Crack bifurcation in laminar ceramic composites

被引:113
|
作者
Oechsner, M
Hillman, C
Lange, FF
机构
[1] Material Department, Univ. of California at Santa Barbara, Santa Barbara
关键词
D O I
10.1111/j.1151-2916.1996.tb08003.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Crack bifurcation was observed in laminar ceramic composites when cracks entered thin Al2O3 layers sandwiched between thicker layers of Zr(12Ce)O-2. The Al2O3 layers contained a biaxial, residual, compressive stress of approximate to 2 GPa developed due to differential contraction upon cooling from the processing temperature. The Zr(12Ce)O-2 layers were nearly free of residual, tensile stresses because they were much thicker than the Al2O3 layers. The ceramic composites were fabricated by a green tape and codensification method. Different specimens were fabricated to examine the effect of the thickness of the Al2O3, layer on the bifurcation phenomena. Bar specimens were fractured in four-point bending. When the propagating crack encountered the Al2O3 layer, it bifurcated as it approached the Zr(12Ce)O-2/ Al2O3 interface. After the crack bifurcated, it continued to propagate close to the center line of the Al2O3 layer. Fracture of the laminate continued after the primary crack reinitiated to propagate through the next Zr(12Ce)O-2 layer. where it bifurcated again as it entered the next Al2O3 layer. If the loading was stopped during bifurcation, the specimen could be unloaded prior to complete fracture. Although the residual stresses mere nearly identical in all Al2O3 layers, crack bifurcation was observed only when the layer thickness was greater than approximate to 70 mu m.
引用
收藏
页码:1834 / 1838
页数:5
相关论文
共 50 条
  • [1] Crack bifurcation in laminar ceramic composites
    Universitaet Karlsruhe, Karlsruhe, Germany
    J Am Ceram Soc, 7 (1834-1838):
  • [2] LAMINAR CERAMIC COMPOSITES
    CHARTIER, T
    MERLE, D
    BESSON, JL
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1995, 15 (02) : 101 - 107
  • [3] MODELING CRACK BIFURCATION IN LAMINAR CERAMICS
    Hbaieb, K.
    McMeeking, R. M.
    Lange, F. F.
    MECHANICAL PROPERTIES AND PERFORMANCE OF ENGINEERING CERAMICS AND COMPOSITES III, 2008, 28 (02): : 411 - +
  • [4] CVD OF LAMINAR CERAMIC COMPOSITES
    BECHT, JGM
    VANDERPUT, PJ
    SCHOONMAN, J
    SOLID STATE IONICS, 1988, 26 (02) : 148 - 148
  • [5] THE FABRICATION AND FAILURE OF LAMINAR CERAMIC COMPOSITES
    CLEGG, WJ
    ACTA METALLURGICA ET MATERIALIA, 1992, 40 (11): : 3085 - 3093
  • [6] Crack bifurcation features in laminar specimens with fixed total thickness
    Lugovy, M
    Orlovskaya, N
    Slyunyayev, V
    Gogotsi, G
    Kübler, J
    Sanchez-Herencia, AJ
    COMPOSITES SCIENCE AND TECHNOLOGY, 2002, 62 (06) : 819 - 830
  • [7] Crack bifurcation at the surface of laminar ceramics that exhibit a threshold strength
    Pontin, MG
    Lange, FF
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2005, 88 (05) : 1315 - 1317
  • [8] Modelling of Crack Bifurcation in Laminar Ceramics with Large Compressive Stress
    Kotoul, Michal
    Sevecek, Oldrich
    Profant, Tomas
    ADVANCES IN FRACTURE AND DAMAGE MECHANICS X, 2012, 488-489 : 130 - 133
  • [9] Crack bifurcation in laminar ceramics having large compressive stress
    Hbaieb, K.
    McMeeking, R. M.
    Lange, F. F.
    INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 2007, 44 (10) : 3328 - 3343
  • [10] New laminar-band ceramic metal composites
    Mater Technol, 4 (186-188):