High-temperature tensile properties of laser powder bed fusion Ti-6.5Al-2Zr-1Mo-1V alloy after annealing

被引:0
|
作者
Zhou, Jiachen [1 ,2 ]
Su, Baoxian [1 ,2 ,3 ]
Zhu, Guoqiang [1 ,2 ]
Jin, Yinling [4 ]
Wang, Binbin [1 ,2 ]
Luo, Liangshun [1 ,2 ]
Chen, Ruirun [1 ]
Wang, Liang [1 ,2 ]
Yang, Qian [5 ]
Yu, Yongsheng [3 ]
Su, Yanqing [1 ,2 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Natl Key Lab Precis Hot Proc Met, Harbin 150001, Peoples R China
[2] Harbin Inst Technol, Zhengzhou Res Inst, Zhengzhou 450000, Peoples R China
[3] Harbin Inst Technol, Sch Chem & Chem Engn, State Key Lab Urban Water Resource & Environm, Harbin 150001, Peoples R China
[4] Shenyang Aircraft Corp, Shenyang 110850, Peoples R China
[5] Yunnan Natl Titanium Met Co Ltd, Chuxiong 651200, Peoples R China
基金
中国博士后科学基金; 中国国家自然科学基金;
关键词
TA15; alloy; Laser powder bed fusion; Microstructure; High-temperature tensile property; MELTED TI-6AL-4V ALLOY; TA15; TITANIUM-ALLOY; MECHANICAL-PROPERTIES; DEFORMATION-BEHAVIOR; MICROSTRUCTURE; EVOLUTION; SLIP; DECOMPOSITION; DUCTILITY; STRESS;
D O I
10.1016/j.msea.2024.147700
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Herein, the high-temperature tensile deformation behavior in the range of 500-750 degrees C for laser powder bed fusion (L-PBF) Ti-6.5Al-2Zr-1Mo-1V (TA15) alloy after annealing treatment has been investigated in detail. The experimental results show that the ultimate tensile strength (UTS) and yield strength (YS) of the sample decrease gradually with the increase of test temperature, while the elongation (EL) of the sample increases gradually. The reduction in strength can be attributed to the decrease in dislocation density. When the tensile temperature is below 550 degrees C, a pronounced work-hardening phenomenon can be observed. At temperatures above 650 degrees C, significant dynamic recovery and dynamic recrystallization effects lead to significant softening. When the tensile temperature is below 600 degrees C, the fracture mode is transgranular fracture, while when the temperature is 650 degrees C, the fracture mode changes to intergranular fracture. After annealing, L-PBF TA15 samples exhibit excellent mechanical properties at medium to high temperatures, which provides an important reference value for the application of L-PBF fabricated titanium alloy components in the aerospace industries.
引用
收藏
页数:12
相关论文
共 50 条
  • [41] Detail fatigue rating method based on bimodal Weibull distribution for DED Ti-6.5Al-2Zr-1Mo-1V titanium alloy
    Wang, Tianshuai
    He, Xiaofan
    Wang, Jinyu
    Li, Yuhai
    CHINESE JOURNAL OF AERONAUTICS, 2022, 35 (04) : 281 - 291
  • [42] Material instability under localized severe plastic deformation during high speed turning of titanium alloy Ti-6.5AL-2Zr-1Mo-1V
    Sun, Jianfei
    Ke, Qingchan
    Chen, Wuyi
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2019, 264 : 119 - 128
  • [43] Microstructural characteristics and recrystallization mechanism of Ti-6.5Al-2Zr-1Mo-1V alloy during two-stage hot deformation
    Xu, Xinyu
    Zhang, Bohan
    Xue, Jiayu
    Li, Feng
    Su, Shan
    Chang, Hui
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 30 : 769 - 781
  • [44] Electron beam powder bed fusion of Ti-6Al-2Sn-4Zr-2Mo alloy: microstructure evolution and high-temperature mechanical properties
    Saboori, Abdollah
    Tognoli, Emanuele
    Galati, Manuela
    Denti, Lucia
    PROGRESS IN ADDITIVE MANUFACTURING, 2025,
  • [45] Hot-wire arc additive manufacturing Ti-6.5Al-2Zr-1Mo-1V titanium alloy: Pore characterization, microstructural evolution, and mechanical properties
    Lu, Tao
    Liu, Changmeng
    Li, Zixiang
    Wu, Qianru
    Wang, Jiachen
    Xu, Tianqiu
    Liu, Jiawei
    Wang, He
    Ma, Shuyuan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 817
  • [46] Deformation Behavior and Microstructure Evolution of a TiB-Reinforced Ti-6.5Al-2Zr-1Mo-1V Matrix Composite
    Ozerov, Maxim
    Stepanov, Nikita
    Sokolovsky, Vitaly
    Astakhov, Ilya
    Klimova, Margarita
    Galtsev, Alexander
    Huang, Lujun
    Zherebtsov, Sergey
    METALS, 2023, 13 (11)
  • [47] Response surface analysis, tensile properties, and microstructure of Ti-6.5Al-3.5Mo-1.5Zr-0.3Si fabricated by laser powder bed fusion
    Ou, Bingxian
    Lu, Lixin
    Meng, Xiangwei
    He, Qing
    Xie, Yilin
    Yan, Junxia
    JOURNAL OF LASER APPLICATIONS, 2023, 35 (03)
  • [48] Development of a Novel High-Temperature Al Alloy for Laser Powder Bed Fusion
    Belelli, Filippo
    Casati, Riccardo
    Riccio, Martina
    Rizzi, Alessandro
    Kayacan, Mevlut Y.
    Vedani, Maurizio
    METALS, 2021, 11 (01) : 1 - 12
  • [49] Ti-6.5Al-2Zr-1Mo-1V钛合金低温应力松弛及组织演变(英文)
    黄镇
    袁武华
    朱佳佳
    稀有金属材料与工程, 2022, 51 (01) : 83 - 91
  • [50] Thermal expansion properties of laser melting deposited Ti-6.5Al-2Zr-1Mo-1W alloy during α plus β zone annealing
    Li, Zhuo
    Cheng, Xu
    Li, Jia
    Wang, Huaming