Toward extended durability and power output of high temperature proton exchange membrane fuel cells with Gd2Zr2O7-C3N4 composite membrane

被引:0
|
作者
Vinothkannan, Mohanraj [1 ,2 ]
Gikunoo, Edzordzi Kwame [1 ]
Shanmugam, Sangaraju [1 ]
机构
[1] Daegu Gyeongbuk Inst Sci & Technol DGIST, Dept Energy Sci & Engn, 50-1,Sang Ri, Daegu 42988, South Korea
[2] Coventry Univ, Ctr Adv Low Carbon Prop Syst C ALPS, Ctr Emobil & Clean Growth, Coventry CV1 2TL, England
基金
新加坡国家研究基金会;
关键词
Sulfonated poly(ether ether ketone); GdZr-CN; HT-PEMFC; Chemical durability; Operational stability; POLYMER ELECTROLYTE MEMBRANES; OXIDE NANOCOMPOSITE MEMBRANE; LOW HUMIDITY; CHEMICAL DURABILITY; CARBON NANOTUBES; HYBRID MEMBRANE; SPEEK MEMBRANE; NAFION; CONDUCTIVITY; OPERATION;
D O I
10.1007/s11581-025-06120-8
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
State-of-the-art proton exchange membrane fuel cell (PEMFC) that operate at 80 degrees C and 100% relative humidity (RH) requires an external humidifier, noble electrocatalyst, and expensive Nafion membrane to obtain appreciable power output and durability. High temperature (HT) operation over 100 degrees C provides an ideal solution to avoid costly components in PEMFC application. However, HT-PEMFC frequently loses its performance excessively because of phosphoric acid leaching from the conventional polybenzimidazole-based membranes. Herein, we present a gadolinium zirconium oxide (Gd2Zr2O7)-carbon nitride (C3N4) (GdZr-CN) additive that reasonably improves the power output, chemical durability, and operational stability of sulfonated poly(ether ether ketone) (SPEEK) membrane in HT-PEMFC. When use SPEEK/GdZr-CN composite membrane in HT-PEMFC, the metal cations (Zr4+ and Gd3+) decompose the free radicals, while the acid-base interactions between functional groups (-SO3H, -NH, -NH2, and -OH) involve the anhydrous proton conduction. Using SPEEK/GdZr-CN composite membrane, we obtain a HT-PEMFC exhibiting a maximal power output of 315 mW cm-2 at 110 degrees C under 15% RH, with minimal chemical degradation after 300 h of operation. Although the incorporation of GdZr-CN significantly enhances the durability of the composite membrane by scavenging free radicals and increasing glass transition temperature, the minimal degradation observed is primarily attributed to the inherent vulnerability of ether linkages in SPEEK backbones to free radical attacks and hygrothermal stress during prolonged operation. This study unveils that SPEEK/GdZr-CN composite membrane is a cost-competitive, energy-efficient, and durable PEM from the perspective of HT-PEMFC.
引用
收藏
页数:12
相关论文
共 50 条
  • [31] Synthesis and Properties of Polysilsesquioxane Functionalized Poly(p-terphenyl-co-N-methyl-4-piperidine) Membrane for High Temperature Proton Exchange Membrane Fuel Cells
    Wang, Lele
    Wang, Ting
    Wang, Qian
    Wang, Jin
    Yang, Jingshuai
    ADVANCED SUSTAINABLE SYSTEMS, 2024, 8 (11):
  • [32] SSH2S: Hydrogen storage in complex hydrides for an auxiliary power unit based on high temperature proton exchange membrane fuel cells
    Baricco, Marcello
    Bang, Mads
    Fichtner, Maximilian
    Hauback, Bjorn
    Linder, Marc
    Luetto, Carlo
    Moretto, Pietro
    Sgroi, Mauro
    JOURNAL OF POWER SOURCES, 2017, 342 : 853 - 860
  • [33] Development of Nafion®/SiO2/phosphotunstic acid nanocomposite membranes for high temperature proton exchange membrane fuel cells
    Liu, YX
    Kunz, HR
    Fenton, JM
    Zhu, L
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2005, 230 : U3700 - U3700
  • [34] Pt/CeO2 Cocatalyst and porogen enhance performance of high-temperature proton exchange membrane fuel cells
    Huang, Chaoran
    Yan, Jie
    Wang, Xueyao
    Gao, Zeren
    Ma, Ding
    Zheng, Junrong
    JOURNAL OF POWER SOURCES, 2025, 629
  • [35] Fabrication of α-Si3N4-nanowire/γ-Y2Si2O7 composite superhydrophobic membrane for membrane distillation
    Yang, Ming-Ye
    Dong, Bin-Bin
    Wang, Fei-Hong
    Xu, Xin
    Agathopoulos, Simeon
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2019, 16 (06) : 2173 - 2180
  • [36] Structurally modulated and functionalized carbon nanotubes as potential filler for Nafion matrix toward improved power output and durability in proton exchange membrane fuel cells operating at reduced relative humidity
    Vinothkannan, Mohanraj
    Kim, Ae Rhan
    Ryu, Sung Kwan
    Yoo, Dong Jin
    JOURNAL OF MEMBRANE SCIENCE, 2022, 649
  • [37] The Solid-Phase Synthesis of an Fe-N-C Electrocatalyst for High-Power Proton-Exchange Membrane Fuel Cells
    Liu, Qingtao
    Liu, Xiaofang
    Zheng, Lirong
    Shui, Jianglan
    ANGEWANDTE CHEMIE-INTERNATIONAL EDITION, 2018, 57 (05) : 1204 - 1208
  • [38] N,N-bis(sulfopropyl)aminyl-4-phenyl polysulfone and O,O′-bis(sulfopropyl)resorcinol-5-yl-4-phenyl polysulfone composite membrane for proton exchange membrane fuel cells
    Pan, Ting
    Yue, Baohua
    Yan, Liuming
    Zeng, Guangbo
    Hu, Yidong
    He, Shufa
    Lu, Wei
    Zhao, Hongbin
    Zhang, Jiujun
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2020, 45 (43) : 23490 - 23503
  • [39] A novel H3PO4/Nafion-PBI composite membrane for enhanced durability of high temperature PEM fuel cells
    Zhai, Yunfeng
    Zhang, Huamin
    Zhang, Yu
    Xing, Danmin
    JOURNAL OF POWER SOURCES, 2007, 169 (02) : 259 - 264
  • [40] Degradation Studies of Single Cell and Short Stack for High Temperature Proton Exchange Membrane Fuel Cells Based on PBI/H3PO4 Membrane
    Sun, Xuejing
    Li, Yinhua
    Qi, Fulai
    Jing, Fenning
    Sun, Hai
    Sun, Gongquan
    CHEMISTRYSELECT, 2019, 4 (42): : 12313 - 12319