Optimization of machining parameters for turning operation of heat-treated Ti-6Al-3Mo-2Nb-2Sn-2Zr-1.5Cr alloy by Taguchi method

被引:2
|
作者
Elshaer, Ramadan N. [1 ]
El-Aty, Ali Abd [2 ,3 ]
Sayed, Esraa M. [2 ]
Barakat, Azza F. [2 ]
Sobh, Arafa S. [2 ,4 ]
机构
[1] Tabbin Inst Met Studies, Cairo, Egypt
[2] Helwan Univ, Fac Engn, Mech Engn Dept, Cairo, Egypt
[3] Prince Sattam bin Abdulaziz Univ, Coll Engn Al Kharj, Mech Engn Dept, Al Kharj 11942, Saudi Arabia
[4] Nile Univ, Sch Engn & Appl Sci, Giza, Egypt
来源
SCIENTIFIC REPORTS | 2024年 / 14卷 / 01期
关键词
Heat treatment; Turning parameters; TC21; Wear of tool insert; Surface roughness; TITANIUM-ALLOY; TOOL LIFE; MACHINABILITY; TC21;
D O I
10.1038/s41598-024-65786-8
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
TC21 alloy is a high-strength titanium alloy that has been gaining attention in various industries for its excellent combination of strength, toughness, and corrosion resistance. Given that this alloy is hard to cut material, therefore this study aims to optimize the process parameters of Turing this alloy under different conditions (i.e. as-received alloy, and heat-treated alloy). The L9 Taguchi approach-base orthogonal array is used to determine the optimum cutting parameters and the least number of experimental trials required. The achievement of this target, three different cutting parameters are used in the experimental work; each cutting parameter has three levels. The cutting speeds are chosen as 120, 100, and 80 m/min. The feed rates' values are 0.15, 0.1, and 0.05, mm/rev, and the depth of cut values are 0.6, 0.4, and 0.2 mm. After applying three steps of heat treatment (First step: is heating the sample to 920 degrees C for 1 h then decreasing to 820 degrees C also for 1 h, second step: cooling the sample to room temperature by water quenching (WQ), the third step: holding the sample at 600 degrees C for 4 h (Aging process)). The results revealed that the triple heat treatment led to the change in the microstructure from (alpha + beta) to (alpha + beta) with secondary alpha platelets (alpha s) formed in residual beta matrix leading to a decreased surface roughness by 56.25% and tool wear by 24.18%. The two most critical factors that affect the tool insert wear and surface roughness are the death of cut and cutting speed, which contribute 46.6% and 46.7% of the total, respectively. Feed rate, on the other hand, has the least importance, contributing 20.2% and 31.9% respectively.
引用
收藏
页数:14
相关论文
共 50 条
  • [41] Experimental studies on the dynamic tensile behavior of Ti-6Al-2Sn-2Zr-3Mo-1Cr-2Nb-Si alloy with Widmanstatten microstructure at elevated temperatures
    Gong, Xuhui
    Wang, Yu
    Xia, Yuanming
    Ge, Peng
    Zhao, Yongqing
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 523 (1-2): : 53 - 59
  • [42] Development of a Free-Machining (+) Titanium Alloy Based on Ti-6Al-2Sn-4Zr-6Mo
    Hussain, M. S.
    Siemers, C.
    Roesler, J.
    MATERIALS AND MANUFACTURING PROCESSES, 2013, 28 (05) : 545 - 549
  • [43] Effect of Strain Hardening and Aging Processes on Microstructure Evolution, Tensile and Fatigue Properties of Cast Ti-6Al-2Sn-2Zr–2Mo-1.5Cr-2Nb-0.1Si Alloy
    Ramadan N. Elshaer
    Mostafa S. S. El-Deeb
    S. S. Mohamed
    Khaled M. Ibrahim
    International Journal of Metalcasting, 2022, 16 : 723 - 737
  • [44] HYDROGEN EMBRITTLEMENT OF TI-6AL-2SN-4ZR-6MO ALLOY
    NIINOMI, M
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 72 (05): : S738 - S738
  • [45] HYDROGEN EMBRITTLEMENT OF TI-6AL-2SN-4ZR-6MO ALLOY
    NIINOMI, M
    SUZUKI, K
    KOBAYASHI, T
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 26 (08) : B286 - B286
  • [46] Pseudoelastic behaviour of a β Ti-25Nb-3Zr-3Mo-2Sn alloy
    Kent, D.
    Wang, G.
    Yu, Z.
    Dargusch, M. S.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (09): : 2246 - 2252
  • [47] Influence of Heat Treatment on the Pseudoelastic Behaviour of a β Ti-25Nb-3Zr-3Mo-2Sn Alloy
    Kent, Damon
    Wang, Gui
    Zheng, Li-Hui
    Yu, Zhentao
    Dargusch, Matthew
    PRICM 7, PTS 1-3, 2010, 654-656 : 871 - +
  • [48] Effect of Heat Treatment on Mechanical Properties of a Novel Ti-6Al-2Mo-2V-3Nb-2Fe-1Zr Alloy
    Peng, Wenfei
    Huang, Qiaodong
    Moliar, Oleksandr
    Dong, Chaoqi
    Wang, Xiaofeng
    Cailiao Yanjiu Xuebao/Chinese Journal of Materials Research, 2024, 38 (07): : 519 - 528
  • [49] An evaluation of the damage tolerance characteristics of Ti-6Al-2Sn-2Zr-2Mo-2Cr sheet
    Bayha, TD
    Yaney, DL
    LIGHT WEIGHT ALLOYS FOR AEROSPACE APPLICATIONS IV, 1996, : 183 - 194
  • [50] Effect of microstructure on fracture characteristics of Ti-6Al-2Sn-2Zr-2Mo-2Cr-Si
    Niinomi, M., 2001, Minerals, Metals and Materials Society (32):