Fatigue and corrosion-fatigue behavior of the β-metastable Ti-5Al-5Mo-5V-3Cr alloy processed by laser powder bed fusion

被引:0
|
作者
Alcantara, Erika Gabriele Alves [1 ]
Meinke, Reinhard [1 ]
Selve, Soeren [2 ]
Kaya, Ali Can [3 ]
Fleck, Claudia [1 ]
机构
[1] Tech Univ Berlin, Inst Mat Sci & Technol, Fac Process Sci 3, Fachgebiet Werkstofftechn Chair Mat Sci & Engn, Str 17 Juni 135, D-10623 Berlin, Germany
[2] Tech Univ Berlin, Ctr Electron Microscopy ZELMI, Berlin, Germany
[3] Turkish German Univ, Dept Mechatron Engn, Sahinkaya Caddesi, Istanbul, Turkiye
关键词
additively manufactured Ti-5Al-5Mo-5V-3Cr; corrosion-fatigue; cyclic deformation behavior; fatigue-induced surface damage; fracture surface; high-cycle fatigue; DUCTILE FRACTURE-TOUGHNESS; TI-BASED ALLOYS; MECHANICAL-PROPERTIES; TENSILE PROPERTIES; ALPHA-PHASE; TITANIUM; MICROSTRUCTURE; STRENGTH; VOLUME;
D O I
10.1111/ffe.14394
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
We performed rotating bending tests and axial (tension-compression) load-increase and constant amplitude high-cycle fatigue tests in air and Hanks' balanced salt solution (HBSS) on the beta-metastable titanium alloy Ti-5Al-5Mo-5V-3Cr, processed by laser powder bed fusion (LPBF-M), solution-treated and aged, and shot-peened. Rotating bending loading in air revealed a strong influence of process-induced flaws on fatigue endurance. Especially in the high-cycle fatigue range and the transition region, the stochastic distribution of the flaws and flaw sizes led to a high scatter of the number of cycles to failure. The axial load-increase tests yielded a good fatigue life estimation, with a negligible difference between air and HBSS. The cyclic deformation behavior in HBSS was also strongly influenced by the local microstructure and defect distribution, and, thus, by crack formation and propagation. Plastic deformation and microcrack growth interact, and their relative amount resulted in different progressions of the plastic strain amplitude over the number of cycles for different specimens. Changes in the free corrosion potential and the corrosion current were highly sensitive indicators for fatigue-induced damage on the rough surfaces, which was correlated to the microscopic examination, fracture surface features, and the fatigue crack development. Failure starts at stochastically distributed inner flaws, yielding high scatter of Nf . Cyclic deformation behavior in HBSS depends on local microstructure and flaws. Simultaneous plastic deformation and microcrack growth influence epsilon a,p levels. Microscopy, electrochemistry, and surface fracture illustrate fatigue crack development.
引用
收藏
页码:3832 / 3847
页数:16
相关论文
共 50 条
  • [21] The Role of High-Index Twinning on Hierarchical α Microstructure in a Metastable β Ti-5Al-5Mo-5V-3Cr Alloy
    Dian Li
    Xing Zhang
    Wenrui Zhao
    H. Darlene Merrill
    Noah T. Meyer
    Stoichko Antonov
    Yiliang Liao
    Yufeng Zheng
    JOM, 2021, 73 : 2303 - 2311
  • [22] The Role of High-Index Twinning on Hierarchical α Microstructure in a Metastable β Ti-5Al-5Mo-5V-3Cr Alloy
    Li, Dian
    Zhang, Xing
    Zhao, Wenrui
    Merrill, H. Darlene
    Meyer, Noah T.
    Antonov, Stoichko
    Liao, Yiliang
    Zheng, Yufeng
    JOM, 2021, 73 (08) : 2303 - 2311
  • [23] Microstructure, texture and mechanical properties of hot rolled metastable β-titanium alloy Ti-5Al-5Mo-5V-3Cr
    Manda, Premkumar
    Chakkingal, Uday
    Singh, A. K.
    MATERIALS TODAY-PROCEEDINGS, 2015, 2 (4-5) : 1118 - 1126
  • [24] Influence of cooling rate on the precipitation kinetics of nanoscale isothermal ω-phase in metastable β-Ti alloy, Ti-5Al-5Mo-5V-3Cr
    Sharma, Deepak
    Parfitt, David
    Chen, Bo
    Roebuck, Bryan
    Venero, Diego Alba
    Kada, Sitarama Raju
    Fabijanic, Daniel
    Fitzpatrick, Michael E.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 859
  • [25] Low cycle fatigue crack initiation in Ti-5Al-5Mo-5V-3Cr in relation to local crystallographic orientations
    Helstroffer, A.
    Hemery, S.
    Andrieu, S.
    Villechaise, P.
    MATERIALS LETTERS, 2020, 276 (276)
  • [26] On mechanism of flow softening in Ti-5Al-5Mo-5V-3Cr
    Jones, N. G.
    Jackson, M.
    MATERIALS SCIENCE AND TECHNOLOGY, 2011, 27 (06) : 1025 - 1032
  • [27] The influence of carbon on precipitation of α in Ti-5Al-5Mo-5V-3Cr
    Wain, N.
    Hao, X. J.
    Ravi, G. A.
    Wu, X.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (29-30): : 7673 - 7683
  • [28] Characterization of a previously unidentified ordered orthorhombic metastable phase in Ti-5Al-5Mo-5V-3Cr
    Zheng, Yufeng
    Williams, Robert E. A.
    Fraser, Hamish L.
    SCRIPTA MATERIALIA, 2016, 113 : 202 - 205
  • [29] Effect of cooling rate on tensile properties of Ti-5Al-5Mo-5V-3Cr alloy
    Fu Yanyan
    Hui Songxiao
    Ye Wenjun
    Mi Xujun
    METALLURGY TECHNOLOGY AND MATERIALS, 2012, 567 : 212 - 215
  • [30] Precipitation processes in the Beta-Titanium alloy Ti-5Al-5Mo-5V-3Cr
    Coakley, James
    Vorontsov, Vassili A.
    Jones, Nicholas G.
    Radecka, Anna
    Bagot, Paul A. J.
    Littrell, Kenneth C.
    Heenan, Richard K.
    Hu, Frederic
    Magyar, Andrew P.
    Bell, David C.
    Dye, David
    JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 646 : 946 - 953