ELECTROCHEMICAL MEASUREMENT OF THE ACTIVITY OF IRON OXIDE IN FeO-SiO2 LIQUID SLAG.

被引:0
|
作者
Wanibe, Yoshimoto
Yamauchi, Yutaka
Kawai, Kenji
Sakao, Hiroshi
机构
来源
| 1600年 / 12期
关键词
D O I
暂无
中图分类号
学科分类号
摘要
To determine the activity of iron oxide in slag, a new type of cell was designed. The electrochemical measurement was carried out for a binary FeO-SiO//2 system by using a solid electrolyte. The standard free energy change determined is expressed as DELTA G degree equals minus 56 750 plus 11. 2 tau for the reaction, Fe( gamma ) plus 1/2 O//2(g) equals FeO( iota ). The activity of iron oxide obtained shows good agreement with literature data.
引用
收藏
相关论文
共 50 条
  • [41] Thermodynamic model of lead oxide activity in PbO-CaO-SiO2-FeO-Fe2O3 slag system
    Wang, Jin-liang
    Wen, Xiao-chun
    Zhang, Chuan-fu
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2015, 25 (05) : 1633 - 1639
  • [42] Calculation Model for Activity of FeO in Quaternary Slag System SiO2-CaO-Al2O3-FeO
    Li, Zhi
    Ma, Guojun
    Liu, Mengke
    Zou, Jingjing
    METALS, 2018, 8 (09):
  • [43] RAMAN-SPECTROSCOPIC STUDY OF THE STRUCTURE OF CAO-MEO-SIO2, MNO-SIO2 AND FEO-SIO2 SLAGS
    IGUCHI, Y
    BANYA, S
    NICHINA, Y
    JOURNAL OF METALS, 1984, 36 (08): : 94 - 94
  • [44] ANALYSIS OF THE ACTIVITY OF AS IN FEO-FE2O3-SIO2 SLAG AND THE DISTRIBUTION OF AS BETWEEN SLAG AND MOLTEN COPPER
    LYNCH, DC
    SCHWARTZE, KW
    CANADIAN METALLURGICAL QUARTERLY, 1981, 20 (03) : 269 - 278
  • [45] Measurement of hydrogen reduction rates of FeO in 2FeO•SiO2 and CaO•FeO•SiO2
    Ono-Nakazato, H
    Tsubone, Y
    Takaki, Y
    Usui, T
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2001, 87 (05): : 320 - 326
  • [46] Rate of 2CaO•SiO2 Dissolution into Molten CaO-FeO-SiO2 Slag Saturated with Solid Iron
    Kobayashi, Yoshinao
    Sadamoto, Takahide
    ISIJ INTERNATIONAL, 2017, 57 (10) : 1703 - 1709
  • [47] Why amorphous FeO-SiO2 slags do not acid-leach at high temperatures
    Perederiy, Ilya
    Papangelakis, Vladimiros G.
    JOURNAL OF HAZARDOUS MATERIALS, 2017, 321 : 737 - 744
  • [48] Activity of Iron Oxide in Steelmaking Slag
    Somnath Basu
    Ashok Kumar Lahiri
    Seshadri Seetharaman
    Metallurgical and Materials Transactions B, 2008, 39 : 447 - 456
  • [49] Activity of iron oxide in steelmaking slag
    Basu, Somnath
    Lahiri, Ashok Kumar
    Seetharaman, Seshadri
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2008, 39 (03): : 447 - 456
  • [50] Phase Diagram of FeO-TiO2-SiO2-5%Al2O3 Slag (Phase Diagram of Smelting Slag of Titanium Oxide Bearing Iron Sand)
    Itaya, Hiroshi
    Watanabe, Takashi
    Hayashi, Miyuki
    Nagata, Kazuhiro
    ISIJ INTERNATIONAL, 2014, 54 (05) : 1067 - 1073