Failure Investigation of Boiler Water Wall Tubes of a Thermal Power Station

被引:14
|
作者
Munda, Parikshit [1 ]
Kumar, Subodh [1 ]
Prakash, Amit [1 ]
Husain, Md Murtuja [1 ]
Rajnikanth, V. [1 ]
Chowdhury, S. Ghosh [1 ]
机构
[1] CSIR Natl Met Lab, Mat Sci & Technol Div, Jamshedpur 831007, Bihar, India
关键词
Boiler tube; Hydrogen-induced cracking; Welding defects; HAZ; Ferrite-pearlite;
D O I
10.1007/s11668-015-0055-0
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Failure investigation was carried out on boiler water wall tubes of a thermal power plant through visual inspection, chemical analysis, and metallurgical analysis. Failure was in the form of thin/micro cracks along the length of the tubes which were located at the girth welding joint of tubes. Experimental results revealed that the cracking was from inward to outward of the tube thickness. Discontinuities/cavities were observed in the welded region which might have occurred due to lack of fusion of base metal and the weld metal. Cracks were initiated from the sharp corner/crack tip of the cavities/discontinuities present at the welded region under the action of hoop/thermal stress existed during the operation. Nature of the crack propagation indicates the case of typical hydrogen-induced cracking. Moreover, the presence of the cavities/discontinuities reduced the cross-sectional area of tubes resulting increased stress intensity. Increased stress beyond the flow stress of the material assisted by hydrogen-induced effect resulted the cracking of the tubes. In order to mitigate the problem, proper welding of tubes joints should be carried out followed by proper inspection after weld. Secondly, hydrogen dissolution during welding should be prevented and treatment for its removal after welding should be carried out.
引用
收藏
页码:9 / 18
页数:10
相关论文
共 50 条
  • [21] Corrosive degradation and failure of vertical furnace wall tubes of a boiler
    Natl Metallurgical Lab, Jamshedpur, India
    [J]. Eng Failure Anal, 4 (279-286):
  • [22] Failure Investigation of Fire-Side Water-Wall Tube Boiler
    Fatah, M. C.
    Agustiadi, D.
    Pramono, A. W.
    [J]. CORROSION SCIENCE AND TECHNOLOGY-KOREA, 2021, 20 (05): : 242 - 248
  • [23] Failure analysis of boiler economizer tubes at power house
    Pal, Urbi
    Kishore, Kaushal
    Mukhopadhyay, Suman
    Mukhopadhyay, Goutam
    Bhattacharya, Sandip
    [J]. ENGINEERING FAILURE ANALYSIS, 2019, 104 : 1203 - 1210
  • [24] A new method for identification of thermal boundary conditions in water-wall tubes of boiler furnaces
    Duda, Piotr
    Taler, Jan
    [J]. INTERNATIONAL JOURNAL OF HEAT AND MASS TRANSFER, 2009, 52 (5-6) : 1517 - 1524
  • [25] Investigation on high temperature corrosion of water-cooled wall tubes at a 300 MW boiler
    Xiong, Xiaohe
    Liu, Xing
    Tan, Houzhang
    Deng, Shuanghui
    [J]. JOURNAL OF THE ENERGY INSTITUTE, 2020, 93 (01) : 377 - 386
  • [26] Design and Study of Water Supply System for Supercritical Unit Boiler in Thermal Power Station
    Du, Zenghui
    [J]. ADVANCES IN MATERIALS, MACHINERY, ELECTRONICS II, 2018, 1955
  • [27] Optimization of Boiler Efficiency at Mettur Thermal Power Station
    Bijli, Muhamed Muzaiyen S. M.
    Paneerselvam, T.
    Alahiyanambi, K.
    Basha, M. A. Jafar
    [J]. PROCEEDINGS OF THE INTERNATIONAL CONFERENCE ON SOFT COMPUTING SYSTEMS, ICSCS 2015, VOL 1, 2016, 397 : 581 - 592
  • [28] Failure Investigation of Radiant Platen Superheater Tube of Thermal Power Plant Boiler
    Ghosh, D.
    Ray, S.
    Mandal, A.
    Roy, H.
    [J]. HIGH TEMPERATURE MATERIALS AND PROCESSES, 2015, 34 (02) : 171 - 175
  • [29] Condition Assessment of Boiler Water Wall Tubes using Robotics
    Vajpayee, Ankit
    Russell, David
    [J]. e-Journal of Nondestructive Testing, 2022, 27 (12):
  • [30] Failure investigation of a water-wall tube of fossil-fuel fired boiler
    Ranjeeth, R.
    Aditya, D.
    Gautam, Anil
    Singh, S. P.
    Bhattacharya, S.
    [J]. ENGINEERING FAILURE ANALYSIS, 2024, 155