The Deterioration of C-S-H Gel in a Severe Sulfate Environment

被引:0
|
作者
Liao, Wei [1 ]
Lu, Chunhua [1 ]
Xu, Zhongzi [1 ]
机构
[1] Nanjing Tech Univ, Coll Mat Sci & Engn, State Key Lab Mat Oriented Chem Engn, Nanjing 210009, Peoples R China
来源
SYMMETRY-BASEL | 2024年 / 16卷 / 06期
关键词
C-S-H gel; sulfate attack; microstructure; Si-29; MAS-NMR; chain length; CALCIUM SILICATE HYDRATE; CEMENT; ATTACK; CONCRETE; MODEL; CRYSTALLIZATION; MICROSTRUCTURE; DURABILITY; MECHANISM;
D O I
10.3390/sym16060703
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
Immersion tests with 5 wt.% Na2SO4 solution were carried out to investigate the deterioration of calcium silicate hydrate (C-S-H) gel in a sulfate environment. C-S-H gels with different Ca/(Si + Al) molar ratios were used for comparison. Particular attention was paid to the changes in element composition and Si-O-Si chain structure of the C-S-H gel. The results show that the C-S-H gels with a low Ca/(Si + Al) ratio (0.8-1.0) and appropriate Si-O-Si chain length (14.8) presented better stability in a severe sulfate environment. The C-S-H gels with a higher Ca/(Si + Al) ratio (>2.0) were more sensitive to the attack of sulfate ions. Calcium ions dissolved rapidly during the immersion process, causing the loss of cohesive strength of the C-S-H gel, and then decomposed into fine particles. The C-S-H gel with a lower Ca/(Si + Al) ratio (about 1.1) rarely leached out calcium ions and maintained good micromorphology. The Si-29 MAS-NMR results indicate that the Si-O-Si chains with too short or too long chain lengths will break and recombine under the attack of sulfate ions. The Si-O-Si chains with an appropriate chain length (14.8) maintained the stability of the structure of the C-S-H gel in a sulfate environment. These changes are closely related to the asymmetric layered structure of amorphous C-S-H gel. Partial calcium ions between the layers of the main chain structure of Si-O-Si are easily taken away by sulfate ions, leading to the structural instability of the C-S-H gel.
引用
收藏
页数:10
相关论文
共 50 条
  • [21] Rietveld refinement of the structures of 1.0 C-S-H and 1.5 C-S-H
    Battocchio, Francesco
    Monteiro, Paulo J. M.
    Wenk, Hans-Rudolf
    CEMENT AND CONCRETE RESEARCH, 2012, 42 (11) : 1534 - 1548
  • [22] Molecular dynamics simulation of C-S-H corrosion in chloride environment
    Zhang, Yunfeng
    Yang, Wendong
    Wang, Yingnan
    Gong, Zhicheng
    Zhang, Kaicheng
    MATERIALS TODAY COMMUNICATIONS, 2022, 33
  • [23] Permeability of C-S-H
    Honorio, Tulio
    CEMENT AND CONCRETE RESEARCH, 2024, 176
  • [24] Molecular dynamics of C-S-H production in graphene oxide environment
    Guo Kai
    He Miaohong
    Pan Wenhao
    Wu Jinguo
    REVIEWS ON ADVANCED MATERIALS SCIENCE, 2022, 61 (01) : 90 - 101
  • [25] Dissolution kinetics of C-S-H gel: Flow-through experiments
    Trapote-Barreira, Ana
    Cama, Jordi
    Soler, Josep M.
    PHYSICS AND CHEMISTRY OF THE EARTH, 2014, 70-71 : 17 - 31
  • [26] Micromechanics of hydrating cement pastes considering C-S-H gel densification
    Koenigsberger, M.
    Pichler, Bernhard
    Hellmich, Christian
    CONCREEP 10: MECHANICS AND PHYSICS OF CREEP, SHRINKAGE, AND DURABILITY OF CONCRETE AND CONCRETE STRUCTURES, 2015, : 574 - 583
  • [27] EFFECTS OF THE TEMPERATURE AND RELATIVE-HUMIDITY ON THE STRUCTURE OF C-S-H GEL
    CONG, XD
    KIRKPATRICK, RJ
    CEMENT AND CONCRETE RESEARCH, 1995, 25 (06) : 1237 - 1245
  • [28] Study on characteristics of siliceous materials used in the synthesis of C-S-H gel
    Hou, Yunfen
    Kuei Suan Jen Hsueh Pao/ Journal of the Chinese Ceramic Society, 2000, 28 (02): : 111 - 115
  • [29] Effect Investigation of Nanofillers on C-S-H Gel Structure with Si NMR
    Wang, Jialiang
    Han, Baoguo
    Li, Zhen
    Yu, Xun
    Dong, Xufeng
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2019, 31 (01)
  • [30] A remark on nano-particle stability of cement C-S-H gel
    Ficker, Tomas
    Len, Adel
    Martisek, Dalibor
    CENTRAL EUROPEAN JOURNAL OF PHYSICS, 2011, 9 (02): : 553 - 557