Advanced biomimetic design strategies for porous structures promoting bone integration with additive-manufactured Ti6Al4V scaffolds

被引:0
|
作者
Li, Yongyue [1 ]
Han, Qing [1 ]
Chen, Hao [1 ]
Yang, Wenbo [1 ]
Xu, Yongjun [2 ]
Zhang, Yongqi [3 ]
Zhang, Jiangbo [1 ]
Liu, Li [1 ]
Zhang, Weilong [1 ]
Liu, Hao [1 ]
Chen, Bingpeng [1 ]
Wang, Jincheng [1 ]
机构
[1] Second Hosp Jilin Univ, Dept Orthoped, Changchun 130041, Peoples R China
[2] Wangqing Cty Peoples Hosp, Yanji 136200, Peoples R China
[3] Second Hosp Jilin Univ, Dept Nephrol & Rheumatol, Changchun 130041, Peoples R China
关键词
Porous scaffold; Implant; Gradient; Ti6Al4V; Bone ingrowth; OF-THE-ART; PORE-SIZE; OSTEOGENIC DIFFERENTIATION; MECHANICAL-PROPERTIES; ALLOY IMPLANTS; FABRICATION; TI-6AL-4V; TITANIUM; STEM; GEOMETRY;
D O I
10.1016/j.jmrt.2024.08.040
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The natural bone structure exhibits a radial gradient with dense cortical bone externally and porous cancellous bone internally. However, previous studies proposing scaffold designs have predominantly focused on homogeneous porous structures. Moreover, no consensus exists on the optimal structure for gradient porous scaffolds. Our scaffold closely imitated the natural bone structure by incorporating a gradient of pillar diameters. Additionally, we introduced a inverse gradient structure and three uniform diameter pillar structures (400 mu m, 600 mu m, and 1000 mu m) for comparative analysis. Mechanical testing revealed that the compressive strength and elastic modulus of the Ti6Al4V porous scaffolds gradually increased with an increase in pillar diameter. In vitro experiments demonstrated that both the biomimetic gradient and inverse gradient scaffolds promoted osteogenic differentiation, with higher ALP activity (alkaline phosphatase) and osteogenesis-related gene expression compared to the uniform pillar structure scaffolds. The in vivo experiments confirmed these results, highlighting the superior ability of the biomimetic gradient Ti6Al4V porous scaffold to induce new bone formation. Based on our findings, we suggest that the optimal porous structure should have fine-diameter pillars (approximately 400 mu m) internally to enhance cell penetration, while coarse-diameter pillars (approximately 800 mu m) should be used externally to increase the cell attachment area and enhance mechanical strength. Overall, our study contributes to the field of bone tissue engineering by providing a biomimetic scaffold design that closely imitates the structure of natural bone and promotes osteogenic activity.
引用
收藏
页码:1901 / 1915
页数:15
相关论文
共 50 条
  • [31] Fracture and failure behavior of additive manufactured Ti6Al4V lattice structures under compressive load
    Li, PeiYao
    Ma, Yu E.
    Sun, WenBo
    Qian, Xudong
    Zhang, Weihong
    Wang, ZhenHai
    ENGINEERING FRACTURE MECHANICS, 2021, 244
  • [32] Simultaneously achieving strength-ductility in additive-manufactured Ti6Al4V alloy via ultrasonic surface rolling process
    Zhou, Changhao
    Yan, Xinyu
    Liu, Dan
    Xu, Xingchen
    Cui, Junfeng
    Li, Mengyao
    Yuan, Chun
    Li, Hairong
    Liang, Yilong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2025, 920
  • [33] Dynamic tensile behavior of electron beam additive manufactured Ti6Al4V
    Rodriguez, O. L.
    Allison, P. G.
    Whittington, W. R.
    Francis, D. K.
    Rivera, O. G.
    Chou, K.
    Gong, X.
    Butler, T. M.
    Burroughs, J. F.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 641 : 323 - 327
  • [34] Investigation on the Microstructure of Direct Laser Additive Manufactured Ti6Al4V Alloy
    Han, Yuanfei
    Lu, Weijie
    Jarvis, Tom
    Shurvinton, John
    Wu, Xinhua
    MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS, 2015, 18 : 24 - 28
  • [35] The Experimental Assessment of Deformation and Springback Behavior for Additive Manufactured Ti6Al4V
    Kadir Aydın
    Mustafa Karamolla
    İbrahim Karaağaç
    Mehmet Okan Kabakçı
    Halit Doğan
    Arabian Journal for Science and Engineering, 2023, 48 : 11773 - 11780
  • [36] The Experimental Assessment of Deformation and Springback Behavior for Additive Manufactured Ti6Al4V
    Aydin, Kadir
    Karamolla, Mustafa
    Karaagac, Ibrahim
    Kabakci, Mehmet Okan
    Dogan, Halit
    ARABIAN JOURNAL FOR SCIENCE AND ENGINEERING, 2023, 48 (09) : 11773 - 11780
  • [37] Effects of Water Cooling on the Microstructure of Electron Beam Additive-Manufactured Ti-6Al-4V
    Panin, Alexey
    Martynov, Sergey
    Kazachenok, Marina
    Kazantseva, Lyudmila
    Bakulin, Alexander
    Kulkova, Svetlana
    Perevalova, Olga
    Sklyarova, Elena
    METALS, 2021, 11 (11)
  • [38] Mechanical behaviors and failure modes of additive manufactured Ti6Al4V lattice structures under compressive load
    Li, PeiYao
    Ma, Yu E.
    Sun, WenBo
    Qian, Xudong
    Zhang, Weihong
    Wang, ZhenHai
    THIN-WALLED STRUCTURES, 2022, 180
  • [39] Bionic mechanical design and SLM manufacture of porous Ti6Al4V scaffolds for load-bearing cancellous bone implants
    Liao, Bo
    Xu, Cheng
    Li, Wei
    Lu, Dong
    Jin, Zhong Min
    ACTA OF BIOENGINEERING AND BIOMECHANICS, 2021, 23 (03) : 97 - 107
  • [40] Mechanical properties of additively manufactured variable lattice structures of Ti6Al4V
    Traxel, Kellen D.
    Groden, Cory
    Valladares, Jesus
    Bandyopadhyay, Amit
    Keck, W. M.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 809