Effect of Sintering Temperature on Aging Resistance and Mechanical Properties of 3Y-TZP Dental Ceramic

被引:0
|
作者
张静超 [1 ,2 ,3 ]
李伟 [1 ,2 ]
机构
[1] State Key Laboratory of Oral Diseases,Sichuan University
[2] West China College of Stomatology,Sichuan University
[3] Hainan Stomatological
关键词
D O I
暂无
中图分类号
学科分类号
摘要
In order to investigate the effect of sintering temperature on aging properties and mechanical properties of 3Y-TZP dental ceramic in simulated oral environment,3Y-TZP nanopowder compacts were pressurelessly sintered at 1 350 ℃,1 400 ℃,1 450 ℃,1 500 ℃,respectively,then were treated by soaking in artificial saliva(65 ℃,pH=7)for two months.The treated specimens sintered at 1 350 ℃ showed there was no phase transformation but whose strength and toughnesswere significantly improved(P<0.05),while those sintered at 1 400 ℃-1 500 ℃ revealed a small amount of phase transformation and insignifi cant mechanical reinforcement(P>0.05).No micro-cracks were detected but increment in lattice volume was found in all specimens.Lowering sintering temperature favors aging resistance and mechanical reinforcement of 3Y-TZP in a simulated oral environment.
引用
收藏
页码:316 / 320
页数:5
相关论文
共 50 条
  • [21] Preparation and Properties of 3Y-TZP Ceramic Tools
    Chen, Zhiwei
    Feng, Liu
    Niu, Jinye
    TESTING AND EVALUATION OF INORGANIC MATERIALS I, 2011, 177 : 373 - 377
  • [22] Investigation of mechanical properties and low-temperature degradation of dental 3Y-TZP ceramics fabricated by stereolithography in combination with microwave sintering
    Wang, Li
    Jiao, Yang
    Yao, Lian
    Sheng, Yang
    Hao, Zongdong
    Tang, Weizhe
    Dou, Rui
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2023, 148
  • [23] Lowering of sintering temperature of 3Y-TZP by CuO additive
    Lemaire, L
    Scholz, SM
    Valmalette, JC
    EUROMAT 97 - PROCEEDINGS OF THE 5TH EUROPEAN CONFERENCE ON ADVANCED MATERIALS AND PROCESSES AND APPLICATIONS: MATERIALS, FUNCTIONALITY & DESIGN, VOL 2: POLYMERS AND CERAMICS, 1997, : 303 - 306
  • [24] Effect of low-temperature aging on friction and wear properties of 3Y-TZP ceramics
    Lu, Qing
    Liang, Xiao-Ping
    Wang, Guang-Hui
    Mocaxue Xuebao/Tribology, 2010, 30 (01): : 64 - 67
  • [25] Influence of sintering profile on the mechanical properties of manganese oxide doped 3Y-TZP
    Theenagaran, S.
    Chin, K. L.
    Jun, H. K.
    Liang, M. S.
    Ng, C. K.
    Ramesh, S.
    Teng, W. D.
    Ting, C. H.
    INTERNATIONAL CONFERENCE ON SUSTAINABLE ENERGY AND GREEN TECHNOLOGY 2019, 2020, 463
  • [26] Microstructural changes in ground 3Y-TZP and their effect on mechanical properties
    Munoz-Tabares, J. A.
    Jimenez-Pique, E.
    Reyes-Gasga, J.
    Anglada, M.
    ACTA MATERIALIA, 2011, 59 (17) : 6670 - 6683
  • [27] Impact strengthening of 3Y-TZP dental ceramic root posts
    Kocjan, Andraz
    Abram, Anze
    Dakskobler, Ales
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2020, 40 (14) : 4765 - 4773
  • [28] EFFECT OF GRAIN SIZE ON MECHANICAL PROPERTIES OF 3Y-TZP CERAMICS
    Trunec, Martin
    CERAMICS-SILIKATY, 2008, 52 (03) : 165 - 171
  • [29] Effects of external staining on mechanical, optical, and biocompatibility properties of additively manufactured 3Y-TZP ceramic for dental applications
    Zhou, Tianhong
    Zhu, Li
    Luo, Xiaonan
    Yu, Jiancheng
    Ye, Chuchu
    Zhou, Xin
    Tong, Xian
    Chen, Zhaoping
    Li, Yuncang
    Lin, Jixing
    Wen, Cuie
    Ma, Jianfeng
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 31 : 3961 - 3970
  • [30] A critical review on sintering and mechanical processing of 3Y-TZP ceramics
    Yin, Youkang
    Xu, Jinyang
    Ji, Min
    Li, Linfeng
    Chen, Ming
    CERAMICS INTERNATIONAL, 2023, 49 (02) : 1549 - 1571