Optimization of machining parameters for turning operation of heat-treated Ti-6Al-3Mo-2Nb-2Sn-2Zr-1.5Cr alloy by Taguchi method

被引:2
|
作者
Elshaer, Ramadan N. [1 ]
El-Aty, Ali Abd [2 ,3 ]
Sayed, Esraa M. [2 ]
Barakat, Azza F. [2 ]
Sobh, Arafa S. [2 ,4 ]
机构
[1] Tabbin Inst Met Studies, Cairo, Egypt
[2] Helwan Univ, Fac Engn, Mech Engn Dept, Cairo, Egypt
[3] Prince Sattam bin Abdulaziz Univ, Coll Engn Al Kharj, Mech Engn Dept, Al Kharj 11942, Saudi Arabia
[4] Nile Univ, Sch Engn & Appl Sci, Giza, Egypt
来源
SCIENTIFIC REPORTS | 2024年 / 14卷 / 01期
关键词
Heat treatment; Turning parameters; TC21; Wear of tool insert; Surface roughness; TITANIUM-ALLOY; TOOL LIFE; MACHINABILITY; TC21;
D O I
10.1038/s41598-024-65786-8
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
TC21 alloy is a high-strength titanium alloy that has been gaining attention in various industries for its excellent combination of strength, toughness, and corrosion resistance. Given that this alloy is hard to cut material, therefore this study aims to optimize the process parameters of Turing this alloy under different conditions (i.e. as-received alloy, and heat-treated alloy). The L9 Taguchi approach-base orthogonal array is used to determine the optimum cutting parameters and the least number of experimental trials required. The achievement of this target, three different cutting parameters are used in the experimental work; each cutting parameter has three levels. The cutting speeds are chosen as 120, 100, and 80 m/min. The feed rates' values are 0.15, 0.1, and 0.05, mm/rev, and the depth of cut values are 0.6, 0.4, and 0.2 mm. After applying three steps of heat treatment (First step: is heating the sample to 920 degrees C for 1 h then decreasing to 820 degrees C also for 1 h, second step: cooling the sample to room temperature by water quenching (WQ), the third step: holding the sample at 600 degrees C for 4 h (Aging process)). The results revealed that the triple heat treatment led to the change in the microstructure from (alpha + beta) to (alpha + beta) with secondary alpha platelets (alpha s) formed in residual beta matrix leading to a decreased surface roughness by 56.25% and tool wear by 24.18%. The two most critical factors that affect the tool insert wear and surface roughness are the death of cut and cutting speed, which contribute 46.6% and 46.7% of the total, respectively. Feed rate, on the other hand, has the least importance, contributing 20.2% and 31.9% respectively.
引用
收藏
页数:14
相关论文
共 50 条
  • [21] Influence of α-Phase Morphology on Mechanical Characteristics, Cycle Oxidation, and Hot Corrosion Behavior of Ti-6Al-3Mo-2Nb-2Zr-2Sn-1.5Cr Alloy
    Ahmed, Fathy S.
    El-Zomor, Mohamed A.
    Ghazala, Magdy S. Abo
    Elshaer, Ramadan N.
    METALLOGRAPHY MICROSTRUCTURE AND ANALYSIS, 2022, 11 (05) : 746 - 760
  • [22] The fatigue limit of Ti-6Al-2Zr-2Sn-3Mo-1Cr-2Nb titanium alloy with different colony features
    Shi, Xiaohui
    Zeng, Weidong
    Zhao, Qinyang
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 645 : 82 - 87
  • [23] Modelling Predication of Flow Stress and Grain Size in the High Temperature Deformation of Ti-6Al-2Zr-2Sn-2Mo- 1.5Cr-2Nb Alloy
    高温变形过程中Ti-6Al-2Zr-2Sn-2Mo-1.5Cr-2Nb合金的流动应力和晶粒尺寸的模型预测
    Luo, Jiao (luojiao@nwpu.edu.cn), 1716, Science Press (47):
  • [24] Effect of heat treatment and silicon addition on the microstructure development of Ti-6Al-2Cr-2Mo-2Sn-2Zr alloy
    Zhang, XD
    Bonniwell, P
    Fraser, HL
    Baeslack, WA
    Evans, DJ
    Ginter, T
    Bayha, T
    Cornell, B
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 343 (1-2): : 210 - 226
  • [25] Solidification Microstructure of Laser Additive Manufactured Ti—6Al—2Zr—2Sn—3Mo—1.5Cr—2Nb Titanium Alloy
    Qiang Zhang
    Jing Chen
    Lilin Wang
    Hua Tan
    Xin Lin
    Weidong Huang
    JournalofMaterialsScience&Technology, 2016, 32 (04) : 381 - 386
  • [26] Comparisons of phenomenological and physically based constitutive models for Ti–6Al–2Zr–2Sn–3Mo–1.5Cr–2Nb alloy
    Hun Pak
    Kyong Ho Sim
    Yun Chol Ri
    Ri Sung Kim
    Jong Hye Ri
    Applied Physics A, 2023, 129
  • [27] Effect of stretching on the strength (Bauschinger effect) of Ti-6Al-2Cr-2Mo-2Sn-2Zr alloy
    Zhang, XD
    Ginter, TJ
    Cornell, B
    Evans, DJ
    Fraser, HL
    JOURNAL OF ADVANCED MATERIALS, 2000, 32 (01): : 34 - 38
  • [28] Effect of stretching on the strength (Bauschinger effect) of Ti-6Al-2Cr-2Mo-2Sn-2Zr alloy
    Zhang, Xiao-Dong
    Ginter, Timothy J.
    Cornell, Brian
    Evans, Dan J.
    Fraser, Hamish L.
    1600, SAMPE, Covina, CA, United States (32):
  • [29] Effect of microstructure on fracture characteristics of Ti-6Al-2Sn-2Mo-2Zr-2Cr-Si alloy
    Niinomi, M
    Fukunaga, K
    Tono, G
    Koike, J
    Eylon, D
    Fujishiro, S
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2001, 87 (01): : 55 - 62
  • [30] Ultrasonically assisted turning of Ti-6Al-2Sn-4Zr-6Mo
    Muhammad, R.
    Maurotto, A.
    Roy, A.
    Silberschmidt, V. V.
    MODERN PRACTICE IN STRESS AND VIBRATION ANALYSIS 2012 (MPSVA 2012), 2012, 382