and (E C) resin nano-ceramic. After cycling loading, half of the samples from each group were loaded axially and the other half was loaded laterally. Fracture resistance was recorded in Newton (N) and failure modes were classified. Two-way ANOVA, Bonferroni post hoc (alpha = .05), Chi-square, and multiple logistic regression tests were used to analyze data. Results Statistically significant interaction were recorded between fracture resistance (N) and loading (P < .001), and groups (conventuional crown and endocrowns; P < .001). Endocrowns presented higher fracture strength than conventional crowns. Fracture resistance was significantly larger under axial loading. The numbers of irreparable failures were extremely important in the endocrowns groups (Groups E E, E V, E C), and only conventional crowns (Group C E) showed almost no irreparable failures under axial loading. Conclusion Lithium disilicate glass-ceramic recorded the highest fracture resistance under axial and lateral loading. Clinical Significance The number of irreparable failures with all endocrown materials tested do not suggest yet the use of this type of restorations in posterior teeth.
引用
收藏
页码:378 / 387
页数:10
相关论文
共 50 条
  • [1] The fracture strength of endocrowns manufactured from different hybrid blocks under axial and lateral forces
    Acar, Duygu Hazal
    Kalyoncuoglu, Elif
    CLINICAL ORAL INVESTIGATIONS, 2021, 25 (04) : 1889 - 1897
  • [2] The fracture strength of endocrowns manufactured from different hybrid blocks under axial and lateral forces
    Duygu Hazal Acar
    Elif Kalyoncuoğlu
    Clinical Oral Investigations, 2021, 25 : 1889 - 1897
  • [3] Fracture resistance of CAD/CAM endocrowns made from different materials in maxillary premolar interproximal defects
    Fuqian Jin
    Xiaoyan Yu
    Haolin Zhou
    Jin Zhou
    Jing Yang
    Yi Luo
    Zhu Chen
    Clinical Oral Investigations, 28
  • [4] Fracture resistance of CAD/CAM endocrowns made from different materials in maxillary premolar interproximal defects
    Jin, Fuqian
    Yu, Xiaoyan
    Zhou, Haolin
    Zhou, Jin
    Yang, Jing
    Luo, Yi
    Chen, Zhu
    CLINICAL ORAL INVESTIGATIONS, 2024, 28 (04)
  • [5] Fracture resistance of endocrowns made from different CAD/CAM materials after prolonged fatigue aging
    Dincturk, B. Arslandas
    Garoushi, Sufyan
    Alp, C. Kedici
    Vallittu, Pk
    Uctasli, M. B.
    Lassila, L.
    CLINICAL ORAL INVESTIGATIONS, 2025, 29 (03)
  • [6] The Effect of Different Materials and Techniques on Stress Distribution in CAD/CAM Endocrowns
    Eskitascioglu, M.
    Kucuk, O.
    Eskitascioglu, G.
    Eraslan, O.
    Belli, S.
    STRENGTH OF MATERIALS, 2020, 52 (05) : 812 - 819
  • [7] The Effect of Different Materials and Techniques on Stress Distribution in CAD/CAM Endocrowns
    M. Eskitaşçioğlu
    O. Küçük
    G. Eskitaşçioğlu
    O. Eraslan
    S. Belli
    Strength of Materials, 2020, 52 : 812 - 819
  • [8] Fracture Resistance and Microleakage of Endocrowns Utilizing Three CAD-CAM Blocks
    El-Damanhoury, H. M.
    Haj-Ali, R. N.
    Platt, J. A.
    OPERATIVE DENTISTRY, 2015, 40 (02) : 201 - 210
  • [9] Fracture Resistance and Failure Modes of Lithium Disilicate or Composite Endocrowns
    Altier, M.
    Erol, F.
    Yildirim, G.
    Dalkilic, E. E.
    NIGERIAN JOURNAL OF CLINICAL PRACTICE, 2018, 21 (07) : 821 - 826
  • [10] Load capacity of occlusal veneers of different restorative CAD/CAM materials under lateral static loading
    Zamzam, Hadiel
    Olivares, Antonio
    Fok, Alex
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2021, 115