Toward extended durability and power output of high temperature proton exchange membrane fuel cells with Gd2Zr2O7-C3N4 composite membrane

被引:0
|
作者
Vinothkannan, Mohanraj [1 ,2 ]
Gikunoo, Edzordzi Kwame [1 ]
Shanmugam, Sangaraju [1 ]
机构
[1] Daegu Gyeongbuk Inst Sci & Technol DGIST, Dept Energy Sci & Engn, 50-1,Sang Ri, Daegu 42988, South Korea
[2] Coventry Univ, Ctr Adv Low Carbon Prop Syst C ALPS, Ctr Emobil & Clean Growth, Coventry CV1 2TL, England
基金
新加坡国家研究基金会;
关键词
Sulfonated poly(ether ether ketone); GdZr-CN; HT-PEMFC; Chemical durability; Operational stability; POLYMER ELECTROLYTE MEMBRANES; OXIDE NANOCOMPOSITE MEMBRANE; LOW HUMIDITY; CHEMICAL DURABILITY; CARBON NANOTUBES; HYBRID MEMBRANE; SPEEK MEMBRANE; NAFION; CONDUCTIVITY; OPERATION;
D O I
10.1007/s11581-025-06120-8
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
State-of-the-art proton exchange membrane fuel cell (PEMFC) that operate at 80 degrees C and 100% relative humidity (RH) requires an external humidifier, noble electrocatalyst, and expensive Nafion membrane to obtain appreciable power output and durability. High temperature (HT) operation over 100 degrees C provides an ideal solution to avoid costly components in PEMFC application. However, HT-PEMFC frequently loses its performance excessively because of phosphoric acid leaching from the conventional polybenzimidazole-based membranes. Herein, we present a gadolinium zirconium oxide (Gd2Zr2O7)-carbon nitride (C3N4) (GdZr-CN) additive that reasonably improves the power output, chemical durability, and operational stability of sulfonated poly(ether ether ketone) (SPEEK) membrane in HT-PEMFC. When use SPEEK/GdZr-CN composite membrane in HT-PEMFC, the metal cations (Zr4+ and Gd3+) decompose the free radicals, while the acid-base interactions between functional groups (-SO3H, -NH, -NH2, and -OH) involve the anhydrous proton conduction. Using SPEEK/GdZr-CN composite membrane, we obtain a HT-PEMFC exhibiting a maximal power output of 315 mW cm-2 at 110 degrees C under 15% RH, with minimal chemical degradation after 300 h of operation. Although the incorporation of GdZr-CN significantly enhances the durability of the composite membrane by scavenging free radicals and increasing glass transition temperature, the minimal degradation observed is primarily attributed to the inherent vulnerability of ether linkages in SPEEK backbones to free radical attacks and hygrothermal stress during prolonged operation. This study unveils that SPEEK/GdZr-CN composite membrane is a cost-competitive, energy-efficient, and durable PEM from the perspective of HT-PEMFC.
引用
收藏
页数:12
相关论文
共 50 条
  • [21] Development of non-noble Co-N-C electrocatalyst for high-temperature proton exchange membrane fuel cells
    Eren, Enis Oguzhan
    Ozkan, Necati
    Devrim, Yilser
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2020, 45 (58) : 33957 - 33967
  • [22] Defective g-C3N4 optimizes phosphate distribution in the catalytic layer and boosts the performance of high-temperature proton exchange membrane fuel cells
    Zhang, Dongcai
    Kong, Zhijie
    Huang, Gen
    Du, Shiqian
    Lin, Jiaqi
    Wang, Yanyong
    Yu, Gang
    Tao, Li
    Wang, Shuangyin
    SCIENCE CHINA-MATERIALS, 2023, 66 (09) : 3468 - 3474
  • [23] High temperature polymer electrolyte membrane fuel cells with Polybenzimidazole-Ce0.9Gd0.1P2O7 and polybenzimidazole-Ce0.9Gd0.1P2O7-graphite oxide composite electrolytes
    Singh, Bhupendra
    Devi, Nitika
    Srivastava, Avanish Kumar
    Singh, Rajesh K.
    Song, Sun-Ju
    Krishnan, N. Nambi
    Konovalova, Anastasiia
    Henkensmeier, Dirk
    JOURNAL OF POWER SOURCES, 2018, 401 : 149 - 157
  • [24] Seizing gaseous Fe2+ to densify O2-accessible Fe-N4 sites for high-performance proton exchange membrane fuel cells
    Yin, Shu-Hu
    Yang, Shuang-Li
    Li, Gen
    Li, Guang
    Zhang, Bin-Wei
    Wang, Chong-Tai
    Chen, Ming-Shu
    Liao, Hong-Gang
    Yang, Jian
    Jiang, Yan-Xia
    Sun, Shi-Gang
    ENERGY & ENVIRONMENTAL SCIENCE, 2022, 15 (07) : 3033 - 3040
  • [25] Porous gC3N4-Gd2Zr2O7 enables the high-temperature operation of Nafion membranes in polymer electrolyte fuel cells over 500 hours
    Vinothkannan, Mohanraj
    Son, Byungrak
    Shanmugam, Sangaraju
    JOURNAL OF MATERIALS CHEMISTRY A, 2022, 10 (16) : 8975 - 8988
  • [26] Achieving high power density and excellent durability for high temperature proton exchange membrane fuel cells based on crosslinked branched polybenzimidazole and metal-organic frameworks
    Wu, Yingnan
    Liu, Xiaoting
    Yang, Fan
    Zhou, Leon Lee
    Yin, Bibo
    Wang, Peng
    Wang, Lei
    JOURNAL OF MEMBRANE SCIENCE, 2021, 630
  • [27] Effect of La2Ce2O7 on the Physicochemical Properties of Phosphoric Acid Doped Polybenzimidazole Nanocomposite Membranes for High Temperature Proton Exchange Membrane Fuel Cells Applications
    Shabanikia, Akbar
    Javanbakht, Mehran
    Amoli, Hossein Salar
    Hooshyari, Khadijeh
    Enhessari, Morteza
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2014, 161 (14) : F1403 - F1408
  • [28] Highly stable and active Pt electrocatalysts on TiO2-Co3O4-C composite support for polymer exchange membrane fuel cells
    Han, Mingjia
    Li, Muwu
    Wu, Xin
    Zeng, Jianhuang
    Liao, Shijun
    ELECTROCHIMICA ACTA, 2015, 154 : 266 - 272
  • [29] A PBI-Sb0.2Sn0.8P2O7-H3PO4 Composite Membrane for Intermediate Temperature Fuel Cells
    Wu, X.
    Mamlouk, M.
    Scott, K.
    FUEL CELLS, 2011, 11 (05) : 620 - 625
  • [30] In situ hybrid Nafion/SiO2-P2O5 proton conductors for high-temperature and low-humidity proton exchange membrane fuel cells
    So, Soon Yong
    Kim, Sung Chul
    Lee, Sang-Young
    JOURNAL OF MEMBRANE SCIENCE, 2010, 360 (1-2) : 210 - 216