Effect of Dehydrogenation and Heat Treatments on the Microstructure and Tribological Behavior of Electroless Ni-P Nanocomposite Coatings

被引:0
|
作者
Pedrizzetti, Giulia [1 ]
Baroni, Enrico [2 ]
Gragnanini, Michele [2 ]
Bottacchiari, Rita [1 ]
Merlin, Mattia [2 ]
Pulci, Giovanni [1 ]
Marra, Francesco [1 ]
机构
[1] Sapienza Univ Rome, Dept Chem Engn, INSTM Reference Lab Engn Surface Treatments, Mat,Environm, Via Eudossiana 18, I-00184 Rome, Italy
[2] Univ Ferrara, Dept Engn DE, I-44121 Ferrara, Italy
关键词
electroless Ni-P coatings; nanocomposite coatings; ZrO2 and Al2O3 nanoparticles; dehydrogenation; thermal treatments; instrumented indentation; wear resistance; PHASE-TRANSFORMATION BEHAVIOR; SUBMICRON SIC PARTICLES; CORROSION-RESISTANCE; COMPOSITE COATINGS; W-P; NICKEL; WEAR; HARDNESS; ALLOY; PERFORMANCE;
D O I
10.3390/ma17225657
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
High phosphorus Ni-P coatings, both unreinforced and modified by the addition of alumina (Al2O3) and zirconia (ZrO2) nanoparticles, were manufactured by electroless deposition technique and heat-treated with different temperature and duration schedules. The effect of dehydrogenation (200 degrees C for 2 h) and its combination with crystallization heat treatment was studied in terms of microstructural changes and wear resistance. The amorphous structure of the coatings was not altered by the introduction of both Al2O3 and ZrO2 nanoparticles, and the addition of 1.5 g/L of ZrO2 yielded the highest microhardness due to better particles dispersion. Dehydrogenation improved hardness because of the early stages of grain growth; however, the greatest improvement in hardness (+120% compared to unreinforced Ni-P) was obtained after annealing at 400 degrees C for 1 h, because of the microprecipitation of the Ni3P crystalline phase induced by thermal treatment. No detectable differences in hardness and microstructure were detected when annealing at 400 degrees C for 1 h with or without prior dehydrogenation; however, the dehydrogenated coatings exhibited a lower Young's modulus. ZrO2-reinforced coatings demonstrated improved wear resistance, and wear tests revealed that dehydrogenation is fundamental for lowering the coefficient of friction (-14%) and wear rate (-97%) when performed before annealing at 400 degrees C for 1 h. The analysis of the wear tracks showed that the non-dehydrogenated samples failed by complete coating delamination from the substrate, with abrasion identified as the predominant wear mechanism. Conversely, the dehydrogenated samples demonstrated better resistance due to the formation of a protective oxide layer, leading to an overall increase in the coating wear resistance.
引用
收藏
页数:22
相关论文
共 50 条
  • [31] Effect of Microstructure on the Friction Properties of the Electroless Ni-P Deposit
    Cheng, Y. H.
    Zou, Y.
    Cheng, L.
    Liu, W.
    ADVANCED TRIBOLOGY, 2009, : 736 - +
  • [32] The corrosion behavior of electroless Ni-P coatings in concentrated KOH electrolyte
    He, A.
    Hu, H.
    Aasen, D.
    Ivey, D. G.
    JOURNAL OF APPLIED ELECTROCHEMISTRY, 2024, 54 (12) : 2919 - 2929
  • [33] CORROSION RESISTANCE OF ELECTROLESS Ni-P/Cu/Ni-P MULTILAYER COATINGS
    Zhao, G. L.
    Zou, Y.
    Hao, Y. L.
    Zou, Z. D.
    ARCHIVES OF METALLURGY AND MATERIALS, 2015, 60 (02) : 1003 - 1008
  • [34] Tribological study of mechanically milled graphite nanoparticles codeposited in electroless Ni-P coatings
    Thakur I.S.
    Pandey V.S.
    Rao P.S.
    Tyagi S.
    Goyal D.
    Goyal, Deepam (bkdeepamgoyal@outlook.com), 1600, Elsevier Ltd (75): : 344 - 349
  • [35] Tribological characteristics of electroless Ni-P alloys as an alternative to chromium coatings: infometric analysis
    Vinokurov, Evgeny G.
    Burukhina, Tatiana F.
    Skopintsev, Vladimir D.
    Meshalkin, Valeriy P.
    MENDELEEV COMMUNICATIONS, 2024, 34 (04) : 472 - 477
  • [36] Optimization of Tribological Properties of Electroless Ni-P Coatings Under Lubrication Using WPCA
    Duari, Santanu
    Barman, Tapan Kr.
    Sahoo, Prasanta
    DYNAMICS OF MACHINES AND MECHANISMS, INDUSTRIAL RESEARCH, 2014, 592-594 : 1341 - 1345
  • [37] Electroless deposition of graded Ni-P coatings
    Hadipour, A.
    Monirvaghefi, S. M.
    Bahrololoom, M. E.
    SURFACE ENGINEERING, 2015, 31 (06) : 399 - 405
  • [38] Influence of heat treatment on tribological behaviour of Ni-P autocatalytic coatings
    León, OA
    Staia, MH
    SURFACE ENGINEERING, 1999, 15 (05) : 391 - 394
  • [39] Friction and wear behavior of electroless Ni-P and Ni-W-P alloy coatings
    Palaniappa, M.
    Seshadri, S. K.
    WEAR, 2008, 265 (5-6) : 735 - 740
  • [40] The Effect of Electroless Bath Parameters and Heat Treatment on the Properties of Ni-P and Ni-P-Cu Composite Coatings
    Anijdan, Seyyed Hashem Mousavi
    Sabzi, Masoud
    Zadeh, Mostafa Roghani
    Farzam, Mansour
    MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS, 2018, 21 (02):