Minimizing pest aluminum in magnesium for the production of high-purity titanium

被引:0
|
作者
Bo Yang
Rui Zheng
Ge Wu
Zhi-Min Chang
Zhi-Wei Shan
机构
[1] Engineering Research Center for Magnesium-based New Materials
[2] Center for Advancing Materials Performance from the Nanoscale (CAMP-Nano)
[3] State Key Laboratory for Mechanical Behavior of Materials
[4] Xi’an Jiaotong
关键词
D O I
暂无
中图分类号
TG146.23 [];
学科分类号
摘要
It is practically difficult to find titanium sponges with low and stable aluminum impurities on the market even though it is the precondition to prepare high-purity titanium. Analysis indicates that almost all the aluminum impurities in the titanium sponge are inherited from the magnesium used to reduce titanium tetrachloride. However, it remains elusive for decades why magnesium produced through the silicothermic reduction method contains a high content of aluminum impurities with large fluctuations. By recourse to thermodynamic calculations and comparative experiments, we demonstrate that fluorite, a material used as a catalyst in the silicothermic reduction method to produce magnesium, is the chief culprit for the pest aluminum and propose a mechanism to rationalize the observed phenomena. Our findings indicate that one practical way to produce qualified magnesium for the production of high-purity titanium is to abandon fluorite during the production of magnesium with the silicothermic reduction method.
引用
收藏
页码:4189 / 4196
页数:8
相关论文
共 50 条
  • [31] PRODUCTION OF HIGH-PURITY SILICIUM
    DRIOLE, J
    BONNIER, E
    METALL, 1971, 25 (01): : 2 - &
  • [32] PRODUCTION OF HIGH-PURITY NICKEL
    PLYUSHCHEVA, SV
    MALYAREVICH, LV
    KOPETSKIY, CV
    RUSSIAN METALLURGY, 1976, (06): : 21 - 24
  • [33] PRODUCTION OF HIGH-PURITY CESIUM
    BLATTER, F
    SCHUMACHER, E
    JOURNAL OF THE LESS-COMMON METALS, 1986, 115 (02): : 307 - 313
  • [34] Preparation of high-purity and ultrafine magnesium oxide
    Guo K.
    Yang X.
    Liu Z.
    Xu H.
    Huang H.
    Cailiao Daobao/Materials Review, 2016, 30 (06): : 95 - 99
  • [35] PRODUCTION OF HIGH-PURITY VANADIUM, CHROMIUM AND TITANIUM FOR USE IN LOW ACTIVATION MATERIALS
    MURPHY, D
    BUTTERWORTH, GJ
    JOURNAL OF NUCLEAR MATERIALS, 1992, 191 : 1444 - 1449
  • [36] Friction Contrast of High-Purity Titanium in Microscale
    Zhifeng Shi
    Yanfei Fang
    Yu Tian
    Liran Ma
    Tribology Letters, 2021, 69
  • [37] Compressive Twinning Behavior in High-purity Titanium
    Ren Yi
    Zhang Xiyan
    Sun Qi
    Liu Qing
    RARE METAL MATERIALS AND ENGINEERING, 2018, 47 (07) : 2061 - 2066
  • [38] Friction Contrast of High-Purity Titanium in Microscale
    Shi, Zhifeng
    Fang, Yanfei
    Tian, Yu
    Ma, Liran
    TRIBOLOGY LETTERS, 2021, 69 (04)
  • [39] The Isothermal Oxidation of High-Purity Aluminum at High Temperature
    Coker, Eric N.
    Donaldson, Burl
    Gill, Walter
    Yilmaz, Nadir
    Vigil, Francisco M.
    APPLIED SCIENCES-BASEL, 2023, 13 (01):
  • [40] PRODUCTION OF HIGH-PURITY ALUMINUM CRYSTALS BY A MODIFIED STRAIN-ANNEAL METHOD
    LEIGHLY, HP
    PERKINS, FC
    TRANSACTIONS OF THE AMERICAN INSTITUTE OF MINING AND METALLURGICAL ENGINEERS, 1960, 218 (02): : 379 - 380