Influence of Cold Drawing on Phase Transformation and Tensile Properties of FeCrMn Austenitic Stainless Steel 201

被引:0
|
作者
Masoumi, Mohammad [1 ]
de Oliveira, Silvio E. [1 ]
Paredes, Marcelo [2 ]
机构
[1] Fed Univ ABC, Ctr Engn Modeling & Appl Social Sci, BR-09210580 Santo Andre, SP, Brazil
[2] Texas A&M Univ, Dept Ocean Engn, Galveston, TX 77554 USA
关键词
crystal orientations; dislocation densities; martensitic transformations; microstructural evolutions; MULTISCALE CHARACTERIZATION; MARTENSITE; REVERSION; MECHANISMS; HCP;
D O I
10.1002/srin.202400469
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Manganese stabilizes the austenite and reduces the stacking fault energy in face-centered cubic (FCC) structures, promoting the formation of hexagonal and cubic structures. This study investigates the phase transformation and mechanical behavior of extremely low-carbon FeCrMn austenitic stainless AISI 201 steel subjected to cold drawing in three stages, ultimately reaching a true strain of 0.93. The objective is to examine the transformation from the parent FCC structure to hexagonal close-packed and body-centered cubic structures as a combination of transformation-induced plasticity and twinning-induced plasticity phenomena. X-ray diffraction and electron backscatter diffraction analyses are utilized to investigate phase transformations under significant plastic deformation and the crystallographic orientation relationships between phases. Additionally, tensile and hardness tests are performed to assess the impact of plastic deformation on mechanical properties. Results indicate that a true strain of 50% is optimal for balancing strength and ductility in CrMnFe austenitic stainless steel. After applying a true strain of epsilon 1 = 26.7%, yield strength (YS) increases by 192% and ultimate tensile strength (UTS) by 35%, while elongation reduces by 41%. With a further strain of epsilon 2 = 57.5%, YS increases by 71% and UTS by 44%, but elongation drastically decreases by 94%. Applying the final strain of epsilon 3 = 94.0%, YS and UTS only increase by 3% and 2%, respectively, while elongation further reduced by 40%. These findings suggest that a true strain of 50% shall be considered the maximum reduction for maintaining a balance between strength and ductility in CrMnFe austenitic stainless steel.
引用
收藏
页数:12
相关论文
共 50 条
  • [31] Effect of Si and Mn on Microstructure and Tensile Properties of Austenitic Stainless Steel
    Lu, Chengxu
    Yi, Haoyu
    Liang, Tian
    Wang, Min
    Xue, Hailong
    Ma, Yingche
    Liu, Kui
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2021, 50 (01): : 187 - 194
  • [32] Tensile properties of a nanocrystalline 316L austenitic stainless steel
    Chen, XH
    Lu, J
    Lu, L
    Lu, K
    SCRIPTA MATERIALIA, 2005, 52 (10) : 1039 - 1044
  • [33] Effect of Si and Mn on Microstructure and Tensile Properties of Austenitic Stainless Steel
    Lu Chengxu
    Yi Haoyu
    Liang Tian
    Wang Min
    Xue Hailong
    Ma Yingche
    Liu Kui
    RARE METAL MATERIALS AND ENGINEERING, 2021, 50 (01) : 187 - 194
  • [34] THE EFFECT OF COLD DRAWING ON PROPERTIES AND MICROSTRUCTURE OF MANGANESE AUSTENITIC STEEL WIRE
    Tomaszewska, Agnieszka
    Jablonska, Magdalena
    Tkocz, Marek
    Bednarczyk, Iwona
    28TH INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS (METAL 2019), 2019, : 495 - 500
  • [35] Martensitic ternary FeCrMn thin films sputtered from austenitic AISI 202 stainless steel target: Phase transition and corresponding magnetic properties under the influence of deposition rate
    Kockar, Hakan Ko
    Kaplan, Nadir
    Karaagac, Oznur
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2023, 587
  • [36] TENSILE PROPERTIES OF HYDROGEN CHARGED FERRITIC-AUSTENITIC 2-PHASE STAINLESS-STEEL
    FUKUYAMA, S
    YOKOGAWA, K
    KUDO, K
    OHTANI, N
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1982, 46 (12) : 1193 - 1199
  • [37] Influence of pre-strain on cryogenic tensile properties of 316LN austenitic stainless steel
    Zhang, Hengcheng
    Huang, Chuanjun
    Huang, Rongjin
    Li, Laifeng
    CRYOGENICS, 2020, 106
  • [38] INFLUENCE OF LITHIUM EXPOSURE ON THE UNIAXIAL TENSILE PROPERTIES OF A CR-MN AUSTENITIC STAINLESS-STEEL
    FENICI, P
    COEN, V
    RUEDL, E
    KOLBE, H
    SASAKI, T
    JOURNAL OF NUCLEAR MATERIALS, 1982, 103 (1-3) : 699 - 702
  • [39] The Influence of Cold Deformation and Annealing on Texture Changes in Austenitic Stainless Steel
    Kowalska, Joanna
    Witkowska, Malgorzata
    ADVANCES IN SCIENCE AND TECHNOLOGY-RESEARCH JOURNAL, 2024, 18 (02) : 143 - 158
  • [40] Strain partitioning and texture evolution during cold rolling of AISI 201 austenitic stainless steel
    Souza Filho, I. R.
    Zilnyk, K. D.
    Sandim, M. J. R.
    Bolmaro, R. E.
    Sandim, H. R. Z.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 702 : 161 - 172