摘要
Recovery of a highly strained Fe-28 at.-% Al alloy has been studied by means of electrical resistivity, Mossbauer spectroscopy, magnetic polarisation, and coercivity measurements. The amount and state of defect rich volumes (interfacial phase) were investigated. Three recovery steps were found in the temperature dependences of resistivity and magnetic polarisation. The first two steps are characterised by almost the same activation energies (epsilon1 = 120 +/- 5 and epsilon2 = 127 +/- 1 kJ mol-1) derived from resistivity measurements, and can be ascribed to the annihilation of defects and relaxation of stresses accompanied by cell wall sharpening and the onset of subboundary formation. The appearance of backward recovery stresses was manifested as changes of spin-orientation. The third step is ascribed to the process of cell wall sharpening. The observation of the third and further steps was complicated by overlapping caused by magnetic transformations and ordering effects. (C) 1993 The Institute of Materials.
引用
收藏
页码:397 / 402
页数:6
相关论文
共 50 条
  • [1] INFLUENCE OF AN EXTERNAL MAGNETIC-FIELD ON THE RECOVERY OF HIGH STRAINED FE-28 AT PERCENT AL-ALLOY
    ZAK, T
    JIRASKOVA, Y
    SCHNEEWEISS, O
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 1993, 127 (1-2) : 140 - 144
  • [2] ELECTROSLAG REMELTING OF FE-28 ATMOSPHERIC-PERCENT-AL INTERMETALLIC ALLOY
    BALIGIDAD, RG
    PRAKASH, U
    RAO, VR
    RAO, PK
    BALLAL, NB
    IRONMAKING & STEELMAKING, 1994, 21 (04) : 324 - 331
  • [3] INFLUENCE OF INTERNAL-STRESSES ON STRUCTURE CHANGES IN ALLOY FE-28 PERCENT NI
    LEPINE, G
    CIZERON, G
    MEMOIRES SCIENTIFIQUES DE LA REVUE DE METALLURGIE, 1976, 73 (06): : 385 - 399
  • [4] Mossbauer studies of phase stability in mechanically stressed Fe-28 at% Al alloy
    Verma, HC
    Suwas, S
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2000, 212 (03) : 361 - 367
  • [5] Effect of chromium ternary additions on the ordering behaviour in Fe-28 at.% Al alloy
    Hamana, D.
    Amiour, L.
    Bouchear, M.
    MATERIALS CHEMISTRY AND PHYSICS, 2008, 112 (03) : 816 - 822
  • [6] Preferential growth direction in Fe-28 at.% Al-4 at.% Cr alloy
    Kopecek, J
    Lejcek, P
    JOURNAL OF CRYSTAL GROWTH, 2006, 287 (02) : 267 - 269
  • [7] MECHANICAL DISORDERING OF FE-28-PERCENT-AL-4-PERCENT-CR ALLOY
    DADRAS, MM
    MORRIS, DG
    SCRIPTA METALLURGICA ET MATERIALIA, 1993, 28 (10): : 1245 - 1250
  • [8] MICROSTRUCTURES AND SOME PROPERTIES OF FE-28 PERCENT CR-4 PERCENT MO ALLOYS
    STREICHER, MA
    CORROSION, 1974, 30 (04) : 115 - 124
  • [9] HIGHLY COMPACT SINTERED ALLOY AL-12.5 (AT)PERCENT FE
    RUSIN, NM
    SAVITSKII, AP
    POWDER METALLURGY AND METAL CERAMICS, 1993, 32 (11-12) : 897 - 900
  • [10] A study of time dependent phase transitions in the Fe-28%Ga alloy by electroresistivity
    Uyi, D. O.
    Mouas, M.
    Gasser, F.
    Gasser, J. G.
    Cheverikin, V. V.
    Balagurov, A. M.
    Golovin, I. S.
    MATERIALS LETTERS, 2025, 384