FRACTURE-TOUGHNESS OF GERMANIUM DETERMINED WITH THE VICKERS INDENTATION TECHNIQUE

被引:20
|
作者
LEMAITRE, P
机构
[1] Studiecentrum voor Kernenergie, Mol, Belg, Studiecentrum voor Kernenergie, Mol, Belg
关键词
MICROSCOPIC EXAMINATION - Scanning Electron Microscopy;
D O I
10.1007/BF00723798
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The introduction and refinement of the indentation technique has made the measurement of fracture toughness simpler. In this work, all Vickers indentations were positioned so that the Vickers-induced radial cracks developed along the same set of planes perpendicular to the (111) plane. The indented surfaces were examined by scanning electron microscopy (SEM). The Vickers indentation technique yields a fracture toughness value of 0. 53 MPa m** one-half plus or minus 0. 06 for monocrystalline germanium. 5 Refs.
引用
收藏
页码:895 / 896
页数:2
相关论文
共 50 条
  • [31] Measurement of fracture toughness in AISI 1018 borided steels by vickers indentation
    Instituto Politécnico Nacional, SEPI-ESIME U.P. Adolfo López Mateos, Zacatenco. México D.F. 07738, Mexico
    不详
    Diffus Defect Data Pt A Diffus Forum, 2008, (675-680): : 675 - 680
  • [32] Measurement of Fracture Toughness in AISI 1018 Borided Steels by Vickers Indentation
    Campos-Silva, I.
    Lopez-Perrusquia, N.
    Ortiz-Dominguez, M.
    Figueroa-Lopez, U.
    Hernandez-Sanchez, E.
    DIFFUSION IN SOLIDS AND LIQUIDS IV, 2009, 283-286 : 675 - +
  • [33] Determination of Vickers indentation fracture toughness of boronised alloyed ductile iron
    Toktas, A.
    TRANSACTIONS OF THE INSTITUTE OF METAL FINISHING, 2019, 97 (05): : 271 - 276
  • [34] Fracture Toughness of HVOF Sprayed Cermet Coatings Measured by Vickers Indentation
    Houdkova, Sarka
    Zahalka, Frantisek
    Kasparova, Michaele
    MATERIALS STRUCTURE & MICROMECHANICS OF FRACTURE, 2011, 465 : 475 - 478
  • [35] THE EFFECTS OF THIN COMPRESSIVE FILMS ON INDENTATION FRACTURE-TOUGHNESS MEASUREMENTS
    KOBRIN, PH
    HARKER, AB
    JOURNAL OF MATERIALS SCIENCE, 1989, 24 (04) : 1363 - 1367
  • [36] INDENTATION FRACTURE-TOUGHNESS AND DYNAMIC YOUNGS MODULUS OF CERAMIC BIOMATERIALS
    JONES, DW
    RIZKALLA, AS
    SUTOW, EJ
    KING, HW
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1988, 105 : 207 - 213
  • [37] Vickers indentation fracture toughness of Y-TZP dental ceramics
    Coric, Danko
    Renjo, Marijana Majic
    Curkovic, Lidija
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2017, 64 : 14 - 19
  • [38] INDENTATION FRACTURE-TOUGHNESS OF 3 NEW CERAMIC CORE MATERIALS
    CHU, TM
    WAGNER, WC
    RAZZOOG, ME
    JOURNAL OF DENTAL RESEARCH, 1995, 74 : 471 - 471
  • [40] ERROR PROPAGATION BIASES IN THE CALCULATION OF INDENTATION FRACTURE-TOUGHNESS FOR CERAMICS
    KELLY, JR
    COHEN, ME
    TESK, JA
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1993, 76 (10) : 2665 - 2668