In literature, the concept of material gradation is shown to inhibit surface crack initiation in glass/ceramic composites subjected to Hertzian indentation. However, surface cracks could yet initiate due to relatively higher loadings or in the presence of surface flaws/defects. Hence, characterization of graded composites concerning the resistance against Hertzian crack initiation and propagation manifests itself as a prominent matter. In this study, axisymmetric Hertzian cracks evolving in graded glass/ceramic composites propelled by a rigid cylindrical punch are investigated employing a novel recursive method, called the stacked-node propagation procedure. Crack trajectories and their propagation susceptibilities are predicted via the minimum strain energy density (MSED) criterion regarding the crack growth resistance (R-curve) of ceramics. The stress trajectory approach is also considered for a homogeneous glass to reveal the reliance and effectiveness of the MSED criterion in the present crack problems. The Mori–Tanaka relations are adopted to model the elastic modulus and Poisson's ratio variations through the composites, which are implemented on the simulations via the homogeneous finite element approach. Hertzian crack problem of a practically producible graded composite comprised of oxynitride glass and a fine-grained silicon nitride ceramics (Si3N4) is treated as a case study. The degree of material gradation is assessed for the mitigation of surface crack initiation and propagation risks. © 2023 The Authors. Journal of the American Ceramic Society published by Wiley Periodicals LLC on behalf of American Ceramic Society.
引用
收藏
页码:4499 / 4514
相关论文
共 50 条
  • [31] FATIGUE CRACK-PROPAGATION IN GLASS-FIBER AND GLASS-SPHERE FILLED PBT COMPOSITES
    VOSS, H
    KARGERKOCSIS, J
    INTERNATIONAL JOURNAL OF FATIGUE, 1988, 10 (01) : 3 - 11
  • [32] Structural and strength degradation of canasite glass-ceramic at Hertzian contacts
    Chan, JY
    Mecholsky, JJ
    Anusavice, KJ
    JOURNAL OF DENTAL RESEARCH, 1996, 75 : 387 - 387
  • [33] Functionally graded ceramic/ceramic and metal/ceramic composites by electrophoretic deposition
    Sarkar, P
    Datta, S
    Nicholson, PS
    COMPOSITES PART B-ENGINEERING, 1997, 28 (1-2) : 49 - 56
  • [34] Curved crack propagation in homogeneous and graded materials
    Tilbrook, MT
    Moon, RJ
    Hoffman, M
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2005, 28 (11) : 939 - 950
  • [35] Crack propagation in fracture mechanical graded structures
    Schramm, B.
    Richard, H. A.
    FRATTURA ED INTEGRITA STRUTTURALE, 2015, 9 (34): : 280 - 289
  • [36] Influence of glass-ceramic thickness on Hertzian and bulk fracture mechanisms
    Tsai, YL
    Petsche, PE
    Anusavice, KJ
    Yang, MC
    INTERNATIONAL JOURNAL OF PROSTHODONTICS, 1998, 11 (01) : 27 - 32
  • [37] Glass ceramic composites for microsystems
    Schiller, WA
    Eberstein, M
    Müller, R
    GLASS SCIENCE AND TECHNOLOGY, 2003, 76 : 54 - 59
  • [38] THE HERTZIAN CONE CRACK
    LI, YZ
    HILLS, DA
    JOURNAL OF APPLIED MECHANICS-TRANSACTIONS OF THE ASME, 1991, 58 (01): : 120 - 127
  • [39] Crack bifurcation in laminar ceramic composites
    Oechsner, M
    Hillman, C
    Lange, FF
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1996, 79 (07) : 1834 - 1838
  • [40] Hertzian cone crack
    Li, Yingzhi, 1600, (58):