Microstructural gradients in Ti-3Al-8V-6Cr-4Zr-4Mo for excellent HCF strength and toughness

被引:0
|
作者
Technical Univ of Brandenburg at, Cottbus, Cottbus, Germany [1 ]
机构
关键词
Annealing - Crack propagation - Fatigue of materials - Fracture toughness - Metallographic microstructure - Rolling - Strength of materials;
D O I
暂无
中图分类号
学科分类号
摘要
Deep-rolling with subsequent annealing was performed on solution heat treated Ti-3Al-SV-6Cr-4Zr-4Mo to develop microstructural gradients in the notch root. Annealing treatments were varied to a wide extent to evaluate optimum conditions for excellent fatigue performance and outstanding fracture toughness of a component. Such a property combination cannot be achieved by non-gradient microstructures.
引用
收藏
相关论文
共 50 条
  • [1] Microstructural gradients in Ti-3Al-8V-6Cr-4Zr-4Mo for excellent HCF strength and toughness
    Berg, A
    Kiese, J
    Wagner, L
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 243 (1-2): : 146 - 149
  • [2] SILICIDE FORMATION IN TI-3AL-8V-6CR-4ZR-4MO
    ANKEM, S
    BANERJEE, D
    MCNEISH, DJ
    WILLIAMS, JC
    SEAGLE, SR
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1987, 18 (12): : 2015 - 2025
  • [3] STABILITY OF AGED TI-3AL-8V-6CR-4ZR-4MO
    RACK, HJ
    HEADLEY, TJ
    SCRIPTA METALLURGICA, 1980, 14 (11): : 1211 - 1216
  • [4] PHASE-TRANSFORMATIONS IN TI-3AL-8V-6CR-4ZR-4MO
    HEADLEY, TJ
    RACK, HJ
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1979, 10 (07): : 909 - 920
  • [5] Microstructure and mechanical properties of selective laser melted Ti-3Al-8V-6Cr-4Zr-4Mo compared to Ti-6Al-4V
    Madikizela, C.
    Cornish, L. A.
    Chown, L. H.
    Moller, H.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 747 : 225 - 231
  • [6] STABILITY OF AGED TI-AL-3-V-8-CR-6-MO-4-ZR-4
    RACK, HJ
    HEADLEY, TJ
    JOURNAL OF METALS, 1979, 31 (12): : 42 - 42
  • [7] EFFECTS OF BETA GRAIN-SIZE AND AGED STRUCTURE ON STRENGTH AND TOUGHNESS OF A TI-3AL-8V-6CR-4MO-4ZR ALLOY
    MUNEKI, S
    KAWABE, Y
    TAKAHASHI, J
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1993, 57 (03) : 268 - 273
  • [8] TI-3AL-8V-6CR-4MO-4ZR WIRE FOR SPRING APPLICATIONS
    BOYER, RR
    BAJORAITIS, R
    GREENWOOD, DW
    MILD, EE
    JOURNAL OF METALS, 1982, 35 (12): : A35 - A35
  • [9] The analysis of the hot deformation behaviour of the Ti-3Al-8V-6Cr-4Zr-4Mo alloy, using processing maps, a map of microstructure and of hardness
    Lukaszek-Solek, Aneta
    Krawczyk, Janusz
    MATERIALS & DESIGN, 2015, 65 : 165 - 173
  • [10] Research on the microstructure and properties of metastable β type Ti-8V4Mo3Cr3Zr3Al alloy with high strength and toughness
    Gao, Xiang
    Tao, Aili
    Zou, Mingcong
    Xu, Zaidong
    Intermetallics, 2024, 175