Microstructural gradients in Ti-3Al-8V-6Cr-4Zr-4Mo for excellent HCF strength and toughness

被引:0
|
作者
Technical Univ of Brandenburg at, Cottbus, Cottbus, Germany [1 ]
机构
关键词
Annealing - Crack propagation - Fatigue of materials - Fracture toughness - Metallographic microstructure - Rolling - Strength of materials;
D O I
暂无
中图分类号
学科分类号
摘要
Deep-rolling with subsequent annealing was performed on solution heat treated Ti-3Al-SV-6Cr-4Zr-4Mo to develop microstructural gradients in the notch root. Annealing treatments were varied to a wide extent to evaluate optimum conditions for excellent fatigue performance and outstanding fracture toughness of a component. Such a property combination cannot be achieved by non-gradient microstructures.
引用
收藏
相关论文
共 50 条
  • [41] Effect of strength on environment-assisted cracking of Ti-8V-6Cr-4Mo-4Zr-3Al in aqueous NaCl: Part II: crack tip strain rate
    Somerday, Brian P.
    Gangloff, Richard P.
    Materials Science and Engineering A, 1998, A254 (1-2): : 179 - 188
  • [42] Effect of strength on environment-assisted cracking of Ti-8V-6Cr-4Mo-4Zr-3Al in aqueous NaCl Part II: Crack tip strain rate
    Somerday, BP
    Gangloff, RP
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 254 (1-2): : 179 - 188
  • [43] MICROSTRUCTURAL FACTOR WHICH CONTROLS THE TOUGHNESS IN TI-6AL-4V ALLOY
    NIINOMI, M
    KOBAYASHI, T
    SASAKI, N
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1985, 25 (10) : B278 - B278
  • [44] HCF properties of laser deposited Ti-6Al-2Zr-Mo-V alloy
    He, Ruijun
    Wang, Huaming
    Hangkong Xuebao/Acta Aeronautica et Astronautica Sinica, 2010, 31 (07): : 1488 - 1493
  • [45] Synergistically achieving high strength and impact toughness in Ti-6Al-4V-0.5Mo-0.5Zr alloy pipe with bimodal microstructure
    Peng, Shuxian
    Liu, Yikui
    Fu, Mingzhu
    Liang, Yuanlong
    Zhang, Kai
    Feng, Chun
    Feng, Weizhong
    Zhang, Pinghui
    Liu, Huiqun
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 895
  • [46] Effects of Zr Content on the Microstructures and Tensile Properties of Ti–3Al–8V–6Cr–4Mo–xZr Alloys
    Hong-Bo Ba
    Li-Min Dong
    Zhi-Qiang Zhang
    Dong-Sheng Xu
    Rui Yang
    Acta Metallurgica Sinica (English Letters), 2016, 29 : 722 - 726
  • [47] IMPROVED TOUGHNESS IN TI-6AL-4V
    EARLY, PW
    BURNS, SJ
    JOM-JOURNAL OF METALS, 1976, 28 (12): : A37 - A37
  • [48] Effect of strength on environment-assisted cracking of Ti-8V-6Cr-4Mo-4Zr-3Al in aqueous NaCl Part 1: Age hardening vs. work hardening
    Somerday, BP
    Gangloff, RP
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 254 (1-2): : 166 - 178
  • [49] IMPACT TOUGHNESS OF HYDROGEN CHARGED TI-6AL-2SN-4ZR-6MO ALLOY
    NIINOMI, M
    SUZUKI, K
    KOBAYASHI, T
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1987, 73 (10): : 1405 - 1412
  • [50] Powder interlayer bonding of titanium alloys: Ti-6Al-2Sn-4Zr-6Mo and Ti-6Al-4V
    P. Davies
    A. Johal
    H. Davies
    S. Marchisio
    The International Journal of Advanced Manufacturing Technology, 2019, 103 : 441 - 452