Defect and atomic ordering studies in highly deformed and disordered Fe72Al28 alloy

被引:0
|
作者
Acad of Sciences of the Czech, Republic, Brno, Czech Republic [1 ]
机构
来源
Acta Mater | / 5卷 / 2147-2154期
关键词
Annealing - Crystal atomic structure - Crystal defects - Crystal lattices - Deformation - Dislocations (crystals) - Morphology - Mossbauer spectroscopy - Phase transitions - Quenching;
D O I
暂无
中图分类号
学科分类号
摘要
The results of positron annihilation and Moessbauer spectroscopies in Fe72Al28 alloy with different structural morphology obtained by severe deformation and by quenching from a high temperature are presented. The changes in atomic ordering and in defect arrangements after recovery and ordering annealing in both highly deformed and highly disordered samples are also pursued and discussed. It is shown that the dominant component of 184 ps in the positron lifetime spectrum of a highly disordered sample corresponds to the annihilation in vacancies which prefer to occupy that sublattice in D03 superstructure containing both aluminum and iron atoms. Important changes in vacancy concentration take place only when an annealing above D03↔B2 (823 K) is performed. Temperature treatment below this phase transformation temperature is characterized above all by changes in the density of dislocations.
引用
收藏
相关论文
共 43 条
  • [21] Influence of atomic ordering on optical conduction of a Fe-Al alloy
    Repets'ky, SP
    Shakhov, IV
    Yaremko, RO
    METALLOFIZIKA I NOVEISHIE TEKHNOLOGII, 2004, 26 (02): : 165 - 172
  • [22] How Fe60Co40 and Fe72Al28 nano-alloys produced by mechanical alloying behave when exposed to microwaves
    Otmane, F.
    Bergheul, S.
    Hamlati, Z.
    Azzaz, M.
    NANOMATERIALS BY SEVERE PLASTIC DEFORMATION IV, PTS 1 AND 2, 2008, 584-586 : 977 - 981
  • [23] RECOVERY OF HIGHLY STRAINED FE-28 AT.-PERCENT-AL ALLOY
    JIRASKOVA, Y
    KOCOVA, M
    PIZUROVA, N
    ZAK, T
    SCHNEEWEISS, O
    MATERIALS SCIENCE AND TECHNOLOGY, 1993, 9 (05) : 397 - 402
  • [24] Mechanical strain characteristics of cold worked Fe72Al28 and Fe75Ni25 alloys:: A positron annihilation coincidence Doppler broadening view
    Pandey, Brajesh
    Verma, H. C.
    INTERMETALLICS, 2008, 16 (03) : 440 - 446
  • [25] Effect of chromium ternary additions on the ordering behaviour in Fe-28 at.% Al alloy
    Hamana, D.
    Amiour, L.
    Bouchear, M.
    MATERIALS CHEMISTRY AND PHYSICS, 2008, 112 (03) : 816 - 822
  • [26] MOSSBAUER-EFFECT AND NMR-STUDIES OF FE72PT28 INVAR ALLOY
    SUMIYAMA, K
    SHIGA, M
    TACHI, K
    NAKAMURA, Y
    JOURNAL OF THE PHYSICAL SOCIETY OF JAPAN, 1976, 40 (04) : 1002 - 1006
  • [27] Superplastic deformation studies in Fe-28Al-3Cr intermetallic alloy
    Sharma, G
    Kishore, R
    Sundararaman, M
    Ramanujan, RV
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 419 (1-2): : 144 - 147
  • [28] Mossbauer studies of phase stability in mechanically stressed Fe-28 at% Al alloy
    Verma, HC
    Suwas, S
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2000, 212 (03) : 361 - 367
  • [29] EXPERIMENTAL AND THEORETICAL-STUDIES ON PHASE SEPARATIONS IN THE FE-AL-CO ORDERING ALLOY SYSTEM
    KOZAKAI, T
    MIYAZAKI, T
    JOURNAL OF MATERIALS SCIENCE, 1994, 29 (03) : 652 - 659
  • [30] Mossbauer and positron annihilation studies in plastically deformed Fe72-xAl28Tix (x=0, 2, 9) alloys
    Pandey, B
    Nambissan, PMG
    Suwas, S
    Verma, HC
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2003, 263 (03) : 307 - 314