Effect of Dehydrogenation and Heat Treatments on the Microstructure and Tribological Behavior of Electroless Ni-P Nanocomposite Coatings

被引:0
|
作者
Pedrizzetti, Giulia [1 ]
Baroni, Enrico [2 ]
Gragnanini, Michele [2 ]
Bottacchiari, Rita [1 ]
Merlin, Mattia [2 ]
Pulci, Giovanni [1 ]
Marra, Francesco [1 ]
机构
[1] Sapienza Univ Rome, Dept Chem Engn, INSTM Reference Lab Engn Surface Treatments, Mat,Environm, Via Eudossiana 18, I-00184 Rome, Italy
[2] Univ Ferrara, Dept Engn DE, I-44121 Ferrara, Italy
关键词
electroless Ni-P coatings; nanocomposite coatings; ZrO2 and Al2O3 nanoparticles; dehydrogenation; thermal treatments; instrumented indentation; wear resistance; PHASE-TRANSFORMATION BEHAVIOR; SUBMICRON SIC PARTICLES; CORROSION-RESISTANCE; COMPOSITE COATINGS; W-P; NICKEL; WEAR; HARDNESS; ALLOY; PERFORMANCE;
D O I
10.3390/ma17225657
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
High phosphorus Ni-P coatings, both unreinforced and modified by the addition of alumina (Al2O3) and zirconia (ZrO2) nanoparticles, were manufactured by electroless deposition technique and heat-treated with different temperature and duration schedules. The effect of dehydrogenation (200 degrees C for 2 h) and its combination with crystallization heat treatment was studied in terms of microstructural changes and wear resistance. The amorphous structure of the coatings was not altered by the introduction of both Al2O3 and ZrO2 nanoparticles, and the addition of 1.5 g/L of ZrO2 yielded the highest microhardness due to better particles dispersion. Dehydrogenation improved hardness because of the early stages of grain growth; however, the greatest improvement in hardness (+120% compared to unreinforced Ni-P) was obtained after annealing at 400 degrees C for 1 h, because of the microprecipitation of the Ni3P crystalline phase induced by thermal treatment. No detectable differences in hardness and microstructure were detected when annealing at 400 degrees C for 1 h with or without prior dehydrogenation; however, the dehydrogenated coatings exhibited a lower Young's modulus. ZrO2-reinforced coatings demonstrated improved wear resistance, and wear tests revealed that dehydrogenation is fundamental for lowering the coefficient of friction (-14%) and wear rate (-97%) when performed before annealing at 400 degrees C for 1 h. The analysis of the wear tracks showed that the non-dehydrogenated samples failed by complete coating delamination from the substrate, with abrasion identified as the predominant wear mechanism. Conversely, the dehydrogenated samples demonstrated better resistance due to the formation of a protective oxide layer, leading to an overall increase in the coating wear resistance.
引用
收藏
页数:22
相关论文
共 50 条
  • [21] The Microstructure and Tribological Behavior of Ultrasonic Electroless Ni-P Plating on TC4 Titanium Alloy with Heat-Treatment
    Cao, Jingjing
    Zhao, Wenwu
    Wang, Xiaoyu
    Zhao, Yifan
    Ma, Penghui
    Jiang, Wentao
    Song, Guangming
    FERROELECTRICS, 2022, 589 (01) : 1 - 11
  • [22] Effects of Alumina Content on Tribological Properties of Electroless Ni-P Composite Coatings
    Zheng Xiaohua
    Liu Hui
    Chen Li
    Zhang Lingjie
    Zhang Ji
    Shen Tao
    Yang Fanger
    RARE METAL MATERIALS AND ENGINEERING, 2018, 47 : 171 - 176
  • [23] Preparation and tribological characterization of graphene incorporated electroless Ni-P composite coatings
    Rana, Ahmad Raza Khan
    Farhat, Zoheir
    SURFACE & COATINGS TECHNOLOGY, 2019, 369 : 334 - 346
  • [24] Effect of coating parameters and heat treatment on the adhesive properties of electroless Ni-P coatings
    Taheri, R
    Oguocha, INA
    Yannacopoulos, S
    CANADIAN METALLURGICAL QUARTERLY, 2004, 43 (03) : 363 - 369
  • [25] Electroless Ni-P composite coatings: The effect of heat treatment on the microhardness of substrate and coating
    Apachitei, I
    Duszczyk, J
    Katgerman, L
    Overkamp, PJB
    SCRIPTA MATERIALIA, 1998, 38 (09) : 1347 - 1353
  • [26] Investigation of tribological and corrosion performance of duplex electroless Ni-P/Ni-Cu-P coatings
    Biswas P.
    Kalyan Das S.
    Sahoo P.
    Materials Today: Proceedings, 2023, 80 : 1122 - 1129
  • [27] Tribological behavior of autocatalytic Ni-P based duplex coatings
    Biswas, Palash
    Das, Suman Kalyan
    Sahoo, Prasanta
    PHYSICA SCRIPTA, 2024, 99 (04)
  • [28] Tribological Behavior and Surface Analysis of Ni-P/BP Coatings
    Wu, Hao
    Luo, Zhiheng
    Dong, Yinghui
    Yao, Lulu
    Xu, Yufu
    JOURNAL OF TRIBOLOGY-TRANSACTIONS OF THE ASME, 2024, 146 (05):
  • [29] Effect of surfactants on the behavior of the Ni-P bath and on the formation of electroless Ni-P-TiC composite coatings
    Czagany, M.
    Baumli, P.
    SURFACE & COATINGS TECHNOLOGY, 2019, 361 : 42 - 49
  • [30] Microstructure characteristics and phase transformations of the Ni-P and Ni-P-Re electroless deposited coatings after heat treatment
    Wojewoda-Budka, J.
    Wierzbicka-Miernik, A.
    Litynska-Dobrzynska, L.
    Szczerba, M. J.
    Mordarski, G.
    Mosialek, M.
    Huber, Z.
    Zieba, P.
    ELECTROCHIMICA ACTA, 2016, 209 : 183 - 191