Temperature dependency of strength of a unidirectional Sic fiber-reinforced (BaSr)Al2Si2O8 celsian composite

被引:0
|
作者
Unal, O [1 ]
Bansal, NP [1 ]
机构
[1] US DOE, Ames Lab, Ames, IA 50010 USA
关键词
D O I
暂无
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Temperature dependency of strength of a high Nicalon-(BaSr)Al2Si2O8 (BSAS) celsian composite was studied between room temperature and 1100 degrees C by the three-point bend test. Test results showed that there is a definite transition in the failure mode with temperature. Up to about 800 degrees C, tensile was the dominant failure mode. Above 800 degrees C, however, the shear failure became prominent. It was shown that mode shift and rapid degradation of shear strength is due to the softening of the untransformed glassy phase in microstructure. The failure mode also exhibited a strong dependency on the L/h ratio of test specimen; large Lih ratio favored the tensile failure, while small L/h ratio promoted the shear failure.
引用
收藏
页码:135 / 147
页数:13
相关论文
共 50 条
  • [21] High-Temperature Dry Sliding Wear Behavior of Al-12Si-CuNiMg Alloy and its Al2O3 Fiber-Reinforced Composite
    Zhang, Qing
    Wei, Shuo
    Gu, Jie
    Qi, Ming
    METALS AND MATERIALS INTERNATIONAL, 2021, 27 (09) : 3641 - 3651
  • [22] High-Temperature Dry Sliding Wear Behavior of Al–12Si–CuNiMg Alloy and its Al2O3 Fiber-Reinforced Composite
    Qing Zhang
    Shuo Wei
    Jie Gu
    Ming Qi
    Metals and Materials International, 2021, 27 : 3641 - 3651
  • [23] A STRUCTURAL STUDY OF OXIDATION IN AN AL2O3 FIBER-REINFORCED TITANIUM ALUMINIDE COMPOSITE
    NOURBAKHSH, S
    SAHIN, O
    MARGOLIN, H
    ACTA METALLURGICA ET MATERIALIA, 1995, 43 (08): : 3035 - 3044
  • [24] MICROCRACKING AND STRENGTH OF AN AL2O3-SIC COMPOSITE
    LANGE, FF
    ARORA, A
    AMERICAN CERAMIC SOCIETY BULLETIN, 1981, 60 (03): : 394 - 394
  • [25] Temperature dependency of interlaminar shear strength of 2D-C/SiC composite
    Wang, H. L.
    Zhang, C. Y.
    Liu, Y. S.
    Han, D.
    Li, M.
    Qiao, S. R.
    MATERIALS & DESIGN, 2012, 36 : 172 - 176
  • [26] Thermal expansion of sintered polycrystals of hexacelsian solid solution (Sr, Ba) Al2Si2O8
    Kobayashi, Yuichi
    Pee, Jae-Hwan
    Murabayashi, Yorikazu
    Katayama, Masaki
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2016, 124 (09) : 881 - 885
  • [27] Development of Al2O3 fiber-reinforced Al2O3-based ceramics
    Tanimoto, Y
    Nemoto, K
    DENTAL MATERIALS JOURNAL, 2004, 23 (03) : 297 - 304
  • [28] Fabrication and characterization of an ultra-high-temperature carbon fiber-reinforced ZrB2-SiC matrix composite
    Tang, Sufang
    Deng, Jingyi
    Wang, Shijun
    Liu, Wenchuan
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2007, 90 (10) : 3320 - 3322
  • [29] HIGH-TEMPERATURE STRUCTURE INVESTIGATION OF ANORTHITE (CA AL2SI2O8) USING X-RAY AND ELECTRON MICROSCOPE
    CZANK, M
    LAVES, F
    SCHULZ, H
    ACTA CRYSTALLOGRAPHICA SECTION A, 1975, 31 : S192 - S192
  • [30] FRACTURE ANGLE OF CRACKS OF THE 2 CRACKS INTERACTION PROBLEM IN A UNIDIRECTIONAL FIBER-REINFORCED COMPOSITE-MATERIAL
    MA, H
    ZHAO, LG
    CHEN, YH
    INTERNATIONAL JOURNAL OF FRACTURE, 1995, 72 (02) : R39 - R43