Fracture resistance and failure modes of endocrowns manufactured with different CAD/CAM materials under axial and lateral loading

被引:49
|
作者
El Ghoul, Wiam [1 ]
Ozcan, Mutlu [2 ]
Silwadi, Munir [1 ]
Salameh, Ziad [1 ]
机构
[1] Lebanese Univ, Fac Med Dent, Dept Prosthodont, Beirut, Lebanon
[2] Univ Zurich, Ctr Dent & Oral Med, Div Dent Biomat, Zurich, Switzerland
关键词
axial loading; CAD; CAM; Endocrown; fracture resistance; glass-ceramic; lateral loading; resin nano-ceramic; ENDODONTICALLY-TREATED TEETH; LITHIUM DISILICATE; RESTORATIONS; STRENGTH; SURVIVAL; RESIN; BEHAVIOR; CROWNS; POSTS; TOOTH;
D O I
10.1111/jerd.12486
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives The purpose of this in vitro study was to evaluate the fracture resistance and failure modes of endocrowns made of three computer-aided design/computer-aided manufacturing (CAD/CAM) materials subjected to thermo-mechanical cycling loading. Materials and Methods Eighty mandibular molars were divided into four groups (n = 20): one (C E) was restored with lithium disilicate glass-ceramic conventional crowns, three were restored with endocrowns made of three different CAD/CAM materials; (E E) lithium disilicate glass-ceramic, (E V) zirconia-reinforced lithium silicate glass-ceramic, and (E C) resin nano-ceramic. After cycling loading, half of the samples from each group were loaded axially and the other half was loaded laterally. Fracture resistance was recorded in Newton (N) and failure modes were classified. Two-way ANOVA, Bonferroni post hoc (alpha = .05), Chi-square, and multiple logistic regression tests were used to analyze data. Results Statistically significant interaction were recorded between fracture resistance (N) and loading (P < .001), and groups (conventuional crown and endocrowns; P < .001). Endocrowns presented higher fracture strength than conventional crowns. Fracture resistance was significantly larger under axial loading. The numbers of irreparable failures were extremely important in the endocrowns groups (Groups E E, E V, E C), and only conventional crowns (Group C E) showed almost no irreparable failures under axial loading. Conclusion Lithium disilicate glass-ceramic recorded the highest fracture resistance under axial and lateral loading. Clinical Significance The number of irreparable failures with all endocrown materials tested do not suggest yet the use of this type of restorations in posterior teeth.
引用
收藏
页码:378 / 387
页数:10
相关论文
共 50 条
  • [41] Wear resistance of crowns made from different CAM/CAD materials
    Wille, Sebastian
    Sieper, Kim
    Kern, Matthias
    DENTAL MATERIALS, 2021, 37 (07) : E407 - E413
  • [42] Comparative Study of the Influence of Heat Treatment on Fracture Resistance of Different Ceramic Materials Used for CAD/CAM Systems
    Balladares, Andrea Ordonez
    Abad-Coronel, Cristian
    Ramos, Joao Carlos
    Fajardo, Jorge I.
    Paltan, Cesar A.
    Biedma, Benjamin Jose Martin
    MATERIALS, 2024, 17 (06)
  • [43] Collapse Resistance of Steel Columns under Combined Axial and Lateral Loading
    Fogarty, J.
    El-Tawil, S.
    JOURNAL OF STRUCTURAL ENGINEERING, 2016, 142 (01)
  • [44] Fracture toughness of chairside CAD/CAM materials - Alternative loading approach for compact tension test
    Badawy, Rania
    El-Mowafy, Omar
    Tam, Laura E.
    DENTAL MATERIALS, 2016, 32 (07) : 847 - 852
  • [45] Evaluation of the fracture resistance and failure types of different CAD-CAM ceramic crowns supported by angled titanium abutments
    Yuksel, Merve
    Saygin, Aysegul Goze
    Bolayir, Giray
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2023, 32 (07): : 594 - 601
  • [46] Comparative Analysis of Fracture Resistance between CAD/CAM Materials for Interim Fixed Prosthesis
    Abad-Coronel, Cristian
    Carrera, Elena
    Mena Cordova, Nancy
    Fajardo, Jorge I.
    Aliaga, Paulina
    MATERIALS, 2021, 14 (24)
  • [47] Fracture of β-SiC bulk with a void of different shapes under different loading modes
    Wang, Liang
    Yu, Wenshan
    Shen, Shengping
    ENGINEERING FRACTURE MECHANICS, 2017, 181 : 29 - 37
  • [48] Fracture strengths of endocrown restorations fabricated with different preparation depths and CAD/CAM materials
    Kanat-Erturk, Burcu
    Saridag, Serkan
    Koseler, Ege
    Helvacioglu-Yigit, Dilek
    Avcu, Egemen
    Yildiran-Avcu, Yasemin
    DENTAL MATERIALS JOURNAL, 2018, 37 (02) : 256 - 265
  • [49] Fracture resistance of CAD/CAM blocks cemented on dentin using different cementation strategies
    Anuntasainont, Munlika
    Po-ngam, Nanthiphorn
    Luhrs, Anne-Katrin
    Neoh, Siew Peng
    Pongprueksa, Pong
    JOURNAL OF PROSTHODONTIC RESEARCH, 2023, 67 (04) : 603 - 609
  • [50] Effect of Differences in Axial Thickness and Type of Cement on Fracture Resistance in Composite Resin CAD/CAM Crowns
    Masuda, Tomotoshi
    Nomoto, Syuntaro
    Sato, Toru
    Kanda, Yuuhei
    Sakai, Takanori
    Tsuyuki, Yu
    BULLETIN OF TOKYO DENTAL COLLEGE, 2019, 60 (01): : 17 - 27