Effects of external staining on mechanical, optical, and biocompatibility properties of additively manufactured 3Y-TZP ceramic for dental applications

被引:0
|
作者
Zhou, Tianhong [1 ]
Zhu, Li [1 ]
Luo, Xiaonan [1 ]
Yu, Jiancheng [1 ]
Ye, Chuchu [1 ]
Zhou, Xin [1 ]
Tong, Xian [1 ]
Chen, Zhaoping [1 ]
Li, Yuncang [2 ]
Lin, Jixing [1 ]
Wen, Cuie [2 ]
Ma, Jianfeng [1 ]
机构
[1] Wenzhou Med Univ, Sch Hosp Stomatol, Inst Stomatol, Wenzhou 325027, Peoples R China
[2] RMIT Univ, Ctr Addit Mfg, Sch Engn, Melbourne, Vic 3001, Australia
基金
澳大利亚研究理事会; 中国国家自然科学基金;
关键词
Additive manufacturing; Optical property; Staining; Zirconia ceramic; FLEXURAL STRENGTH; COLORING LIQUIDS; IN-VITRO; ZIRCONIA; SURFACE; TEETH;
D O I
10.1016/j.jmrt.2024.07.126
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Three mole percent yttria-stabilized tetragonal zirconia polycrystal (3Y-TZP) ceramics are exemplary materials for dental restoration due to their high mechanical strength, fracture toughness, chemical endurance, and biocompatibility. Nevertheless, 3Y-TZP ceramics are opaque and their CAD/CAM manufacturing process may cause micro-cracks in conventional clinical practice. In this study, 3Y-TZP ceramic samples were prepared using vat photopolymerization, pre-sintering, external staining, and final high-temperature sintering. The microstructures, mechanical properties, optical properties, and cytotoxicity of the 3Y-TZP ceramic samples were investigated. The results indicate that with increasing Fe3+ concentration of staining solution from 0.1 mol/L to 0.3 mol/L and increasing staining time from 5 s to 30 min, the 3Y-TZP ceramic samples showed a tetragonal crystal structure of zirconia with densely packed grains and a slight increase in grain size. The flexural strength, Vickers hardness, and fracture toughness of 3Y-TZP ceramic samples stained in 0.1-0.3 mol/L Fe3+ solution for 5 s to 3 min were all greater than 665 MPa, 11.9 GPa, and 5 MPa m1/2, respectively, meeting the mechanical requirements for clinical application. Colorimetric analysis revealed a decrease in L* (black-white index) from 90.4 to 81.3, an increase in a* (green-red index) from -1.5 to 3.2, and an increase in b* (blue-yellow index) from 11.6 to 20.3, approximating the commercial VITA 3D-Master Shade Guide chromaticity. Furthermore, the 3YTZP ceramic samples exhibited a cell viability of 90% or higher toward L929 cells.
引用
收藏
页码:3961 / 3970
页数:10
相关论文
共 50 条
  • [1] Effect of Sintering Conditions on Mechanical and Optical Properties of 3Y-TZP Dental Ceramic
    Dateraksa, Kannigar
    Ngernbamrung, Sukunthakan
    McCuiston, Ryan
    TRADITIONAL AND ADVANCED CERAMICS, 2014, 608 : 181 - +
  • [2] INFLUENCE OF PROCESSING ON MECHANICAL PROPERTIES OF 3Y-TZP FOR DENTAL APPLICATIONS
    Aboras, Mohamed
    Muchtar, Andanastuti
    Azhari, Che Husna
    Yahaya, Norziha
    Hao, Chin Chuin
    JURNAL TEKNOLOGI, 2016, 78 (11-3): : 7 - 12
  • [3] Mechanical, low temperature degradation, and biocompatibility of Al-doped dental 3Y-TZP ceramic
    Wang, Zihan
    Luo, Shao-hua
    Li, Peng-yu
    Guo, Song
    Yan, Sheng-xue
    CERAMICS INTERNATIONAL, 2024, 50 (02) : 3997 - 4004
  • [4] Effect of Sintering Temperature on Microscopic and Mechanical Properties of 3Y-TZP Dental Ceramic
    Zhang, Jingchao
    Liao, Yunmao
    Li, Wei
    Mo, Anchun
    INEC: 2010 3RD INTERNATIONAL NANOELECTRONICS CONFERENCE, VOLS 1 AND 2, 2010, : 1434 - 1435
  • [5] Effects of Aging on the Mechanical Properties of Dental Pigmented 3Y-TZP Ceramics
    Yi, Yuanfu
    Wen, Ning
    Bin, Den
    Shao, Longquan
    Wang, Chen
    Tian, Jiemo
    TESTING AND EVALUATION OF INORGANIC MATERIALS I, 2011, 177 : 136 - +
  • [6] Effect of sintering temperature on aging resistance and mechanical properties of 3Y-TZP dental ceramic
    Jingchao Zhang
    Yongqi Zhao
    Yunmao Liao
    Li Jiang
    Xiaofei Yun
    Wei Li
    Journal of Wuhan University of Technology-Mater. Sci. Ed., 2012, 27 : 316 - 320
  • [7] Effect of Sintering Temperature on Aging Resistance and Mechanical Properties of 3Y-TZP Dental Ceramic
    张静超
    李伟
    Journal of Wuhan University of Technology(Materials Science), 2012, (02) : 316 - 320
  • [8] Effect of Sintering Temperature on Aging Resistance and Mechanical Properties of 3Y-TZP Dental Ceramic
    Zhang Jingchao
    Zhao Yongqi
    Liao Yunmao
    Jiang Li
    Yun Xiaofei
    Li Wei
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2012, 27 (02): : 316 - 320
  • [9] Effect of Sintering Temperature on Aging Resistance and Mechanical Properties of 3Y-TZP Dental Ceramic
    张静超
    李伟
    Journal of Wuhan University of Technology(Materials Science Edition), 2012, 27 (02) : 316 - 320
  • [10] Preparation and Properties of 3Y-TZP Ceramic Tools
    Chen, Zhiwei
    Feng, Liu
    Niu, Jinye
    TESTING AND EVALUATION OF INORGANIC MATERIALS I, 2011, 177 : 373 - 377