Effect of Starting SiC Particle Size on Nitridation and Strength of Silicon Nitride-Bonded Silicon Carbide Ceramics

被引:6
|
作者
Choi, Young-Hoon [1 ]
Kim, Young-Wook [1 ]
Woo, Sang-Kuk [2 ]
Han, In-Sub [2 ]
机构
[1] Univ Seoul, Dept Mat Sci & Engn, Seoul 130743, South Korea
[2] Korea Inst Energy Res, Energy Mat Res Ctr, Daejeon 305343, South Korea
关键词
Silicon carbide; Silicon nitride; Silicon nitride-bonded silicon carbide; Nitridation rate; Flexural strength;
D O I
10.4191/KCERS.2010.47.2.157
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Effect of starting SiC particle size on nitridation rate and flexural strength of Si3N4-bonded-SiC (SNBSC) ceramics was investigated by using SiC particles of different size (similar to 200 mu m, similar to 100 mu m and similar to 45 mu m). The specimen prepared from smaller SiC particles resulted in higher nitridation rate after nitridation at 1450 degrees C, owing to the lower packing density in green body. The flexural strength showed maxima after 1-h nitridation for all specimens and then decreased with prolonged nitridation because of local densification-induced pore coarsening. The specimen prepared from smaller SiC particles showed better flexural strength because of smaller pore size and partly higher nitridation rate in the specimen. A maximal flexural strength of 29 MPa was obtained in the specimen with a density of 2.04 g.cm(3), which was prepared from 45 mu m-SiC particles.
引用
收藏
页码:157 / 162
页数:6
相关论文
共 50 条
  • [41] Indentation Size Effect on the Hardness of Silicon Carbide Ceramics
    Curkovic, L.
    Rede, V.
    Grilec, K.
    KEMIJA U INDUSTRIJI-JOURNAL OF CHEMISTS AND CHEMICAL ENGINEERS, 2010, 59 (10): : 483 - 488
  • [42] Effect of aluminum source on flexural strength of mullite-bonded porous silicon carbide ceramics
    Kumar, B. V. Manoj
    Eom, Jung-Hye
    Kim, Young-Wook
    Han, In-Sub
    Woo, Sang-Kuk
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2010, 118 (1373) : 13 - 18
  • [43] FABRICATION OF SILICON NITRIDE-SILICON CARBIDE NANOCOMPOSITE CERAMICS
    KENNEDY, T
    HAMPSHIRE, S
    POORTEMAN, M
    CAMBIER, F
    ADVANCES IN ENGINEERING MATERIALS, 1995, 99-1 : 257 - 263
  • [44] Indentation fatigue in silicon nitride, alumina and silicon carbide ceramics
    A. K. Mukhopadhyay
    Bulletin of Materials Science, 2001, 24 : 105 - 109
  • [45] Indentation fatigue in silicon nitride, alumina and silicon carbide ceramics
    Mukhopadhyay, AK
    BULLETIN OF MATERIALS SCIENCE, 2001, 24 (02) : 105 - 109
  • [46] EFFECT OF OXIDATION ON THE STRENGTH OF SILICON-NITRIDE CERAMICS
    GOGOTSI, YG
    SOPENKO, SI
    TRUNOV, GV
    STRENGTH OF MATERIALS, 1985, 17 (01) : 82 - 87
  • [47] Effect of microstructures on dielectric breakdown strength of sintered reaction-bonded silicon nitride ceramics
    Nakashima, Yuki
    Zhou, You
    Tanabe, Keisuke
    Arima, Souhei
    Hirao, Kiyoshi
    Ohji, Tatsuki
    Murayama, Norimitsu
    Fukushima, Manabu
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2023, 106 (02) : 1139 - 1148
  • [48] THE EFFECT OF CARBIDE AND NITRIDE ADDITIVES ON THE OXIDATION RESISTANCE OF SILICON-NITRIDE CERAMICS
    GOGOTSI, YG
    LAVRENKO, VA
    HIGH TEMPERATURE TECHNOLOGY, 1988, 6 (02): : 79 - 87
  • [49] Influence of silicon carbide particle size on the microstructure and mechanical properties of zirconium diboride-silicon carbide ceramics
    Zhu, Sumin
    Fahrenholtz, William G.
    Hilmas, Gregory E.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2007, 27 (04) : 2077 - 2083
  • [50] MICROSTRUCTURAL CHARACTERIZATION OF SILICON-NITRIDE BONDED SILICON-CARBIDE
    EDWARDS, DP
    MUDDLE, BC
    HANNINK, RHJ
    SILICON NITRIDE 93, 1994, 89-9 : 417 - 421