摘要
Chevron-notch short-rod fracture toughness (K(Iv)) and scanning electron microscopy analyses of leucite-, tetrasilicic fluormica-, and alumina- reinforced dental ceramics and control materials were investigated. Shortrod fracture toughness is a measure of the bulk resistance to crack propagation but not of the surface resistance to crack initiation. Results indicated significant differences in K(Iv) among the following six groups (from lowest to highest (a) Dicor and Optec, (b) Optec, Excelco's Incisal, Macor and Excelco's Gingival, (c) Excelco's Brush-O-Paque, (d) Vitadur-N core, (e) Corning's 9606 glass-ceramic, and (f) Vita Hi Ceram. Good agreement occurred with published data for Macor and 9606. Comparisons of K(Iv)'s to published bending properties revealed poor correlation with both Dicor and Optec. This was attributed to sample geometry and surface preparational differences between short-rod and bending samples. Fractography analysis revealed the brittle nature of the glassy matrix with all fractured surfaces. The alumina particles inhibited crack propagation by pinning the crack at the particle-matrix interface. The fluormica and leucite phases revealed a higher incidence for cleavage fracture. The opaque particles offered some reinforcement effect.
引用
收藏
页码:265 / 278
页数:14
相关论文
共 50 条
  • [21] EVALUATION OF STATIC AND DYNAMIC FRACTURE-TOUGHNESS IN CERAMICS
    KOBAYASHI, T
    MATSUNUMA, K
    IKAWA, H
    MOTOYOSHI, K
    ENGINEERING FRACTURE MECHANICS, 1988, 31 (05) : 873 - 885
  • [22] THE FRACTURE-TOUGHNESS OF PARTICULATE-REINFORCED CERAMICS
    SMITH, E
    INTERNATIONAL JOURNAL OF FRACTURE, 1989, 40 (02) : R27 - R30
  • [23] FRACTURE-TOUGHNESS MEASUREMENTS OF DENTAL COMPOSITE RESINS
    PILLIAR, RM
    MARIC, B
    SMITH, DC
    ZINS, D
    JOURNAL OF DENTAL RESEARCH, 1983, 62 : 285 - 285
  • [24] THE RELATIVE FRACTURE-TOUGHNESS OF COMMERCIAL DENTAL COMPOSITES
    WHITE, BM
    SEGHI, RR
    JOURNAL OF DENTAL RESEARCH, 1995, 74 : 30 - 30
  • [25] VARIABLES AFFECTING THE FRACTURE-TOUGHNESS OF DENTAL COMPOSITES
    FERRACANE, JL
    ANTONIO, RC
    MATSUMOTO, H
    JOURNAL OF DENTAL RESEARCH, 1987, 66 (06) : 1140 - 1145
  • [26] INFLUENCE OF MOLECULAR-WEIGHT ON FRACTURE-TOUGHNESS AND FRACTOGRAPHY OF GLASSY-POLYMERS
    GRECO, R
    RAGOSTA, G
    PLASTICS AND RUBBER PROCESSING AND APPLICATIONS, 1987, 7 (03): : 163 - 171
  • [27] THE FRACTURE-TOUGHNESS TESTING OF CERAMICS AND ACOUSTIC-EMISSION
    DALGLEISH, BJ
    PRATT, PL
    RAWLINGS, RD
    FAKHR, A
    MATERIALS SCIENCE AND ENGINEERING, 1980, 45 (01): : 9 - 20
  • [28] IMPROVED FRACTURE-TOUGHNESS OF SIC-BASED CERAMICS
    LORENZ, J
    GAUCKLER, LJ
    PETZOW, G
    AMERICAN CERAMIC SOCIETY BULLETIN, 1979, 58 (03): : 338 - 338
  • [29] MEASURING THE FRACTURE-TOUGHNESS OF CERAMICS BY MEANS OF A HARDNESS TESTER
    KROUPA, F
    HNILICA, F
    SILIKATY, 1985, 29 (02): : 157 - +
  • [30] APPLICATION OF INDENTATION TECHNIQUE IN DETERMINING FRACTURE-TOUGHNESS OF CERAMICS
    XIA, SB
    LI, GX
    LI, CC
    ENGINEERING FRACTURE MECHANICS, 1988, 31 (02) : 309 - 313