Failure behavior of an aluminide coating on a Co-base superalloy during high-temperature oxidation in air

被引:1
|
作者
Liu, P.S. [1 ,2 ]
Liang, K.M. [1 ]
Gu, S.R. [1 ]
机构
[1] Dept. of Mat. Sci. and Engineering, Tsinghua University, Beijing 100084, China
[2] Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110015, China
来源
Oxidation of Metals | 2000年 / 54卷 / 03期
关键词
D O I
10.1023/a:1004650328779
中图分类号
学科分类号
摘要
9
引用
收藏
页码:277 / 283
相关论文
共 50 条
  • [21] Main degradation way of aluminide coating on Co-base superalloys oxidized in air at high temperatures
    Liu, P.S.
    Liang, K.M.
    Gu, S.R.
    Sun, X.F.
    Guan, H.R.
    Jin, T.
    Yang, K.N.
    Cailiao Gongcheng/Journal of Materials Engineering, 2001, (03):
  • [22] Transport mechanisms during the high-temperature oxidation of ternary γ/γ′ Co-base model alloys
    Martin Weiser
    Richard J. Chater
    Barbara A. Shollock
    Sannakaisa Virtanen
    npj Materials Degradation, 3
  • [23] Transport mechanisms during the high-temperature oxidation of ternary γ/γ′ Co-base model alloys
    Weiser, Martin
    Chater, Richard J.
    Shollock, Barbara A.
    Virtanen, Sannakaisa
    NPJ MATERIALS DEGRADATION, 2019, 3 (01)
  • [24] EFFECT OF HEAT-TREATMENT ON PRECIPITATION BEHAVIOR AND HIGH-TEMPERATURE STRENGTH IN A WROUGHT CO-BASE SUPERALLOY
    IIZUKA, H
    TANAKA, M
    JOURNAL OF MATERIALS SCIENCE, 1986, 21 (08) : 2803 - 2811
  • [25] HIGH-TEMPERATURE OXIDATION BEHAVIORS OF NI-BASE AND CO-BASE SUPERALLOYS
    BI, XF
    GOTO, KS
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1987, 51 (11) : 1060 - 1068
  • [26] Carbide Behavior during High Temperature Creep in DZ40M Co-base Superalloy
    Wenhui JIANG
    Xiangdong YAO
    Hengrong GUAN and Zhuangqi HU(Institute of Metal Research
    Journal of Materials Science & Technology, 1999, (06) : 515 - 518
  • [27] Carbide behavior during high temperature creep in DZ40M Co-base superalloy
    Jiang, Wenhui
    Yao, Xiangdong
    Guan, Hengrong
    Hu, Zhuangqi
    Journal of Materials Science and Technology, 1999, 15 (06): : 515 - 518
  • [28] Carbide behavior during high temperature creep in DZ40M co-base superalloy
    Jiang, WH
    Yao, XD
    Guan, HR
    Hu, ZQ
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 1999, 15 (06) : 515 - 518
  • [29] High temperature oxidation behavior for aluminide coating on the single crystal superalloy containing rhenium
    Liu, Chun-Ting
    Sun, Xiao-Feng
    Guan, Heng-Rong
    Hangkong Cailiao Xuebao/Journal of Aeronautical Materials, 2003, 23 (SUPPL.): : 118 - 122
  • [30] Abnormal oxidation behavior of β-NiAl base aluminide coating on a nickel-base superalloy
    Xiaofeng, Sun
    Hengrong, Guan
    Tao, Jin
    Taofeng, An
    Zhuangqi, Hu
    International Journal of Materials and Product Technology, 2001, (SPEC ISS. VOL.2) : 734 - 739