Fatigue and corrosion-fatigue behavior of the β-metastable Ti-5Al-5Mo-5V-3Cr alloy processed by laser powder bed fusion

被引:0
|
作者
Alcantara, Erika Gabriele Alves [1 ]
Meinke, Reinhard [1 ]
Selve, Soeren [2 ]
Kaya, Ali Can [3 ]
Fleck, Claudia [1 ]
机构
[1] Tech Univ Berlin, Inst Mat Sci & Technol, Fac Process Sci 3, Fachgebiet Werkstofftechn Chair Mat Sci & Engn, Str 17 Juni 135, D-10623 Berlin, Germany
[2] Tech Univ Berlin, Ctr Electron Microscopy ZELMI, Berlin, Germany
[3] Turkish German Univ, Dept Mechatron Engn, Sahinkaya Caddesi, Istanbul, Turkiye
关键词
additively manufactured Ti-5Al-5Mo-5V-3Cr; corrosion-fatigue; cyclic deformation behavior; fatigue-induced surface damage; fracture surface; high-cycle fatigue; DUCTILE FRACTURE-TOUGHNESS; TI-BASED ALLOYS; MECHANICAL-PROPERTIES; TENSILE PROPERTIES; ALPHA-PHASE; TITANIUM; MICROSTRUCTURE; STRENGTH; VOLUME;
D O I
10.1111/ffe.14394
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
We performed rotating bending tests and axial (tension-compression) load-increase and constant amplitude high-cycle fatigue tests in air and Hanks' balanced salt solution (HBSS) on the beta-metastable titanium alloy Ti-5Al-5Mo-5V-3Cr, processed by laser powder bed fusion (LPBF-M), solution-treated and aged, and shot-peened. Rotating bending loading in air revealed a strong influence of process-induced flaws on fatigue endurance. Especially in the high-cycle fatigue range and the transition region, the stochastic distribution of the flaws and flaw sizes led to a high scatter of the number of cycles to failure. The axial load-increase tests yielded a good fatigue life estimation, with a negligible difference between air and HBSS. The cyclic deformation behavior in HBSS was also strongly influenced by the local microstructure and defect distribution, and, thus, by crack formation and propagation. Plastic deformation and microcrack growth interact, and their relative amount resulted in different progressions of the plastic strain amplitude over the number of cycles for different specimens. Changes in the free corrosion potential and the corrosion current were highly sensitive indicators for fatigue-induced damage on the rough surfaces, which was correlated to the microscopic examination, fracture surface features, and the fatigue crack development. Failure starts at stochastically distributed inner flaws, yielding high scatter of Nf . Cyclic deformation behavior in HBSS depends on local microstructure and flaws. Simultaneous plastic deformation and microcrack growth influence epsilon a,p levels. Microscopy, electrochemistry, and surface fracture illustrate fatigue crack development.
引用
收藏
页码:3832 / 3847
页数:16
相关论文
共 50 条
  • [31] In situ study to understand the effect of cooling rate on the phase transformation behaviour of metastable β-Ti alloy, Ti-5Al-5Mo-5V-3Cr
    Sharma, Deepak
    Roebuck, Bryan
    Joshi, Shubham Sanjay
    Sharma, Rohit
    Fitzpatrick, Michael E.
    MATERIALS LETTERS, 2023, 353
  • [32] Transformations of Ti-5Al-5V-5Cr-3Mo powder due to reuse in laser powder bed fusion: A surface analytical approach
    Sen-Britain, Shohini T.
    Keilbart, Nathan D.
    Kweon, Kyoung E.
    Pham, Tuan Anh
    Orme, Chris A.
    Wood, Brandon C.
    Nelson, Art J.
    APPLIED SURFACE SCIENCE, 2021, 564
  • [33] Isothermal omega formation and evolution in the Beta-Ti alloy Ti-5Al-5Mo-5V-3Cr
    Coakley, James
    Radecka, Anna
    Dye, David
    Bagot, Paul A. J.
    Stone, Howard J.
    Seidman, David N.
    Isheim, Dieter
    PHILOSOPHICAL MAGAZINE LETTERS, 2016, 96 (11) : 416 - 424
  • [34] Microstructural evolution and its effect on the mechanical behavior of Ti-5Al-5Mo-5V-3Cr alloy during aging
    Jiang, Baozhen
    Emura, Satoshi
    Tsuchiya, Koichi
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 731 : 239 - 248
  • [35] Stress induced martensitic transformation in metastable β Ti-5Al-5Mo-5V-3Cr alloy: Triggering stress and interaction with deformation bands
    Zafari, Ahmad
    Xia, Kenong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 724 : 75 - 79
  • [36] Microstructure, Texture, and Mechanical Properties of β Solution-Treated and Aged Metastable β Titanium Alloy, Ti-5Al-5Mo-5V-3Cr
    Premkumar Manda
    Rama Manohar Samudrala
    M. K. Mohan
    A. K. Singh
    Metallurgical and Materials Transactions A, 2017, 48 : 4539 - 4552
  • [37] Microstructure, Texture, and Mechanical Properties of β Solution-Treated and Aged Metastable β Titanium Alloy, Ti-5Al-5Mo-5V-3Cr
    Manda, Premkumar
    Samudrala, Rama Manohar
    Mohan, M. K.
    Singh, A. K.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2017, 48A (10): : 4539 - 4552
  • [38] Processing-microstructure-yield strength correlation in a near β Ti alloy, Ti-5Al-5Mo-5V-3Cr
    Kar, Sujoy Kumar
    Suman, Swati
    Shivaprasad, S.
    Chaudhuri, Atanu
    Bhattacharjee, Amit
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 610 : 171 - 180
  • [39] High cycle fatigue behavior of Ti-5Al-5Mo-5V-3Cr-1Zr titanium alloy with bimodal microstructure
    Huang, Chaowen
    Zhao, Yongqing
    Xin, Shewei
    Zhou, Wei
    Li, Qian
    Zeng, Weidong
    Tan, Changsheng
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 695 : 1966 - 1975
  • [40] High cycle fatigue behavior of Ti-5Al-5Mo-5V-3Cr-1Zr titanium alloy with lamellar microstructure
    Huang, Chaowen
    Zhao, Yongqing
    Xin, Shewei
    Tan, Changsheng
    Zhou, Wei
    Li, Qian
    Zeng, Weidong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 682 : 107 - 116