Transient Liquid-Phase Bonding Using Sn/Ni/Sn Laminated Metal Preform for Power Device Packaging

被引:0
|
作者
Lee, Dong-Bok [1 ]
Seo, Young-Jin [1 ]
Yoon, Jeong-Won [1 ]
机构
[1] Chungbuk Natl Univ, Dept Adv Mat Engn, 1 Chungdae Ro, Cheongju 28644, Chungbuk, South Korea
基金
新加坡国家研究基金会;
关键词
Intermetallic compounds; soldering; electronic packaging; thermo-compression bonding; microstructure; laminated metal preform; SOLDER; MICROSTRUCTURE; EVOLUTION;
D O I
10.1007/s11664-025-11738-5
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Intermetallic compound (IMC) joints formed via transient liquid-phase (TLP) bonding offer excellent high-temperature durability. However, IMC formation at the joint requires long bonding times and high pressures. In this study, to reduce the bonding time and pressure required for IMC formation, a Sn/Ni/Sn laminated metal preform was fabricated by inserting Ni foil between Sn foils, and this material was used to bond a chip to a substrate. The microstructure of the joint cross-section was analyzed using field-emission scanning electron microscopy and energy-dispersive x-ray spectroscopy. The Sn foil was completely converted to 7 mu m Ni3Sn4 within 15 min, forming a stable TLP-bonded joint. After bonding, a shear test was conducted to evaluate the mechanical properties of the joints, which revealed high shear strength, exceeding 46 MPa.
引用
收藏
页码:1592 / 1601
页数:10
相关论文
共 50 条
  • [31] Mechanical reliability of transient liquid phase bonding of Au-Sn solder with Ni(Cu) substrates
    Peng, J.
    Wang, R. C.
    Liu, H. S.
    Li, J. Y.
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2018, 29 (01) : 313 - 322
  • [32] Compaction Kinetics with Liquid-Phase Sintering of W – Ni – Sn Pseudoalloys
    Valentin I. Nizhenko
    Valerii V. Skorokhod
    Powder Metallurgy and Metal Ceramics, 2004, 43 : 364 - 370
  • [33] Low-temperature transient liquid phase bonding via electroplated Sn/In-Sn metallization
    Tsai, Chin-Hao
    Hung, Han-Tang
    Chang, Fu-Ling
    Bickel, Steffen
    Mueller, Maik
    Panchenko, Iuliana
    Bock, Karlheinz
    Kao, C. R.
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 19 : 2510 - 2515
  • [34] Transient Liquid Phase Sintering of Ni and Sn-58Bi on Microstructures and Mechanical Properties for Ni-Ni Bonding
    Min, Kyung Deuk
    Jung, Kwang-Ho
    Lee, Choong-Jae
    Jeong, Haksan
    Hwang, Byeong-Uk
    Jung, Seung-Boo
    ELECTRONIC MATERIALS LETTERS, 2020, 16 (04) : 347 - 354
  • [35] Novel and fast transient liquid phase bonding using etched Cu foam/Sn-3.0Ag-0.5Cu composite solder preform
    Heo, Min-Haeng
    Seo, Young-Jin
    Yoon, Jeong-Won
    MATERIALS TODAY COMMUNICATIONS, 2023, 35
  • [36] Transient liquid-phase bonding in the Ni-Al-B system
    C. E. Campbell
    W. J. Boettinger
    Metallurgical and Materials Transactions A, 2000, 31 : 2835 - 2847
  • [37] Transient liquid-phase bonding in the Ni-Al-B system
    Campbell, CE
    Boettinger, WJ
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2000, 31 (11): : 2835 - 2847
  • [38] Transient liquid phase (TLP) bonding using Sn/Ag multilayers for high temperature applications
    Nobeen, Nadeesh Singh
    Imade, Riko
    Lee, Byung Hoon
    Phua, Erie Jian Rung
    Wong, Chee Cheong
    Gan, Chee Lip
    Chen, Zhong
    PROCEEDINGS OF THE 2013 IEEE 15TH ELECTRONICS PACKAGING TECHNOLOGY CONFERENCE (EPTC 2013), 2013, : 647 - 652
  • [39] Transient Liquid Phase Bonding Process Using Sn-coated Cu Dendritic Particles
    Jun Ho Hwang
    Jong-Hyun Lee
    Metals and Materials International, 2021, 27 : 4638 - 4644
  • [40] Transient Liquid Phase Bonding Process Using Sn-coated Cu Dendritic Particles
    Hwang, Jun Ho
    Lee, Jong-Hyun
    METALS AND MATERIALS INTERNATIONAL, 2021, 27 (11) : 4638 - 4644