The Deterioration of C-S-H Gel in a Severe Sulfate Environment

被引:0
|
作者
Liao, Wei [1 ]
Lu, Chunhua [1 ]
Xu, Zhongzi [1 ]
机构
[1] Nanjing Tech Univ, Coll Mat Sci & Engn, State Key Lab Mat Oriented Chem Engn, Nanjing 210009, Peoples R China
来源
SYMMETRY-BASEL | 2024年 / 16卷 / 06期
关键词
C-S-H gel; sulfate attack; microstructure; Si-29; MAS-NMR; chain length; CALCIUM SILICATE HYDRATE; CEMENT; ATTACK; CONCRETE; MODEL; CRYSTALLIZATION; MICROSTRUCTURE; DURABILITY; MECHANISM;
D O I
10.3390/sym16060703
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
Immersion tests with 5 wt.% Na2SO4 solution were carried out to investigate the deterioration of calcium silicate hydrate (C-S-H) gel in a sulfate environment. C-S-H gels with different Ca/(Si + Al) molar ratios were used for comparison. Particular attention was paid to the changes in element composition and Si-O-Si chain structure of the C-S-H gel. The results show that the C-S-H gels with a low Ca/(Si + Al) ratio (0.8-1.0) and appropriate Si-O-Si chain length (14.8) presented better stability in a severe sulfate environment. The C-S-H gels with a higher Ca/(Si + Al) ratio (>2.0) were more sensitive to the attack of sulfate ions. Calcium ions dissolved rapidly during the immersion process, causing the loss of cohesive strength of the C-S-H gel, and then decomposed into fine particles. The C-S-H gel with a lower Ca/(Si + Al) ratio (about 1.1) rarely leached out calcium ions and maintained good micromorphology. The Si-29 MAS-NMR results indicate that the Si-O-Si chains with too short or too long chain lengths will break and recombine under the attack of sulfate ions. The Si-O-Si chains with an appropriate chain length (14.8) maintained the stability of the structure of the C-S-H gel in a sulfate environment. These changes are closely related to the asymmetric layered structure of amorphous C-S-H gel. Partial calcium ions between the layers of the main chain structure of Si-O-Si are easily taken away by sulfate ions, leading to the structural instability of the C-S-H gel.
引用
收藏
页数:10
相关论文
共 50 条
  • [31] An atomistic building block description of C-S-H - Towards a realistic C-S-H model
    Mohamed, Aslam Kunhi
    Parker, Stephen C.
    Bowen, Paul
    Galmarini, Sandra
    CEMENT AND CONCRETE RESEARCH, 2018, 107 : 221 - 235
  • [32] A potential C-S-H nucleation mechanism: atomistic simulations of the portlandite to C-S-H transformation
    Aretxabaleta X.M.
    López-Zorrilla J.
    Labbez C.
    Etxebarria I.
    Manzano H.
    Cement and Concrete Research, 2022, 162
  • [33] Estimation of the poroelastic properties of calcium-silicate-hydrate (C-S-H) gel
    Hu, Chuanlin
    Gao, Yueyi
    Chen, Binmeng
    Zhang, Yamei
    Li, Zongjin
    MATERIALS & DESIGN, 2016, 92 : 107 - 113
  • [34] The nanogranular nature of C-S-H
    Constantinides, Georgios
    Ulm, Franz-Josef
    JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 2007, 55 (01) : 64 - 90
  • [35] INTERACTION OF CHLORIDE AND C-S-H
    BEAUDOIN, JJ
    RAMACHANDRAN, VS
    FELDMAN, RF
    CEMENT AND CONCRETE RESEARCH, 1990, 20 (06) : 875 - 883
  • [36] C-S-H and concrete properties
    Nonat, Andre
    CEMENT WAPNO BETON, 2010, 15 (06): : 315 - +
  • [37] Estimate the relative electrical conductivity of C-S-H gel from experimental results
    Ma, Hongyan
    Hou, Dongshuai
    Liu, Jun
    Li, Zongjin
    CONSTRUCTION AND BUILDING MATERIALS, 2014, 71 : 392 - 396
  • [38] Mechanical properties and microstructure characterization of calcium silicate hydrate (C-S-H) gel
    Qiao, Ling
    Guo, Li
    Hong, Jun
    Guo, Xiaoming
    ENERGY AND ENVIRONMENT MATERIAL S, 2010, 650 : 63 - 66
  • [39] Hydration Activity of Silica Fume and Its Effect on The Structure of C-S-H Gel
    Wang Lei
    He Zhen
    Yan Jianjun
    APPLIED MECHANICS AND MATERIALS I, PTS 1-3, 2013, 275-277 : 2084 - +
  • [40] In situ monitoring of C-S-H gel processing by magnetic susceptibility and turbidity measurements
    Wang, ZH
    Sun, LM
    Hou, YF
    Tang, EZ
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2005, 88 (07) : 1799 - 1802